Growth and orientation dependence of electrical properties of 0.92Na0.5Bi0.5TiO3-0.08 K0.5Bi0.5TiO3 lead-free piezoelectric single crystal

被引:22
作者
Sun, Renbing [1 ,2 ,3 ]
Zhao, Xiangyong [1 ]
Zhang, Qinhui [1 ,3 ]
Fang, Bijun [2 ]
Zhang, Haiwu [1 ,3 ]
Li, Xiaobing [1 ]
Lin, Di [1 ]
Wang, Sheng [1 ]
Luo, Haosu [1 ]
机构
[1] Chinese Acad Sci, Key Lab Inorgan Funct Mat & Device, Shanghai Inst Ceram, Shanghai 201800, Peoples R China
[2] Changzhou Univ, Sch Mat Sci & Engn, Changzhou 213164, Jiangsu, Peoples R China
[3] Chinese Acad Sci, Grad Sch, Beijing 10039, Peoples R China
关键词
DEPOLARIZATION TEMPERATURE; PHASE-TRANSITIONS; SYSTEM; POLARIZATION; BEHAVIOR;
D O I
10.1063/1.3601116
中图分类号
O59 [应用物理学];
学科分类号
摘要
A 0.92Na(0.5)Bi(0.5)TiO(3)-0.08 K0.5Bi0.5TiO3 (0.92NBT-0.08KBT) lead-free piezoelectric single crystal with dimensions of Phi 35 x 10 mm was successfully grown by the top-seeded solution growth method. The effective segregation coefficient for K was calculated to be 0.27. An x-ray powder diffraction measurement showed that the as-grown crystal possesses a rhombohedral perovskite structure at room temperature. The room-temperature dielectric constants for poled < 001 >, < 110 >, and < 111 > oriented crystal samples are found to be 683, 567, and 435 at 1 kHz, respectively. The (T-m, epsilon(m)) values for < 001 >, < 110 >, and < 111 > oriented crystals are (316 degrees C, 4318), (317 degrees C, 4160), and (318 degrees C, 4348) at 1 kHz, which indicate that the dielectric parameters of the as-grown crystals show weaker anisotropy. The curves, epsilon(T), for the three crystallographic orientations show two anomalies at about 170 and 320 degrees C, respectively, relating to the ferroelectric-antiferroelectric phase and the antiferroelectric-paraelectric phase. There is a thermal hysteresis, Delta T approximate to 35 degrees C for the ferroelectric-antiferroelectric phase transformation between heating and cooling. The antiferroelectric phase, the thermal hysteresis, and the dielectric relaxor behavior around 170 degrees C can be attributed to the formation of an intermediate orthorhombic modulated phase at 170-320 degrees C. For the < 001 >, < 110 >, and < 111 > crystal samples, the room-temperature piezoelectric constants, d(33), reach 175, 130, and 70 pC/N, respectively. The remanent polarization for the < 001 >, < 110 >, and < 111 > crystal samples are 8.1, 10.8, and 13.5 mu C/cm(2), respectively, and the ratio is 1:1.33: 1.67, close to 1:root 2:root 3. The diffusive factors, a, are found to be 1.94, 1.91, and 1.50 for the < 001 >, < 110 >, and < 111 > oriented crystal samples, which indicate that the antiferroelectric-paraelectric phase transition of the as-grown 0.92NBT-0.08KBT crystal is a strong diffuse one. The electromechanical coupling coefficients for the < 001 >, < 110 >, and < 111 > oriented 0.92NBT-0.08KBT crystals at room temperature are 52, 50, and 48%, respectively. The values of k(t) for the three main crystallographic orientations change slightly with the increase of temperature from 15 to 140 degrees C, demonstrating a relatively stable thermal electromechanical coupling property. (C) 2011 American Institute of Physics. [doi:10.1063/1.3601116]
引用
收藏
页数:8
相关论文
共 32 条
[1]   SOME PROPERTIES OF BISMUTH PEROVSKITES [J].
BUHRER, CF .
JOURNAL OF CHEMICAL PHYSICS, 1962, 36 (03) :798-&
[2]   Structure and electrical properties of (Na0.5Bi0.5)1-xBaxTiO3 piezoelectric ceramics [J].
Chen, Min ;
Xu, Qing ;
Kim, Bok Hee ;
Ahn, Byeong Kuk ;
Ko, Jung Hoon ;
Kang, Woo Jin ;
Nam, O. Jeong .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2008, 28 (04) :843-849
[3]   Electrical properties of Na1/2Bi1/2TiO3-BaTiO3 ceramics [J].
Chu, BJ ;
Chen, DR ;
Li, GR ;
Yin, QR .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (13) :2115-2121
[4]   Reinvestigation of phase transitions in Na0.5Bi0.5TiO3 by TEM.: Part I:: First order rhombohedral to orthorhombic phase transition [J].
Dorcet, V. ;
Trolliard, G. ;
Boullay, P. .
CHEMISTRY OF MATERIALS, 2008, 20 (15) :5061-5073
[5]   Detection of phase transitions in sodium bismuth titanate-barium titanate single crystals by acoustic emission [J].
Dul'kin, E. ;
Mojaev, E. ;
Roth, M. ;
Greicius, S. ;
Granzow, T. .
APPLIED PHYSICS LETTERS, 2008, 92 (01)
[6]   Na0.5Bi0.5TiO3-K0.5Bi0.5TiO3 (NBT-KBT) system: A structural and electrical study [J].
Elkechai, O ;
Manier, M ;
Mercurio, JP .
PHYSICA STATUS SOLIDI A-APPLICATIONS AND MATERIALS SCIENCE, 1996, 157 (02) :499-506
[7]   Polarization rotation mechanism for ultrahigh electromechanical response in single-crystal piezoelectrics [J].
Fu, HX ;
Cohen, RE .
NATURE, 2000, 403 (6767) :281-283
[8]   Sodium-bismuth titanate based lead-free ferroelectric materials [J].
Gomah-Pettry, JR ;
Saïd, E ;
Marchet, P ;
Mercurio, JP .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (06) :1165-1169
[9]   Phase transition temperature and electrical properties of (Bi1/2Na1/2)TiO3-(Bi1/2A1/2)TiO3 (A=Li and K) lead-free ferroelectric ceramics [J].
Hiruma, Yuji ;
Yoshii, Kazushige ;
Nagata, Hajime ;
Takenaka, Tadashi .
JOURNAL OF APPLIED PHYSICS, 2008, 103 (08)
[10]   Large electric-field-induced strain in Bi0.5Na0.5TiO3-Bi0.5K0.5TiO3 solid solution single crystals [J].
Izumi, Makoto ;
Yamamoto, Katsuya ;
Suzuki, Muneyasu ;
Noguchi, Yuji ;
Miyayama, Masaru .
APPLIED PHYSICS LETTERS, 2008, 93 (24)