Effects of Al, Si and Mo on passivation characteristics of Fe-10Cr alloys

被引:1
作者
Hio, K [1 ]
Adachi, T
Yamada, T
Tsuchida, Y
Nakajima, K
Hosoi, Y
机构
[1] Mie Prefectural Ind Res Inst, Met Lab, Kuwana 5110937, Japan
[2] Daido Inst Technol, Fac Engn, Dept Mech Engn, Nagoya, Aichi 4578531, Japan
[3] Nagoya Municipal Ind Res Inst, Nagoya, Aichi 4560058, Japan
关键词
iron-chromium alloy; aluminum; silicon; molybdenum; anodic polarization; pitting potential; decay curve; passive film; Auger electron spectroscopy; x-ray photoelectron spectroscopy;
D O I
10.2320/jinstmet1952.64.12_1148
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
A study has been made on the effects of Al, Si and Mo on anodic polarization characteristics of Fe-10Cr alloys in 0.05-1.0 kmol.m(-3) H2SO4 and NaCl aqueous solutions. Potential decay curves have also been measured in order to evaluate the stability of the passive films formed on Fe-10Cr alloys containing Al, Si and Mo. The analysis of the chemical composition of the passive film has been carried out by AES and XPS. The addition of Mo was very useful to decrease the critical passivation current density of Fe-10Cr alloys which contained Al and Si. The passive current density decreased with addition of 2 mass%Mo to an Fe-10Cr-3Si alloy, while it increased in an Fe-10Cr-3Al alloy. Fitting potential was moved toward the noble direction by the addition of Mo, except for the case of an Fe-10Cr-3Al-3Si-2Mo alloy. It seems that Laves phase (Fe2Mo) was precipitated in this alloy, and Mo-depleted zone was formed locally. The activation time was increased by the addition of Al, Si and Mo to Fe-10Cr alloys. Two step potential decay curves were obtained in Si-containing alloys, and this behavior of the decay curve was shown more clearly in an Fe-10Cr-3Si-2Mo alloy. The results of AES and XPS analysis indicated that Cr and Al concentrated in the passive film of an Fe-10Cr-Al alloy. In the case of an Fe-10Cr-Si alloy, Si concentrated in the surface region of the film and Cr did in the internal region of the film. The confirmation was not possible for the enrichment of Mo in the passive film.
引用
收藏
页码:1148 / 1155
页数:8
相关论文
共 50 条
  • [31] Electrochemical characteristics of nano and microcrystalline Fe–Cr alloys
    Rajeev K. Gupta
    R. K. Singh Raman
    C. C. Koch
    Journal of Materials Science, 2012, 47 : 6118 - 6124
  • [32] Influence of Al and Si on austenite formation in Cr–Ni–Mo steel in the intercritical temperature range
    Gervas’ev M.A.
    Yurovskikh A.S.
    Belikov S.V.
    Maslova O.V.
    Zhilin A.S.
    Steel in Translation, 2015, 45 (9) : 658 - 661
  • [33] Thermodynamic properties of Si-Al, -Ca, -Mg binary and Si-Ca-Al, -Ti, -Fe ternary alloys
    Miki, T
    Morita, K
    Sano, N
    MATERIALS TRANSACTIONS JIM, 1999, 40 (10): : 1108 - 1116
  • [34] The Effects of Mg and Si Contents on the Microstructure and Solidification Behavior of Dilute Al-Mg-Si-Fe Alloys
    Jin, Dong
    Li, Hongying
    Yang, Changlong
    Han, Yu
    Zhu, Zhixiang
    Miao, Yaojun
    Xu, Chao
    Chen, Baoan
    JOM, 2023, 75 (11) : 4845 - 4857
  • [35] Corrosion behavior of a Co-Cr-Mo-Si alloy in pure Al and Al-Si melt
    Yamanaka, Kenta
    Mori, Manami
    Yoshida, Kazuo
    Tunthawiroon, Phacharaphon
    Chiba, Akihiko
    HIGH TEMPERATURE MATERIALS AND PROCESSES, 2023, 42 (01)
  • [36] Microstructure Solidification Maps for Al-10 Wt Pct Si Alloys
    Hearn, William
    Bogno, Abdoul-Aziz
    Spinelli, Jose
    Valloton, Jonas
    Henein, Hani
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2019, 50A (03): : 1333 - 1345
  • [37] 3D characteristics and growth behavior of Fe-rich phases in Al-Si-Fe-Mn alloys during melt holding
    Song, Dong-fu
    Zhao, Yu-liang
    Jia, Yi-wang
    Li, Xin-tao
    Zhou, Nan
    Zheng, Kai-hong
    Zhang, Wei-wen
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2024, 34 (06) : 1745 - 1758
  • [38] STRUCTURAL CHARACTERISTICS OF Ni-Al-Mo BASED ALLOYS
    Malcharczikova, Jitka
    Kursa, Miroslav
    Pohludka, Martin
    Kohut, Pavel
    METAL 2015: 24TH INTERNATIONAL CONFERENCE ON METALLURGY AND MATERIALS, 2015, : 1576 - 1581
  • [39] Effects of Sr on Fe-rich intermetallics in recycled Al-Si-Cu alloys
    Li, Quan
    Wang, Junsheng
    Xue, Chengpeng
    Miao, Yisheng
    Hou, Qinghuai
    Yang, Xinghai
    Meng, Yanan
    Yang, Zhihao
    Tian, Guangyuan
    Su, Hui
    Li, Xingxing
    JOURNAL OF MATERIALS SCIENCE, 2024, 59 (25) : 11572 - 11595
  • [40] PREPARATION OF FE-AL-SI ALLOYS BY REACTIVE SINTERING
    Novak, Pavel
    Knotek, Vitezslav
    Serak, Jan
    Vojtech, Dalibor
    Michalcova, Alena
    METAL 2009, CONFERENCE PROCEEDINGS, 2009, : 338 - 343