Liquation and post-weld heat treatment cracking in Rene 80 laser repair welds

被引:36
|
作者
Rush, Matthew T. [1 ]
Colegrove, Paul A. [1 ]
Zhang, Zhu [2 ]
Broad, David [2 ]
机构
[1] Cranfield Univ, Welding Engn & Laser Proc Res Ctr, Cranfield MK43 0AL, Beds, England
[2] Doncasters Grp Ltd, Burton Upon Trent DE14 2WR, Staffs, England
基金
英国工程与自然科学研究理事会;
关键词
Liquation cracking; Nickel superalloy; Laser welding; Strain-age cracking; Post weld heat treatment cracking; Rene; 80; Repair welding; PWHT cracking; NICKEL-BASED SUPERALLOY; INCONEL 738LC SUPERALLOY; WELDABILITY; DEPOSITION;
D O I
10.1016/j.jmatprotec.2011.09.001
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An extensive experimental study on a nickel-based superalloy, Rene 80 using autogenous laser welding has been undertaken to determine the effect of the process parameters and weld bead geometry on cracking in the as-welded and post-weld heat treated conditions. Little cracking was observed in the as-welded condition with low powers and beam diameters around 2.5 mm. Welding speed had little effect on the incidence of cracking in the as-welded condition. Investigation of the aspect ratio (penetration divided by width) indicated that little cracking occurred in the as-welded condition when the aspect ratio was approximately 0.5. The same effect was observed with the post-weld heat treated samples. An analysis of the microstructures indicated that the cracking was caused primarily by liquation in the as-welded condition and was exacerbated by post-weld heat treatment cracking during the subsequent heat treatment. Finally the study resolved some of the contradictory findings in the literature on the effect of process parameters on the incidence of cracking in the as-welded and post-weld heat treated conditions. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:188 / 197
页数:10
相关论文
共 50 条
  • [41] Influence of pre- and post-weld heat treats on microstructures of laser welded GTD-111 with IN-718 as filler metal
    Jaruratchataphun, Juthamate
    Kiatwisarnkij, Napat
    Rojhirunsakool, Tanaporn
    Lothongkum, Gobboon
    Wangyao, Panyawat
    MATERIALS TESTING, 2022, 64 (12) : 1710 - 1719
  • [42] The effect of Nd:YAG laser pulse duration and post-weld heat treatment on the microstructure and mechanical properties of laser-welded NiTi shape memory alloy
    Rasouli, Ali
    Naffakh-Moosavy, Homam
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2023, 23 : 6065 - 6074
  • [43] Induction heat treatment of laser welds
    Bagger, C
    Sorensen, JI
    Olsen, FO
    JOURNAL OF LASER APPLICATIONS, 2003, 15 (04) : 211 - 219
  • [44] Effects of post-weld heat treatment on the microstructure and mechanical properties of laser-welded NiTi/304SS joint with Ni filler
    Chen, Yuhua
    Sun, Songwei
    Zhang, Timing
    Zhou, Xingwen
    Li, Shuhan
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2020, 771
  • [45] Microstructure of Al-Li alloy electron beam welding joint after post-weld heat treatment
    Wang, Shaogang
    Yu, Kuang
    Luo, Chuanxiao
    Xing, Li
    ADVANCED MATERIALS AND PROCESS TECHNOLOGY, PTS 1-3, 2012, 217-219 : 1921 - 1927
  • [46] Effect of Post Weld Heat Treatment on Mechanical Properties and Microstructure of Nickel based Super Alloy Welds
    Agilan, M.
    Venkateswaran, T.
    Sivakumar, D.
    Pant, Bhanu
    ADVANCES IN MATERIALS AND PROCESSING: CHALLENGES AND OPPORTUNITIES, 2012, 585 : 435 - 439
  • [47] Effects of post-weld heat treatment on microstructure and mechanical properties of TLP bonded Incone1718 superalloy
    Cao, J.
    Wang, Y. F.
    Song, X. G.
    Li, C.
    Feng, J. C.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 590 : 1 - 6
  • [48] Effects of post-weld heat treatment on mechanical properties and microstructure of resistance spot-welded lightweight steel
    Hwang, Insung
    Cho, Heewon
    Nam, Sangwoo
    Kang, Munjin
    Koo, Min-Seo
    Kim, Young-Min
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2019, 104 (9-12) : 4813 - 4825
  • [49] Dissimilar Laser Welding of Austenitic Stainless Steel and Abrasion-Resistant Steel: Microstructural Evolution and Mechanical Properties Enhanced by Post-Weld Heat Treatment
    Hietala, Mikko
    Jaskari, Matias
    Ali, Mohammed
    Jarvenpaa, Antti
    Hamada, Atef
    MATERIALS, 2021, 14 (19)
  • [50] Effect of local carbide formation behavior on repair weld liquation cracking susceptibility for long-term-serviced 247LC superalloy
    Jeong, Hye-Eun
    Seo, Seong-Moon
    Chun, Eun-Joon
    JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2024, 28 : 110 - 122