Correlation of fatigue life of fillet welded joints based on stress at 1 mm in depth

被引:0
作者
Xiao, ZG [1 ]
Yamada, K [1 ]
机构
[1] Nagoya Univ, Dept Civil Engn, Chikusa Ku, Nagoya, Aichi 4648603, Japan
来源
ADVANCES IN STEEL STRUCTURES, VOLS I & II, PROCEEDINGS | 2002年
关键词
fatigue; fillet weld; stress concentration factor; local stress; FEM; FEA; gusset; attachment; cruciform joint;
D O I
暂无
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Fillet welds are widely used to connect attachments, such as gussets or cover plates, to steel structures. The geometric discontinuity caused by the introduction of fillet weld and the attachments leads to stress concentration. Fatigue cracks may form at weld toe at the end or edge of the attachment when the structure is subjected to cyclic loadings. In this study, stress distribution around weld toe region is studied with a non-load-carrying cruciform joint. It is found that the weld toe shape, i.e., weld toe angle and weld toe radius, is crucial in affecting stress concentration at weld toe, but the affecting region is limited with 1 mm in depth. The effect of weld size (leg length) of the weld bead is less significant than that of weld toe shape. The stress at 1 mm in depth in the cross section of the main plate passing weld toe is taken as an indication of geometric effects of the welded joints. If fatigue test results of fillet welded joints are expressed in terms of stress range at 1 mm in depth, which contains effect of geometry of welded joint except that of weld bead, the scatter of test data will only reflect the effect of weld profile. Thus correlation between different types of fillet welds can be established by means of stress at 1 mm in depth. Fatigue test results are collected for non-load-carrying cruciform joints with about 10 mm thick of main plate and attachment. In these joints, the geometric effect of transverse attachment is rather small, and FEM analyses also show their stresses at 1 mm in depth to be around unity. The scatter band of these test data matches well with those of test data of in-plane and out-of-plane gussets plotted in terms of stress range of 1 mm in depth.
引用
收藏
页码:1001 / 1008
页数:8
相关论文
共 8 条
[1]  
Hobbacher A., 1995, XIII153995XV84595 II
[2]  
*JSSC, 1995, FAT DES REC STEEL ST
[3]   A notch intensity factor approach to the stress analysis of welds [J].
Lazzarin, P ;
Tovo, R .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 1998, 21 (09) :1089-1103
[4]  
Niemi E, 2002, P IIW FAT SEM, P73
[5]  
*SRAC, 2000, COSM M US GUID COSM
[6]  
Tveiten B.W., 2000, MAR STRUCT, V13, P189, DOI 10.1016/S0951-8339(00)00022-8
[7]   CRITERIA FOR THE FATIGUE ASSESSMENT OF HOLLOW STRUCTURAL SECTION CONNECTIONS [J].
VANWINGERDE, AM ;
JEFFREY, AP ;
WARDENIER, J .
JOURNAL OF CONSTRUCTIONAL STEEL RESEARCH, 1995, 35 (01) :71-115
[8]  
YAMADA K, 2002, J STRUCT ENG JSCE, V48, P1047