Correlating capacity fading and structural changes in Li1+yMn2-yO4-δ spinel cathode materials -: A systematic study on the effects of Li/Mn ratio and oxygen deficiency

被引:211
作者
Xia, YY [1 ]
Sakai, T
Fujieda, T
Yang, XQ
Sun, X
Ma, ZF
McBreen, J
Yoshio, M
机构
[1] Osaka Natl Res Inst, Battery Sect, Osaka 5638577, Japan
[2] Brookhaven Natl Lab, Upton, NY 11973 USA
[3] Saga Univ, Dept Appl Chem, Saga 8408502, Japan
关键词
D O I
10.1149/1.1376117
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Several series of Li1+/-yMn2O4+/-delta samples with the spinel structure were synthesized. These samples had different Li/Mn ratios (by varying the Li/Mn ratio used in stirling materials) and various oxygen contents (by controlling synthesis conditions, including temperature, heat-treatment time, and purging gas during both the solid-state reaction and annealing). In systematic studies of charge-discharge cycling behavior and in situ X-ray diffraction (XRD) at room temperature, it was found that both the charge/ discharge profile and the structural changes during cycling are closely related to the degree of oxygen deficiency created in the synthesis process. Their effects on the capacity fading are much more important than the Li/Mn ratio or other factors. A higher degree of oxygen deficiency is accompanied with a faster fading of capacity during cycling. In cells using spinel cathodes with an oxygen deficiency. the capacity fading during cycling occurs on both the 4.2 and 4.0 V plateaus. This behavior is quite different from that found in cathodes without an oxygen deficiency, where most of the capacity fading occurs on the 4.7 V plateau region only. Our in situ XRD results indicate clearly that the capacity fading on the 4.2 V plateau is related to the phase transition between the cubic II and cubic III (lambda -MnO2) structure, while the capacity fading on the 4.0 V plateau is related to the phase transition between the cubic I and cubic II spinel structures. The effects of oxygen deficiency on the structural phase transition of Li1+/-yMn2O4+/-delta-type materials at temperatures around 10 degreesC were also studied. It was found that this phase transition is closely related to the degree of oxygen deficiency of the material. In samples with no oxygen deficiency, this phase transition disappeared. (C) 2001 The Electrochemical Society.
引用
收藏
页码:A723 / A729
页数:7
相关论文
共 22 条
  • [1] Materials' effects on the elevated and room temperature performance of C/LiMn2O4 Li-ion batteries
    Amatucci, GG
    Schmutz, CN
    Blyr, A
    Sigala, C
    Gozdz, AS
    Larcher, D
    Tarascon, JM
    [J]. JOURNAL OF POWER SOURCES, 1997, 69 (1-2) : 11 - 25
  • [2] In situ X-ray diffraction and X-ray absorption studies of high-rate lithium-ion batteries
    Balasubramanian, M
    Sun, X
    Yang, XQ
    McBreen, J
    [J]. JOURNAL OF POWER SOURCES, 2001, 92 (1-2) : 1 - 8
  • [3] Synthesis and characterization of Li1+xMn2-xO4 for Li-ion battery applications
    Gao, Y
    Dahn, JR
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (01) : 100 - 114
  • [4] IMPROVED CAPACITY RETENTION IN RECHARGEABLE 4V LITHIUM LITHIUM MANGANESE OXIDE (SPINEL) CELLS
    GUMMOW, RJ
    DEKOCK, A
    THACKERAY, MM
    [J]. SOLID STATE IONICS, 1994, 69 (01) : 59 - 67
  • [5] Dissolution of spinel oxides and capacity losses in 4V Li/LixMn2O4 coils
    Jang, DH
    Shin, YJ
    Oh, SM
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1996, 143 (07) : 2204 - 2211
  • [6] HIGH-SURFACE-AREA ELECTROMIGRATION DAMAGE FOR 3-V LI-CELL CATHODES
    KURIMOTO, H
    SUZUOKA, K
    MURAKAMI, T
    XIA, YY
    NAKAMURA, H
    YOSHIO, M
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1995, 142 (07) : 2156 - 2162
  • [7] Li GH, 1996, J ELECTROCHEM SOC, V143, P178, DOI 10.1149/1.1836405
  • [8] ELECTROCHEMISTRY OF MANGANESE-DIOXIDE IN LITHIUM NONAQUEOUS CELL .3. X-RAY DIFFRACTIONAL STUDY ON THE REDUCTION OF SPINEL-RELATED MANGANESE-DIOXIDE
    OHZUKU, T
    KITAGAWA, M
    HIRAI, T
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1990, 137 (03) : 769 - 775
  • [9] Structural phase transition of the spinel-type oxide LiMn2O4
    Oikawa, K
    Kamiyama, T
    Izumi, F
    Chakoumakos, BC
    Ikuta, H
    Wakihara, M
    Li, JQ
    Matsui, Y
    [J]. SOLID STATE IONICS, 1998, 109 (1-2) : 35 - 41
  • [10] Electronic crystallization in a lithium battery material:: Columnar ordering of electrons and holes in the spinel LiMn2O4
    Rodriguez-Carvajal, J
    Rousse, G
    Masquelier, C
    Hervieu, M
    [J]. PHYSICAL REVIEW LETTERS, 1998, 81 (21) : 4660 - 4663