Al2O3-TiO2 composite oxide films on etched aluminum foil fabricated by electrodeposition and anodization

被引:12
作者
Bu JunFu [1 ]
Sun Lan [1 ]
Wu Qi [1 ]
Wang MengYe [1 ]
Lin ChangJian [1 ,2 ]
机构
[1] Xiamen Univ, Dept Chem, Coll Chem & Chem Engn, Xiamen 361005, Peoples R China
[2] Xiamen Univ, State Key Lab Phys Chem Solid Surfaces, Xiamen 361005, Peoples R China
基金
中国国家自然科学基金;
关键词
electrodeposition; titanium oxide; composite film; aluminum electrolytic capacitor; anodization; ANODIC-DISSOLUTION; TITANIUM; PRECIPITATION; VOLTAGE;
D O I
10.1007/s11426-011-4377-9
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Ti species have been deposited on low-voltage etched aluminum foils by a simple electrochemical method using a Ti anode as Ti source in a Ti-free I-2-dissolved acetone solution. After annealing at 500-600 degrees C in air, an Al2O3-TiO2 composite oxide film was formed on the surface of the etched aluminum foil by anodizing galvanostatically in an ammonium adipate solution. The effects of I-2 concentration in the acetone solution, applied anode voltage, electrolysis time, and annealing temperature on the specific capacitance of the aluminum anode foils were investigated. The TiO2-deposited specimens prepared by applying a potential of 50 V for 3 min in 2.5 mM I-2-added acetone solution followed by annealing at 550 degrees C after anodization exhibited the highest specific capacitance, with an enhancement of 22% compared with pure etched aluminum foil specimens. The electro-deposition process and the change of the anode voltage during the anodization were analyzed.