Surface SiO2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

被引:42
|
作者
Schnabel, Manuel [1 ]
Harvey, Steven P. [1 ]
Arca, Elisabetta [1 ,2 ]
Stetson, Caleb [1 ]
Teeter, Glenn [1 ]
Ban, Chunmei [1 ]
Stradins, Paul [1 ]
机构
[1] Natl Renewable Energy Lab, Golden, CO 80401 USA
[2] Lawrence Berkeley Natl Lab, Berkeley, CA 94720 USA
关键词
silicon anode; silicon oxide; lithiation; lithium ion battery; solid electrolyte interphase; pinhole; carbonate electrolyte; SOLID-ELECTROLYTE INTERPHASE; IN-SITU; THERMAL-OXIDATION; ULTRATHIN SIO2; LI; LAYER; NANOPARTICLES; PERFORMANCE; REDUCTION; CONTACTS;
D O I
10.1021/acsami.0c03158
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid-electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiOx coatings of varying thicknesses that form the true surface of the electrode. In this paper, the lithiation of SiO2-coated Si is studied in a controlled manner using SiO2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li+. Si lithiation is reversible, and SiO2 lithiation is largely irreversible. Above 2 nm SiO2, voltammetric currents decrease exponentially with SiO2 thickness. For 2-3 nm SiO2, SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO2 coating is thicker than 3-4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO2/Si interface radially outward from an existing pinhole, followed by the lithiation of SiO2 from the interface outward.
引用
收藏
页码:27017 / 27028
页数:12
相关论文
共 50 条
  • [21] Crack-Free Silicon Monoxide as Anodes for Lithium-Ion Batteries
    Lu, Wenquan
    Zhou, Xinwei
    Liu, Yuzi
    Zhu, Likun
    ACS APPLIED MATERIALS & INTERFACES, 2020, 12 (51) : 57141 - 57145
  • [22] Extreme Rate Capability Cycling of Porous Silicon Composite Anodes for Lithium-Ion Batteries
    Dhanabalan, Abirami
    Song, Botao Farren
    Biswal, Sibani Lisa
    CHEMELECTROCHEM, 2021, 8 (17) : 3318 - 3325
  • [23] Research Progress of Functional Binders in Silicon-Based Anodes for Lithium-Ion Batteries
    Zhang, Jingshuo
    Zhai, Yue
    Zhao, Ziyun
    He, Jiaxing
    Wei, Wei
    Xiao, Jing
    Wu, Shichao
    Yang, Quan-Hong
    ACTA PHYSICO-CHIMICA SINICA, 2024, 40 (06)
  • [24] Accessing the solid electrolyte interphase on silicon anodes for lithium-ion batteries in-situ through transmission soft X-ray absorption spectroscopy
    Schellenberger, M.
    Golnak, R.
    Garzon, W. G. Quevedo
    Risse, S.
    Seidel, R.
    MATERIALS TODAY ADVANCES, 2022, 14
  • [25] Exploring the practical applications of silicon anodes: a review of silicon-based composites for lithium-ion batteries
    Dong, Hong
    Wang, Jie
    Ding, Hao
    Zong, Feifei
    Wang, Peng
    Song, Ru
    Zhang, Ningshuang
    Cui, Xiaoling
    Cui, Xuchun
    Li, Shiyou
    IONICS, 2022, 28 (07) : 3057 - 3077
  • [26] Stable Cycling of SiO2 Nanotubes as High-Performance Anodes for Lithium-Ion Batteries
    Favors, Zachary
    Wang, Wei
    Bay, Hamed Hosseini
    George, Aaron
    Ozkan, Mihrimah
    Ozkan, Cengiz S.
    SCIENTIFIC REPORTS, 2014, 4
  • [27] Kinetics of Initial Lithiation of Crystalline Silicon Electrodes of Lithium-Ion Batteries
    Pharr, Matt
    Zhao, Kejie
    Wang, Xinwei
    Suo, Zhigang
    Vlassak, Joost J.
    NANO LETTERS, 2012, 12 (09) : 5039 - 5047
  • [28] Electrochemical Characteristics of Nanostructured Silicon Anodes for Lithium-Ion Batteries
    Astrova, E. V.
    Li, G. V.
    Rumyantsev, A. M.
    Zhdanov, V. V.
    SEMICONDUCTORS, 2016, 50 (02) : 276 - 283
  • [29] Overlooked challenges of interfacial chemistry upon developing high energy density silicon anodes for lithium-ion batteries
    Cai, Tao
    Wahyudi, Wandi
    Kumar, Pushpendra
    Ma, Zheng
    Sun, Qujiang
    Xie, Hongliang
    Wang, Yuqi
    Zhao, Fei
    Cao, Zhen
    Cavallo, Luigi
    Li, Qian
    Ming, Jun
    MATERIALS SCIENCE & ENGINEERING R-REPORTS, 2024, 161
  • [30] 0D-1D Hybrid Silicon Nanocomposite as Lithium-Ion Batteries Anodes
    Pinilla, Sergio
    Park, Sang-Hoon
    Fontanez, Kenneth
    Marquez, Francisco
    Nicolosi, Valeria
    Morant, Carmen
    NANOMATERIALS, 2020, 10 (03)