The fracture behaviour of nanostructure added adhesives under ambient temperature and thermal cyclic conditions

被引:38
作者
Kanar, Belin [1 ]
Akpinar, Salih [1 ]
Akpinar, Iclal Avinc
Akbulut, Hamit [2 ]
Ozel, Adnan [3 ]
机构
[1] Erzurum Tech Univ, Dept Mech Engn, TR-25050 Erzurum, Turkey
[2] Ataturk Univ, Dept Mech Engn, TR-25240 Erzurum, Turkey
[3] Erzincan Univ, Dept Mech Engn, TR-24100 Erzincan, Turkey
关键词
Nanocomposites; Adhesive joints; Fracture mechanics; Numerical modelling; Double cantilever beam test; SINGLE-LAP JOINTS; COHESIVE ZONE MODELS; BONDED JOINTS; CARBON NANOTUBES; NANOPARTICLES; STRENGTH; FAILURE;
D O I
10.1016/j.tafmec.2018.08.006
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
In this study, the fracture behavior of nanocomposite adhesives produced by adding nanostructure in to the adhesives were investigated using Double Cantilever Beam (DCB) test under ambient temperature and thermal cycle conditions. Adhesively bonded DCB joints were produced using DP460 toughened adhesive type and DP125 flexible adhesive type as the adhesives; AA2024-T3 aluminum alloy was used as the adherend, and 1 wt. % Graphene-COOH, Carbon Nanotube-COOH and Fullerene C60 were used as the added nanostructures. As a result, when the experimental fracture energy was examined, the nanocomposite adhesives obtained by adding nanostructure were found to have increased the fracture energy of the joint. In the joints bonded with the flexible DP125 adhesive that were subjected to thermal cycles, the addition of Graphene-COON into the adhesive increases the fracture energy of the joint by 55%, the addition of Fullerene increases the fracture energy of the joint by 135%. Also, it was observed that there is a significant difference between the displacements that were obtained directly from the test machines stroke and measured via video extensometer giving the crack opening between the top and bottom adherends during the DCB test. This situation significantly effects the correct calculation of the fracture energy of adhesive.
引用
收藏
页码:120 / 130
页数:11
相关论文
共 36 条
[31]   Finite-thickness cohesive elements for modeling thick adhesives [J].
Sarrado, Carlos ;
Leone, Frank A. ;
Turon, Albert .
ENGINEERING FRACTURE MECHANICS, 2016, 168 :105-113
[32]   Experimental study of the Mode I adhesive fracture energy in DCB specimens bonded with a polyurethane adhesive [J].
Sekiguchi, Yu ;
Katano, Masato ;
Sato, Chiaki .
JOURNAL OF ADHESION, 2017, 93 (03) :235-255
[33]   Effect of carbon nanotubes on the strength of adhesive lap joints of C/C and C/C-SiC ceramic fibre composites [J].
Srivastava, V. K. .
INTERNATIONAL JOURNAL OF ADHESION AND ADHESIVES, 2011, 31 (06) :486-489
[34]   Numerical investigation on the loading-delamination-unloading behavior of adhesive joints [J].
Xu, Qiang ;
Nian, Guodong ;
Shan, Yejie ;
Qu, Shaoxing ;
Peng, Hua-Xin .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2016, 90 :45-50
[35]   The effect of nanoparticles on the adhesion of epoxy adhesive [J].
Zhai, Lanlan ;
Ling, Guoping ;
Li, Jian ;
Wang, Youwen .
MATERIALS LETTERS, 2006, 60 (25-26) :3031-3033
[36]  
Zhengwen J., 2016, ENG FRACT MECH, V164, P49