Physical Properties of (As2Se3)1-x:Snx and (As4S3Se3)1-x:Snx Glasses

被引:0
作者
Iaseniuc, O. V. [1 ]
Harea, D. V. [1 ]
Harea, E. E. [1 ]
Volodina, G. F. [1 ]
Iovu, M. S. [1 ]
机构
[1] Moldavian Acad Sci, Inst Appl Phys, Acad Str 5, MD-2028 Kishinev, Moldova
来源
NANOMATERIALS FOR SECURITY | 2016年
关键词
S-SE FILMS; CHALCOGENIDE GLASSES; AMORPHOUS AS2SE3; OPTICAL-PROPERTIES; SURFACE-RELIEF; THIN-FILMS; AS-SE; RELAXATION;
D O I
10.1007/978-94-017-7593-9_10
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Experimental results on some physical and optical properties of (As2Se3)(1-x): Sn-x and (As4S3Se3)(1-x): Sn-x (x = 0 divided by 10 at %) glasses and amorphous films (d similar to 2.0 mu m) are presented. The bulk chalcogenide glasses are studied by X-ray diffraction spectroscopy and nanoindentation methods. It is established that the addition of these amounts of tin (x = 0 divided by 10 at %) does not lead to significant changes in the physical properties of the glass, such as values of stress and Young's modulus related to the modification of the density and compactness. The XRD measurements show that the Sn impurities in the (As4S3Se3)(1-x):Sn(x)do not significantly change the shape of the first sharp diffraction peak (FSDP) of the X-ray diffraction patterns either; the intensity and the position of the FSDP nonmonotonically depend on the Sn concentration. It has been found that the addition of these amounts of tin in (As4S3Se3)(1-x): Snx does not lead to significant changes in the glass physical properties, such as values of stress and Young's modulus related to the modification of the density and compactness. The study of the photoplastic effect is performed in situ, with illumination of the bulk and thin film samples during indentation as well as their indentation after illumination with a green laser (lambda = 532 nm) at a power of P = 50 mV/cm(2). The hardness is calculated from load-displacement curves by the Oliver-Pharr method. A sharp increase in hardness is registered if the tin concentration exceeds a value of 3-4% Sn. The hardness H of (As2Se3)(1-x): Sn-x films varies between 115 and 130 kg/mm(2). It is found that the hardness H of amorphous thin films is generally higher than the hardness of bulk samples with the same chemical composition. In this study, we are focused on the mechanical characteristics of high-purity As2Se3:Sn-x thin films.
引用
收藏
页码:127 / 140
页数:14
相关论文
共 38 条
[11]  
Inoue A, 2009, MAT SCI ENG A-STRUCT, V1, P304
[12]  
Inoue A, 2008, MICROSTRUCTURE TRIBO, P1
[13]  
Iovu MS, 2008, J OPTOELECTRON ADV M, V10, P862
[14]  
Iovu MS, 2007, J OPTOELECTRON ADV M, V9, P3138
[15]  
Iovu MS, 1999, PHYS STATUS SOLIDI A, V175, P615, DOI 10.1002/(SICI)1521-396X(199910)175:2<615::AID-PSSA615>3.0.CO
[16]  
2-N
[17]  
Iovu MS, 2005, J OPTOELECTRON ADV M, V7, P763
[18]   Transient photocurrents under optical bias in time-of-flight experiment with amorphous films of As2Se3:Sn and As2S3:Sb2S3 [J].
Iovu, MS ;
Shutov, SD ;
Toth, L .
PHYSICA STATUS SOLIDI B-BASIC RESEARCH, 1996, 195 (01) :149-157
[19]   Effect of Sn doping on photoconductivity in amorphous As2Se3 and AsSe films [J].
Iovu, MS ;
Shutov, SD ;
Arkhipov, VI ;
Adriaenssens, GJ .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2002, 299 :1008-1012
[20]   Relaxation of photodarkening in amorphous As-Se films doped with metals [J].
Iovu, MS ;
Shutov, SD ;
Popescu, M .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 2002, 299 :924-928