Evolution of Fretting Wear Behaviors and Mechanisms of 20CrMnTi Steel after Carburizing

被引:20
作者
Tang, Jinchi [1 ,2 ]
Hu, Xiongfeng [3 ]
Lai, Fuqiang [3 ,4 ]
Guo, Xiaolong [1 ,2 ]
Qu, Shengguan [3 ]
He, Ruiliang [3 ]
Qin, Shunshun [1 ,2 ]
Li, Jianwen [1 ,2 ]
机构
[1] State Key Lab Engine Reliabil, Weifang 261061, Peoples R China
[2] Weichai Power Co Ltd, Weifang 261061, Peoples R China
[3] South China Univ Technol, Sch Mech & Automot Engn, Guangzhou 510641, Peoples R China
[4] Fuzhou Univ, Sch Mech Engn & Automat, Qishan Campus, Fuzhou 350108, Peoples R China
关键词
valvetrain; carburizing; fretting wear; 20CrMnTi steel; ELECTRONIC-STRUCTURE; FRACTURE-TOUGHNESS; FRICTION; RESISTANCE; CEMENTITE; FATIGUE; CHROMIUM; LOAD;
D O I
10.3390/met10020179
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper, the fretting wear properties of 20CrMnTi steel, a common material for a rocker bracket, was discussed for the first time after it was suffered carburizing treatment. Subsequently, the fretting wear behaviors of virgin, quenched, and carburized states were studied. The effect of loads (corresponding to different engine power output) and reciprocating frequencies (corresponding to different engine speed) on wear behaviors and mechanisms of carburized specimen were further discussed. The results showed that the coefficient of friction (CoF) and wear volume loss (WVL) of the carburized specimens were significantly lower than that of virgin and quenched states. During the wear test, the surface CoF decreased gradually with the increase of applied load, while the linear correlation trend was not observed with the increase of fretting frequency as it showed an increase first and then a decrease. It was observed that the WVL increased gradually with the increase of load and frequency. With an increase of the load, the wear mechanism gradually deteriorated from the initial adhesive wear to the mixed wear mechanism. When the load was high, the oxidative wear became more severe. However, no significant effect of frequency was observed on the wear mechanism.
引用
收藏
页数:16
相关论文
共 50 条
  • [41] Effect of carburizing and nitriding duplex treatment on the friction and wear properties of 20CrNi2Mo steel
    Chen, Jian
    Li, Shaolong
    Liang, Yilong
    Tian, Xiangyu
    Gu, Jiabao
    MATERIALS RESEARCH EXPRESS, 2023, 10 (03)
  • [42] Evolution of the Fretting Wear Damage of a Complex Phase Compound Layer for a Nitrided High-Carbon High-Chromium Steel
    Duan, Yong
    Qu, Shengguan
    Jia, Siyu
    Li, Xiaoqiang
    METALS, 2020, 10 (10) : 1 - 12
  • [43] Effect of fretting wear on very high cycle bending fatigue behaviors of FV520B steel
    Song, Ya-nan
    Wang, Hai-dou
    Xu, Bin-shi
    Xing, Zhi-guo
    TRIBOLOGY INTERNATIONAL, 2016, 103 : 132 - 138
  • [44] Wear mechanisms in oil-lubricated and dry fretting of silicon nitride against bearing steel contacts
    Kalin, M
    Vizintin, J
    Novak, S
    Drazic, G
    WEAR, 1997, 210 (1-2) : 27 - 38
  • [45] Comparative tribological performance of a-C:H, ta-C and AlCrSiN coatings on 20CrMnTi gear steel under dry sliding condition
    Lei, Zonglin
    Li, Zunge
    Xiao, Yangyi
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2023, 75 (10) : 1125 - 1137
  • [46] Evolution of wear damage in Inconel 600 alloy due to fretting against type 304 stainless steel
    Li, J.
    Ma, M.
    Lu, Y. H.
    Xin, L.
    WEAR, 2016, 346 : 15 - 21
  • [47] Evolution of wear damage in gross sliding fretting of a nitrided high-carbon high-chromium steel
    Duan, Yong
    Qu, Shengguan
    Jia, Siyu
    Li, Xiaoqiang
    WEAR, 2021, 464
  • [48] Evolution of wear damage in 690 alloy tube mated with 405 stainless steel plate due to fretting conditions
    Tang, Pan
    Mi, Xue
    Zhang, Jun
    Xiong, Fu-rui
    Zheng, Bin
    Shao, Xue-jiao
    Peng, Jin-fang
    Zhu, Min-hao
    TRIBOLOGY INTERNATIONAL, 2021, 163
  • [49] Effect of carbonitride on the friction and wear properties of M50NiL steel after sequential carburizing and nitriding treatment
    Zeng, Guangwei
    Liang, Yilong
    Li, Shaolong
    Sun, Yuguan
    Wang, Peng
    MATERIALS TODAY COMMUNICATIONS, 2024, 41
  • [50] Fretting wear rate evolution of a flat-on-flat low alloyed steel contact: A weighted friction energy formulation
    Baydoun, Soha
    Fouvry, Siegfried
    Descartes, Sylvie
    Arnaud, Pierre
    WEAR, 2019, 426 : 676 - 693