Mechanical Performance of Heat Treated Ti-6Al-4V Friction Stir Welds

被引:10
作者
Edwards, Paul [1 ,2 ]
Petersen, Marc [2 ]
Ramulu, M. [1 ]
Boyer, R. [2 ]
机构
[1] Boeing Co, POB 3707,MC 5K-63, Seattle, WA 98124 USA
[2] Univ Washington, Dept Mech Engn, Seattle, WA 98195 USA
来源
COST-AFFORDABLE TITANIUM III | 2010年 / 436卷
关键词
Friction stir welding; titanium; microstructure; heat treatments; fatigue; tensile; fracture toughness; crack growth; FATIGUE-CRACK GROWTH;
D O I
10.4028/www.scientific.net/KEM.436.213
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Heat treatment processes for standard fusion welding techniques in titanium are well established, but the optimal heat treatment for Friction Stir Welded titanium has not been evaluated. In this study, 6 mm thickness titanium 6Al-4V butt welds were subjected to heat treatments ranging from 700 to 900 C. Results of the metallographic analysis for each heat treatment condition will be presented in addition to microhardness, tensile and fatigue properties. It was found that increased heat treatment temperatures lead to lower hardness and tensile strengths, higher elongation to failure and improved high cycle fatigue performance. Furthermore, fracture toughness and crack growth tests were performed for welds subjected to a standard post-weld stress relief. The fracture toughness was lower than the parent material, but crack growth rates in the weld were similar to that of the base metal.
引用
收藏
页码:213 / +
页数:2
相关论文
共 8 条
[1]   Effect of process conditions on superplastic forming behaviour in Ti-6Al-4V friction stir welds [J].
Edwards, P. ;
Ramulu, M. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2009, 14 (07) :669-680
[2]   Investigation of microstructure, surface and subsurface characteristics in titanium alloy friction stir welds of varied thicknesses [J].
Edwards, P. D. ;
Ramulu, M. .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2009, 14 (05) :476-483
[3]   Residual stress effects on near-threshold fatigue crack growth in friction stir welds in aerospace alloys [J].
John, R ;
Jata, KV ;
Sadananda, K .
INTERNATIONAL JOURNAL OF FATIGUE, 2003, 25 (9-11) :939-948
[4]  
Lienert T.J., 2007, Friction Stir Welding and Processing, P123
[5]   Residual stress effects on fatigue crack growth in a Ti-6Al-4V friction stir weld [J].
Pasta, S. ;
Reynolds, A. P. .
FATIGUE & FRACTURE OF ENGINEERING MATERIALS & STRUCTURES, 2008, 31 (07) :569-580
[6]  
SANDERS D, 2008, AEROMAT C AUST TX JU
[7]   Characterization of superplastically formed friction stir weld in titanium 6AL-4V: Preliminary results [J].
Sanders, D. G. ;
Ramulu, M. ;
Klock-McCook, E. J. ;
Edwards, P. D. ;
Reynolds, A. P. ;
Trapp, T. .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2008, 17 (02) :187-192
[8]   Microstructural characteristics and mechanical properties of Ti-6Al-4V friction stir welds [J].
Zhang, Yu ;
Sato, Yutaka S. ;
Kokawa, Hiroyuki ;
Park, Seung Hwan C. ;
Hirano, Satoshi .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 485 (1-2) :448-455