共 20 条
[1]
INTERGRANULAR FRACTURE IN 4340-TYPE STEELS - EFFECTS OF IMPURITIES AND HYDROGEN
[J].
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1978, 9 (02)
:237-247
[3]
THERMAL-ANALYSIS OF TRAPPED HYDROGEN IN PURE IRON
[J].
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1982, 13 (01)
:135-140
[4]
Kimura Y, 2000, ULTRAFINE GRAINED MATERIALS, P277
[5]
Work-hardening mechanism during super-heavy plastic deformation in mechanically milled iron powder
[J].
MATERIALS TRANSACTIONS JIM,
1999, 40 (10)
:1149-1157
[6]
KIMURA Y, 1998, P 1998 PM WORLD C NA, P573
[7]
Kimura Y., 2000, ISIJ INT, V40, pS174
[8]
GRAIN-SIZE EFFECTS IN HYDROGEN-ASSISTED CRACKING
[J].
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1976, 7 (07)
:953-960
[9]
Matsuyama S., 1972, TETSU TO HAGANE, V58, P395
[10]
HYDROGEN INDUCED CRACKING IN A LOW-ALLOY STEEL
[J].
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE,
1983, 14 (11)
:2347-2356