Microstructural and Mechanical Behaviors of Friction Stir Welded Dissimilar AA6082-AA7075 Joints

被引:24
|
作者
Sezhian, M. Vetrivel [1 ]
Giridharan, K. [1 ]
Pushpanathan, D. Peter [1 ]
Chakravarthi, G. [1 ]
Stalin, B. [2 ]
Karthick, Alagar [3 ]
Kumar, P. Manoj [4 ]
Bharani, Murugesan [5 ]
机构
[1] Easwari Engn Coll, Dept Mech Engn, Chennai 600089, Tamil Nadu, India
[2] Anna Univ, Dept Mech Engn, Reg Campus Madurai, Madurai 625019, Tamil Nadu, India
[3] KPR Inst Engn & Technol, Dept Elect & Elect Engn, Coimbatore 641407, Tamil Nadu, India
[4] KPR Inst Engn & Technol, Dept Mech Engn, Coimbatore 641407, Tamil Nadu, India
[5] Wollo Univ, Sch Text Leather & Fash Technol, Kombolcha Inst Technol, Kombolcha 208, South Wollo, Ethiopia
关键词
TOOL ROTATIONAL SPEED; ALUMINUM-ALLOY; STRENGTH; PROFILE;
D O I
10.1155/2021/4113895
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this research, microstructural events and mechanical behaviors in dissimilar friction stir welding (FSW) of aluminium (Al) alloy AA6082-AA7075 joints have been evaluated to apply aerospace, defense, and military sectors. FSW parametric effects have a more significant impact on the mechanical performances and microstructure of produced joints. FSW tool rotational speed, welding speed, and tool plunge speed were chosen to make the weld joints. The rotational tool speeds of 1600 rpm and 2300 rpm, welding speeds of 40 mm/min and 60 mm/min, and tool plunge speeds of 20 mm/min and 30 mm/min were set as the upper and lower limits. A constant axial force of 5 kN was maintained throughout the joint fabrication process. A taper pin-profiled tool was utilized to produce the butt welded joints. Mechanical properties of microhardness, tensile strength, yield strength, elongation, and bending strength of the joints were analyzed. The response of the stir zone microstructure to processing parameters was evaluated using optical microscopy (OM) and fractographic analysis of a tensile specimen shown by scanning electron microscope (SEM). The weld joints produced at 2300 rpm, tool traveling rate of 40 mm/min, and tool plunge speed of 30 mm/min showed the greatest tensile strength of the 191 MPa hardness of 145 Hv at the weld center and also the maximum bending strength of 114.23 N/mm(2) was achieved. The lowest bending strength of 25.38 N/mm(2) was obtained at 1600 rpm with 60 mm/min due to inappropriate mixing of the base metals and poor joint quality. Furthermore, this study revealed that a higher tool plunge speed facilitates the formation of equiaxed grains in the thermomechanically affected zone (TMAZ) on the advancing side (AS). Additionally, the increment in tool rotational speed significantly improved the tensile strength, weld joint quality, and joint efficiency.
引用
收藏
页数:13
相关论文
共 50 条
  • [21] Texture-Induced Corrosion Resistance of Dissimilar AA7204/AA6082 Friction Stir Welded Joints
    Guan, Liqun
    Yuan, Manfa
    Zhang, Jin
    Deng, Yunlai
    Xu, Xuehong
    Wan, Li
    MATERIALS, 2023, 16 (18)
  • [22] Effect of in-process cooling on microstructure and mechanical properties of dissimilar AA2014 and AA7075 friction stir welded joints
    Kumar, Raj
    Upadhyay, Vikas
    Misra, Joy P.
    Sharma, Chaitanya
    PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART C-JOURNAL OF MECHANICAL ENGINEERING SCIENCE, 2022, 236 (20) : 10496 - 10507
  • [23] Grey relational analysis of friction stir welding parameters for the development of dissimilar joints between AA6082 and AA7075
    Ramakrishna, M. V. A.
    Srinivas, K.
    ADVANCES IN MATERIALS AND PROCESSING TECHNOLOGIES, 2022, 8 : 954 - 965
  • [24] INFLUENCE OF POST-WELDING HEAT TREATMENT ON MECHANICAL AND MICROSTRUCTURAL BEHAVIOR OF FRICTION STIR WELDED AA7075-T651 AND AA6061 DISSIMILAR JOINTS
    Yuvaraj, K. P.
    Varthanan, P. Ashoka
    Boopathiraja, K. P.
    HIGH TEMPERATURE MATERIAL PROCESSES, 2018, 22 (01): : 17 - 34
  • [25] Defects Morphology in the Dissimilar Friction Stir Welded T-lap Joints of AA7075 and AA5083
    Duong Dinh Hao
    Okazaki, Masakazu
    Tran Hung Tra
    Quach Hoai Nam
    ADVANCES IN ENGINEERING RESEARCH AND APPLICATION, 2019, 63 : 210 - 216
  • [26] Mechanical and Microstructural Characterisation of Dissimilar Friction Stir Welded AA2024-T3 and AA7075-T6 Aluminium Alloys
    da Silva, A. A. M.
    Aldanondo, E.
    Alvarez, P.
    Lizarralde, A.
    Echeverria, A.
    THERMEC 2009, PTS 1-4, 2010, 638-642 : 1221 - 1226
  • [27] Optimization of Tensile and Corrosion Properties of Dissimilar Friction Stir Welded AA2024-7075 Joints
    Zhang, Chenghang
    Huang, Guangjie
    Cao, Yu
    Wu, Xiaodong
    Huang, Xinde
    Liu, Qing
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2019, 28 (01) : 183 - 199
  • [28] Optimization of Tensile and Corrosion Properties of Dissimilar Friction Stir Welded AA2024-7075 Joints
    Chenghang Zhang
    Guangjie Huang
    Yu Cao
    Xiaodong Wu
    Xinde Huang
    Qing Liu
    Journal of Materials Engineering and Performance, 2019, 28 : 183 - 199
  • [29] Effect of tool probe geometry on the material flow and mechanical behaviour of dissimilar AA2024/AA7075 friction stir welded joints
    B. Nikhil
    P. Govindan
    International Journal on Interactive Design and Manufacturing (IJIDeM), 2024, 18 : 1645 - 1664
  • [30] Microstructure and mechanical properties of friction stir welded dissimilar aluminum joints of AA2024-T3 and AA7075-T6
    Khodir, Saad Ahmed
    Shibayanagi, Toshiya
    MATERIALS TRANSACTIONS, 2007, 48 (07) : 1928 - 1937