Zircaloy-4 high temperature oxidation in atmospheres representative of SFP-LOCA: Investigation of the influence of a low temperature pre-oxidation scale

被引:11
|
作者
Duriez, C. [1 ]
Coindreau, O. [1 ]
Gestin, M. [1 ,2 ]
Kasperski, A. [1 ,4 ]
Peres, V [2 ]
Pijolat, M. [2 ]
Buscail, H. [3 ]
Issartel, C. [3 ]
Rolland, R. [3 ]
Mermoux, M. [4 ]
机构
[1] PSN RES, Inst Radioprotect & Surete Nucl, Cadarache BP 3, F-13115 St Paul Les Durance, France
[2] Ecole Natl Super Mines, Ctr SPIN, CNRS, Lab George Friedel,UMR 5307, 158 Cours Fauriel, F-42023 St Etienne, France
[3] Univ Clermont Auvergne, LVEEM, 8 Rue JB Fabre,CS 10219, F-43009 Le Puy En Velay, France
[4] Univ Grenoble Alpes, UMR CNRS 5279, LEPMI, F-38402 St Martin dHeres, France
关键词
OXYGEN DIFFUSION; ZIRCONIUM ALLOYS; AIR; CORROSION; KINETICS; NITROGEN; STRESS; TIN; MIXTURES; PRE;
D O I
10.1016/j.jnucmat.2018.10.019
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Within the framework of the French DENOPI project dedicated to the study of Spent Fuel Pool accidents, the high temperature degradation of Zircaloy-4 cladding material has been investigated in the 700-950 degrees C range, in air and air-steam atmospheres. In particular, we focused on the effect of the pretransient corrosion-oxide scale formed on the cladding materiel during in-reactor use, here simulated by an out-off-pile low-temperature pre-oxidation step. In-situ X-Ray Diffraction evidenced strong evolutions of the stress state and grain size of these laboratory-grown pre-oxidation scales upon high temperature exposures. From O-18 tracer experiments and thermogravimetric analysis, the pre-oxide was shown to be a rather efficient barrier against further high temperature attack by the nitrogen-containing atmosphere, despite its multi-layered, porous microstructure. Oxygen apparent diffusion coefficients were derived from the O-18 tracer experiments. These diffusion coefficients suggest that the pre-oxide rather behaves like a dense monoclinic zirconia layer. The protective effect was sometimes observed to be maintained during very long exposure times at high temperature, depending on the presence of defects in the scale. Where the protective effect was first lost, the nitrogen-"catalyzed" oxidation initiated and progressively propagated to the whole specimen surface. A propagation mechanism is proposed, which involves progressive mechanical failure of the pre-oxide scale, below which the high temperature, nitrogen-assisted, porous oxidation formation occurs. The cladding degradation kinetics, driven by this propagation mechanism, is only weakly affected by the presence of steam. However, where the porous oxide formed, strong hydrogen pick-up in the underlying metallic substrate was observed. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:152 / 174
页数:23
相关论文
共 50 条
  • [41] Development of Temperature Control System for Large-Scale Pre-oxidation Furnace
    Yu Kuan
    Zhu Bo
    ADVANCED MANUFACTURING SYSTEMS, 2011, 339 : 43 - 47
  • [42] Investigation on Microstructures and High-Temperature Oxidation Resistance of Cr Coatings on Zircaloy-4 by Multi-Arc Ion Plating Technology
    Peng, Yingbo
    Du, Peinan
    Liu, Yuxi
    Wang, Haijiang
    Liu, Shuyu
    Zhang, Wei
    MATERIALS, 2022, 15 (19)
  • [43] High temperature oxidation of zirconium and zircaloy-4 under applied load: Nuclear microprobe study of the growth of the oxide
    Berger, P
    El Tahhann, R
    Moulin, G
    Viennot, M
    NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2003, 210 : 519 - 525
  • [45] Study of oxide and α-Zr(O) growth kinetics from high temperature steam oxidation of Zircaloy-4 cladding
    Sawarn, Tapan K.
    Banerjee, Suparna
    Samanta, Akanksha
    Rath, B. N.
    Kumar, Sunil
    JOURNAL OF NUCLEAR MATERIALS, 2015, 467 : 820 - 831
  • [46] Effect of low-temperature pre-oxidation on the self-heating of coal
    Liu, Hao
    Li, Zenghua
    Yang, Yongliang
    Miao, Guodong
    Li, Purui
    Wang, Guoqin
    FUEL, 2024, 356
  • [47] Thermal Behavior of the Low-temperature Secondary Oxidation of Coal under Different Pre-oxidation Temperatures
    Wang, Kai
    Gao, Peng
    Sun, Weili
    Fan, Haohao
    He, Yunzhong
    Han, Tao
    COMBUSTION SCIENCE AND TECHNOLOGY, 2022, 194 (08) : 1712 - 1729
  • [48] The Oxidation Behaviors of NiCoCrAlY Coatings After Pre-Oxidation Treatment During High-Temperature Oxidation at 800 ℃ and 900 ℃
    Masahiro Negami
    Yoko Yamabe-Mitarai
    High Temperature Corrosion of Materials, 2024, 101 : 511 - 527
  • [49] Oxidation kinetics of low-Sn Zircaloy-4 at the temperature range from 773 to 1,573 K
    Nagase, F
    Otomo, T
    Uetsuka, H
    JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY, 2003, 40 (04) : 213 - 219
  • [50] Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel
    Bai Yin
    Liu Zhengdong
    Xie Jianxin
    Bao Hansheng
    Chen Zhengzong
    ACTA METALLURGICA SINICA, 2018, 54 (06) : 895 - 904