Surface SiO2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

被引:42
|
作者
Schnabel, Manuel [1 ]
Harvey, Steven P. [1 ]
Arca, Elisabetta [1 ,2 ]
Stetson, Caleb [1 ]
Teeter, Glenn [1 ]
Ban, Chunmei [1 ]
Stradins, Paul [1 ]
机构
[1] Natl Renewable Energy Lab, Golden, CO 80401 USA
[2] Lawrence Berkeley Natl Lab, Berkeley, CA 94720 USA
关键词
silicon anode; silicon oxide; lithiation; lithium ion battery; solid electrolyte interphase; pinhole; carbonate electrolyte; SOLID-ELECTROLYTE INTERPHASE; IN-SITU; THERMAL-OXIDATION; ULTRATHIN SIO2; LI; LAYER; NANOPARTICLES; PERFORMANCE; REDUCTION; CONTACTS;
D O I
10.1021/acsami.0c03158
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid-electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiOx coatings of varying thicknesses that form the true surface of the electrode. In this paper, the lithiation of SiO2-coated Si is studied in a controlled manner using SiO2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li+. Si lithiation is reversible, and SiO2 lithiation is largely irreversible. Above 2 nm SiO2, voltammetric currents decrease exponentially with SiO2 thickness. For 2-3 nm SiO2, SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO2 coating is thicker than 3-4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO2/Si interface radially outward from an existing pinhole, followed by the lithiation of SiO2 from the interface outward.
引用
收藏
页码:27017 / 27028
页数:12
相关论文
共 50 条
  • [1] Enhanced Interfacial Stability of Si Anodes for Li-Ion Batteries via Surface SiO2 Coating
    Schnabel, Manuel
    Arca, Elisabetta
    Ha, Yeyoung
    Stetson, Caleb
    Teeter, Glenn
    Han, Sang-Don
    Stradins, Paul
    ACS APPLIED ENERGY MATERIALS, 2020, 3 (09) : 8842 - 8849
  • [2] Surface-modified silicon nanowire anodes for lithium-ion batteries
    Xu, Wanli
    Vegunta, Sri Sai S.
    Flake, John C.
    JOURNAL OF POWER SOURCES, 2011, 196 (20) : 8583 - 8589
  • [3] Lithiation Behavior of Silicon Nanowire Anodes for Lithium-Ion Batteries: Impact of Functionalization and Porosity
    Schmerling, Marcus
    Fenske, Daniela
    Peters, Fabian
    Schwenzel, Julian
    Busse, Matthias
    CHEMPHYSCHEM, 2018, 19 (01) : 123 - 129
  • [4] Strategies for improving the storage performance of silicon-based anodes in lithium-ion batteries
    Tao, Wei
    Wang, Ping
    You, Ya
    Park, Kyusung
    Wang, Cao-Yu
    Li, Yong-Ke
    Cao, Fei-Fei
    Xin, Sen
    NANO RESEARCH, 2019, 12 (08) : 1739 - 1749
  • [5] Parasitic Reactions in Nanosized Silicon Anodes for Lithium-Ion Batteries
    Gao, Han
    Xiao, Lisong
    Plueme, Ingo
    Xu, Gui-Liang
    Ren, Yang
    Zuo, Xiaobing
    Liu, Yuzi
    Schulz, Christof
    Wiggers, Hartmut
    Amine, Khalil
    Chen, Zonghai
    NANO LETTERS, 2017, 17 (03) : 1512 - 1519
  • [6] The Critical Role of Fluoroethylene Carbonate in the Gassing of Silicon Anodes for Lithium-Ion Batteries
    Schiele, Alexander
    Breitung, Ben
    Hatsukade, Toru
    Berkes, Balazs B.
    Hartmann, Pascal
    Janek, Juergen
    Brezesinski, Torsten
    ACS ENERGY LETTERS, 2017, 2 (10): : 2228 - 2233
  • [7] Silicon anodes for lithium-ion batteries produced from recovered kerf powders
    Wagner, Nils Peter
    Tron, Artur
    Tolchard, Julian Richard
    Noia, Gianluigi
    Bellmann, Martin Pawel
    JOURNAL OF POWER SOURCES, 2019, 414 : 486 - 494
  • [8] 25th Anniversary Article: Understanding the Lithiation of Silicon and Other Alloying Anodes for Lithium-Ion Batteries
    McDowell, Matthew T.
    Lee, Seok Woo
    Nix, William D.
    Cui, Yi
    ADVANCED MATERIALS, 2013, 25 (36) : 4966 - 4984
  • [9] Insights on microstructural evolution and capacity fade on diatom SiO2 anodes for lithium-ion batteries
    Hua, Weicheng
    Nylund, Inger-Emma
    Cova, Federico
    Svensson, Ann Mari
    Blanco, Maria Valeria
    SCIENTIFIC REPORTS, 2023, 13 (01):
  • [10] SiO2/C Composite Derived from Rice Husks with Enhanced Capacity as Anodes for Lithium-Ion Batteries
    Feng, Yi
    Liu, Xiaoyang
    Liu, Li
    Zhang, Ziqing
    Teng, Yifei
    Yu, Deyang
    Sui, Jiayang
    Wang, Xiaofeng
    CHEMISTRYSELECT, 2018, 3 (37): : 10338 - 10344