Deposition of Boron-Doped Thin CVD Diamond Films from Methane-Triethyl Borate-Hydrogen Gas Mixture

被引:9
作者
Polushin, Nikolay Ivanovich [1 ]
Laptev, Alexander Ivanovich [1 ]
Spitsyn, Boris Vladimirovich [2 ]
Alexenko, Alexander Evgenievich [2 ]
Polyansky, Alexander Mihailovich [3 ]
Maslov, Anatoly Lvovich [1 ]
Martynova, Tatiana Vladimirovna [1 ]
机构
[1] Natl Univ Sci & Technol MISIS, Res Lab Superhard Mat, Leninsky Ave 4, Moscow 119049, Russia
[2] Russian Acad Sci, Inst Phys Chem, Leninsky Ave 31, Moscow 119991, Russia
[3] JSC NPO Energomash, Burdenko St 1, Chimki 141401, Russia
关键词
CVD process; doping; single-crystal diamond; boron; triethyl borate; thin films; boron-doped diamond; QUALITY HOMOEPITAXIAL DIAMOND; ELECTRICAL-PROPERTIES; TEMPERATURE; DIBORANE; GROWTH; GLASS;
D O I
10.3390/pr8060666
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Boron-doped diamond is a promising semiconductor material that can be used as a sensor and in power electronics. Currently, researchers have obtained thin boron-doped diamond layers due to low film growth rates (2-10 mu m/h), with polycrystalline diamond growth on the front and edge planes of thicker crystals, inhomogeneous properties in the growing crystal's volume, and the presence of different structural defects. One way to reduce structural imperfection is the specification of optimal synthesis conditions, as well as surface etching, to remove diamond polycrystals. Etching can be carried out using various gas compositions, but this operation is conducted with the interruption of the diamond deposition process; therefore, inhomogeneity in the diamond structure appears. The solution to this problem is etching in the process of diamond deposition. To realize this in the present work, we used triethyl borate as a boron-containing substance in the process of boron-doped diamond chemical vapor deposition. Due to the oxygen atoms in the triethyl borate molecule, it became possible to carry out an experiment on simultaneous boron-doped diamond deposition and growing surface etching without the requirement of process interruption for other operations. As a result of the experiments, we obtain highly boron-doped monocrystalline diamond layers with a thickness of about 8 mu m and a boron content of 2.9%. Defects in the form of diamond polycrystals were not detected on the surface and around the periphery of the plate.
引用
收藏
页数:13
相关论文
共 50 条
[31]   Heat resistance properties of various boron-doped diamond films prepared via hot filament chemical vapor deposition [J].
Bae, Mun Ki ;
Kim, Chi Hwan ;
Park, Yeong Min ;
Yoon, Su Jong ;
Kim, Tae Gyu .
MODERN PHYSICS LETTERS B, 2020, 34 (7-9)
[32]   Preparation of grain size controlled boron-doped diamond thin films and their applications in selective detection of glucose in basic solutions [J].
Zhao JianWen ;
Wang JinLiang ;
Zhi JinFang ;
Zhang ZhiMing .
SCIENCE CHINA-CHEMISTRY, 2010, 53 (06) :1378-1384
[33]   Growth of boron-doped diamond-like carbon films from a low-pressure high-density plasma in inductively coupled chemical vapour deposition [J].
Saha, Sucharita ;
Das, Debajyoti .
THIN SOLID FILMS, 2024, 797
[34]   CONDUCTION PROCESSES IN BORON-DOPED AND NITROGEN-DOPED DIAMOND-LIKE CARBON-FILMS PREPARED BY MASS-SEPARATED ION-BEAM DEPOSITION [J].
RONNING, C ;
GRIESMEIER, U ;
GROSS, M ;
HOFSASS, HC ;
DOWNING, RG ;
LAMAZE, GP .
DIAMOND AND RELATED MATERIALS, 1995, 4 (5-6) :666-672
[35]   Growth Rate and Electrochemical Properties of Boron-Doped Diamond Films Prepared by Hot-Filament Chemical Vapor Deposition Methods [J].
Nagasaka, Hiroshi ;
Teranishi, Yoshikazu ;
Kondo, Yuriko ;
Miyamoto, Takeshi ;
Shimizu, Tetsuhide .
E-JOURNAL OF SURFACE SCIENCE AND NANOTECHNOLOGY, 2016, 14 :53-58
[36]   Deposition of boron-doped nanocrystalline silicon carbide thin films using H2-Ar mixed dilution for the application on thin film solar cells [J].
Liu, Jia ;
Zhang, Yongsheng ;
Fan, Zhiqiang ;
Sun, Hui ;
Shan, Feng .
NANOTECHNOLOGY, 2020, 31 (27)
[37]   Enhancing the Responsiveness of Thermoelectric Gas Sensors with Boron-Doped and Thermally Annealed SiGe Thin Films via Low-Pressure Chemical Vapor Deposition [J].
Shin, Woosuck ;
Nishibori, Maiko ;
Itoh, Toshio ;
Izu, Noriya ;
Matsubara, Ichiro .
SENSORS, 2024, 24 (10)
[38]   Effective electrochemical uranium extraction from aqueous solution using boron-doped diamond films as a sustainable electrode [J].
Liu, Jia ;
Deng, Hao ;
Zhang, Jiqiao ;
Lin, Xu ;
Liu, Huiqiang ;
Yang, Wanlin ;
Jiang, Long ;
Yin, Jing ;
Chen, Yanyan ;
Wang, Bing ;
Zhang, Shengdong ;
Xiong, Ying .
SEPARATION AND PURIFICATION TECHNOLOGY, 2025, 367
[39]   Improvement of morphology and electrical properties of boron-doped diamond films via seeding with HPHT nanodiamonds synthesized from 9-borabicyclononane [J].
Stehlik, Stepan ;
Potocky, Stepan ;
Dragounova, Katerina Aubrechtova ;
Belsky, Petr ;
Medlin, Rostislav ;
Vincze, Andrej ;
Ekimov, Evgeny A. ;
Kromka, Alexander .
DIAMOND AND RELATED MATERIALS, 2025, 154
[40]   Surface morphology and electrical properties of boron-doped diamond films synthesized by microwave-assisted chemical vapor deposition using trimethylboron on diamond (100) substrate [J].
Tsubota, T ;
Fukui, T ;
Saito, T ;
Kusakabe, K ;
Morooka, S ;
Maeda, H .
DIAMOND AND RELATED MATERIALS, 2000, 9 (07) :1362-1368