Planar dislocation structure during creep-fatigue interactions of TP347H heat-resistant austenitic steel at 600 °C

被引:21
作者
Zhou, Hongwei [1 ,2 ]
Zhang, Hongyan [1 ,2 ]
Bai, Fengmei [3 ,4 ]
Song, Meng [1 ,4 ]
Chen, Yan [1 ,2 ]
Zhang, Liqiang [3 ]
Fang, Xudong [5 ]
He, Yizhu [1 ,2 ]
机构
[1] Anhui Univ Technol, Key Lab Green Fabricat & Surface Technol Adv Met, Minist Educ, Maanshan 243002, Peoples R China
[2] Anhui Univ Technol, Sch Mat Sci & Engn, Maanshan 243002, Anhui, Peoples R China
[3] Anhui Univ Technol, Sch Met Engn, Maanshan 243002, Anhui, Peoples R China
[4] Northeastern Univ, State Key Lab Rolling & Automat, Shenyang 110189, Peoples R China
[5] Taiyuan Iron & Steel Grp Co Ltd, State Key Lab Adv Stainless Steel, Taiyuan 030003, Peoples R China
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2020年 / 779卷
基金
中国国家自然科学基金;
关键词
Heat-resistant austenitic steel; Creep-fatigue; Low cycle fatigue; Fatigue fracture mode; Planar slip structure; LOW-CYCLE FATIGUE; GRAIN-BOUNDARY CARBIDES; 316L STAINLESS-STEEL; INTERACTION BEHAVIOR; PREDICTION METHODS; DAMAGE MECHANISM; LIFE PREDICTION; DEFORMATION; EVOLUTION; PRECIPITATION;
D O I
10.1016/j.msea.2020.139141
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The low-cycle fatigue (LCF) and creep-fatigue (CF) interaction tests of TP347H austenitic stainless steel are carried out in air under a fully-reversed strain amplitude of 1.0% at 600 degrees C. A 10 min tensile dwell is applied in CF interaction testing. The influences of dwell on dislocation structures and fracture behavior have been evaluated. It is found that CF interaction life is lower than LCF one. The fatigue fracture mode changes from transgranular crack under LCF to transgranular plus intergranular fracture with tensile dwell. A lot of dislocation planar slip bands (PSBs) were found under CF interaction condition. PSB interacts with PSB of another slip system, twins, grain boundary (GB), and triangular GB. Strongly PSB-GB interaction causes stress concentration at GB, creating cavities and crack initiation, causing intergranular fracture. The stress concentration within the PSBs will also cause cracks, resulting in transgranular fracture morphology with fatigue striation.
引用
收藏
页数:11
相关论文
共 38 条
  • [31] Low cycle fatigue and creep-fatigue interaction behavior of 316L(N) stainless steel and life prediction by artificial neural network approach
    Srinivasan, VS
    Valsan, A
    Rao, KBS
    Mannan, SL
    Raj, B
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2003, 25 (12) : 1327 - 1338
  • [32] STUDY ON CREEP-FATIGUE FAILURE PREDICTION METHODS FOR TYPE-304 STAINLESS-STEEL
    TAKAHASHI, Y
    OGATA, T
    TAKE, K
    [J]. NUCLEAR ENGINEERING AND DESIGN, 1995, 153 (2-3) : 235 - 244
  • [33] Study on creep-fatigue life prediction methods for low-carbon nitrogen-controlled 316 stainless steel (316FR)
    Takahashi, Yukio
    Shibarnoto, Hiroshi
    Inoue, Kazuhiko
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2008, 238 (02) : 322 - 335
  • [34] Zhou H., 2014, J CHEM, V2014, P6, DOI DOI 10.1145/2676870.2676875
  • [35] Mechanism of Dynamic Strain Aging in a Niobium-Stabilized Austenitic Stainless Steel
    Zhou, Hongwei
    Bai, Fengmei
    Yang, Lei
    Wei, Hailian
    Chen, Yan
    Peng, Guosheng
    He, Yizhu
    [J]. METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2018, 49A (04): : 1202 - 1210
  • [36] Dependence of dynamic strain ageing on strain amplitudes during the low-cycle fatigue of TP347H austenitic stainless steel at 550 °C
    Zhou, HongWei
    He, YiZhu
    Cui, Mian
    Cen, YuWan
    Jiang, JianQing
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2013, 56 : 1 - 7
  • [37] Influence of dynamic strain aging pre-treatment on the low-cycle fatigue behavior of modified 9Cr-1Mo steel
    Zhou, HongWei
    He, YiZhu
    Zhang, Hui
    Cen, YuWan
    [J]. INTERNATIONAL JOURNAL OF FATIGUE, 2013, 47 : 83 - 89
  • [38] Precipitation behavior of type 347H heat-resistant austenitic steel during long-term high-temperature aging
    Zhou, Yinghui
    Li, Yanmo
    Liu, Yongchang
    Guo, Qianying
    Liu, Chenxi
    Yu, Liming
    Li, Chong
    Li, Huijun
    [J]. JOURNAL OF MATERIALS RESEARCH, 2015, 30 (23) : 3642 - 3652