Development of a predictive optimization model for the compressive strength of sodium activated fly ash based geopolymer pastes

被引:29
作者
Fillenwarth, Brian A. [1 ]
Sastry, Shankar M. L. [1 ]
机构
[1] Washington Univ, Dept Mech Engn & Mat Sci, St Louis, MO 63130 USA
关键词
Alkali activated cement; Geopolymer paste; Compressive strength; Fly ash; Predictive optimization model; Genetic programming; ALKALINE ACTIVATION; CURING CONDITIONS; TEMPERATURE; REACTIVITY;
D O I
10.1016/j.fuel.2015.01.029
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
As concerns about global CO2 emissions grow, there exists a need for widespread commercialization of lower emission building materials such as geopolymers. The commercialization of geopolymers is currently impeded by the high variability of the materials used for their synthesis and limited knowledge of the interrelationships between mix design variables. To overcome these barriers, this work demonstrates a relationship between the compressive strength and the chemical design variables derived from experimental data using genetic programming. The developed model indicates the main chemical factors responsible for the compressive strength of sodium activated geopolymers are the contents of Na2O, reactive SiO2, and H2O. The contents of reactive Al2O3 and CaO were found to not have a significant impact on the compressive strength. The optimization model is shown to predict the compressive strength of fully cured sodium activated fly ash based geopolymer pastes from their chemical composition to within 6.60 MPa. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:141 / 146
页数:6
相关论文
共 35 条
[21]   Influence of slag as additive on compressive strength of fly ash-based geopolymer [J].
Li, Zongjin ;
Liu, Sifeng .
JOURNAL OF MATERIALS IN CIVIL ENGINEERING, 2007, 19 (06) :470-474
[22]   Costs and carbon emissions for geopolymer pastes in comparison to ordinary portland cement [J].
McLellan, Benjamin C. ;
Williams, Ross P. ;
Lay, Janine ;
van Riessen, Arie ;
Corder, Glen D. .
JOURNAL OF CLEANER PRODUCTION, 2011, 19 (9-10) :1080-1090
[23]   Modeling the compressive strength of geopolymeric binders by gene expression programming-GEP [J].
Nazari, Ali ;
Torgal, F. Pacheco .
EXPERT SYSTEMS WITH APPLICATIONS, 2013, 40 (14) :5427-5438
[24]   Alkaline activation of fly ashes:: NMR study of the reaction products [J].
Palomo, A ;
Alonso, S ;
Femandez-Jiménez, A .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2004, 87 (06) :1141-1145
[25]   Effect of synthesis parameters on the mechanical properties of fly ash-based geopolymers [J].
Panias, Dimitrios ;
Giannopoulou, Ioanna P. ;
Perraki, Theodora .
COLLOIDS AND SURFACES A-PHYSICOCHEMICAL AND ENGINEERING ASPECTS, 2007, 301 (1-3) :246-254
[26]   Compressive Strength Assessment of Geopolymer Composites by a Phenomenological Model [J].
Radhakrishna ;
Shashishankar, A. ;
Udayashankar, B. C. ;
Devi, M. V. Renuka .
JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 2010, 29 (06) :840-854
[27]  
Ravindra N.T., 2009, Asian Research Publishing Network Journal of Engineering and Applied science, V4, P68
[28]   Distilling Free-Form Natural Laws from Experimental Data [J].
Schmidt, Michael ;
Lipson, Hod .
SCIENCE, 2009, 324 (5923) :81-85
[29]  
Skvara F, 2003, P 11 INT C CHEM CEM
[30]   Utilisation of fly ash in a geopolymeric material [J].
Swanepoel, JC ;
Strydom, CA .
APPLIED GEOCHEMISTRY, 2002, 17 (08) :1143-1148