Dielectric Breakdown of Thinned BaO-Al2O3-B2O3-SiO2 Glass

被引:39
作者
Lee, Hoikwan [1 ]
Smith, Nicholas J. [1 ]
Pantano, Carlo G. [1 ]
Furman, Eugene [1 ]
Lanagan, Michael T. [1 ]
机构
[1] Penn State Univ, Mat Res Inst, University Pk, PA 16802 USA
基金
美国国家科学基金会;
关键词
ACID;
D O I
10.1111/j.1551-2916.2010.03749.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The dielectric breakdown behavior of alkali-free glass was determined as a function of thickness and surface roughness. The thickness of commercially available glass (as-received thickness=50 mu m) was reduced to a range of thicknesses between 47 and 5 mu m by chemical etching. The RMS surface roughness of the as-received glass was in the range of 0.14-0.47 nm, and the surface roughness increased to up 10 nm after etching; it was also found that agitating the etching solution by ultrasound reduced the overall surface roughness. The evaluation of these samples revealed that the dielectric breakdown strength increased as the thickness decreased. However, the Weibull modulus representing the distribution of dielectric strengths showed a dependence on the surface roughness of the etched glass. A power law dependence, E-B proportional to d-n, where d is the glass thickness and n=0.14 and 0.86, has been found to fit the data in the respective thickness ranges of 5-20 and 25-50 mu m. Self-healing behavior, which allows the dielectric to continue to support a high electric field after breakdown, was found to be more likely as the dielectric layer thickness decreased. The susceptibility to self healing was correlated with the stored electrostatic energy and latent heat of vaporization for the gold electrode material.
引用
收藏
页码:2346 / 2351
页数:6
相关论文
共 26 条
[11]   Effects of chemical etching with sulfuric acid on glass surface [J].
Jang, HK ;
Chung, YD ;
Whangbo, SW ;
Lee, YS ;
Lyo, IW ;
Whang, CN ;
Lee, SJ ;
Kim, G .
JOURNAL OF VACUUM SCIENCE & TECHNOLOGY A-VACUUM SURFACES AND FILMS, 2000, 18 (02) :401-404
[12]  
JHOU H, 2003, MICROELECTRON J, V34, P259
[13]   Thickness dependent dielectric strength of a low-permittivity dielectric film [J].
Kim, HK ;
Shi, FG .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2001, 8 (02) :248-252
[14]  
Klein N., 1969, Advances in Electronics and Electron Physics, V26, P309
[15]  
Lee H., J APPL PHYS IN PRESS
[16]   Dependence of breakdown field on dielectric (interelectrode) thickness in base-metal electroded multilayer capacitors [J].
Milliken, Alexander D. ;
Bell, Andrew J. ;
Scott, James F. .
APPLIED PHYSICS LETTERS, 2007, 90 (11)
[17]  
O'Dwyer J., 1973, THEORY ELECT CONDUCT
[18]   VARIATION OF TRAPPING DETRAPPING PROPERTIES AS A FUNCTION OF THE INSULATOR SIZE [J].
OH, KH ;
ONG, CK ;
TAN, BTG ;
LEGRESSUS, C ;
BLAISE, G .
JOURNAL OF APPLIED PHYSICS, 1993, 74 (03) :1960-1967
[19]   Alkali-free glass as a high energy density dielectric material [J].
Smith, Nicholas J. ;
Rangarajan, Badri ;
Lanagan, Michael T. ;
Pantano, Carlo G. .
MATERIALS LETTERS, 2009, 63 (15) :1245-1248
[20]   Reactive ion etching of glass for biochip applications:: Composition effects and surface damages [J].
Thienot, Edouard ;
Domingo, Florian ;
Cambril, Edmond ;
Gosse, Charlie .
MICROELECTRONIC ENGINEERING, 2006, 83 (4-9) :1155-1158