Influence of metallic matrix on erosion-corrosion behaviour of high chromium cast irons under slurry impingement conditions

被引:11
作者
Giourntas, L. [1 ]
Brownlie, F. [1 ,2 ]
Hodgkiess, T. [1 ,3 ]
Galloway, A. M. [2 ]
机构
[1] Weir Adv Res Ctr, Glasgow, Lanark, Scotland
[2] Univ Strathclyde, Dept Mech & Aerosp Engn, Glasgow, Lanark, Scotland
[3] Univ Glasgow, Sch Engn, Glasgow, Lanark, Scotland
关键词
Erosion-corrosion; Chromium cast irons; Slurry impingement; CARBIDE VOLUME FRACTION; WEAR-RESISTANCE; ABRASION RESISTANCE; STAINLESS-STEELS; MICROSTRUCTURE; PARTICLES; TITANIUM; IMPACT; ANGLE;
D O I
10.1016/j.wear.2021.203834
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Chromium cast irons (CCI) comprise versatile materials that encompass a range of compositions and microstructures often chosen to promote good wear resistance. There are, however, issues that arise when the cast iron is required to operate in conditions where corrosion, as well as, wear is a factor. This scenario usually results in adapting the composition of the CCI in order to achieve higher chromium content in the metallic matrix and, thereby, to attain the corrosion resistance exhibited by high-Cr stainless steels. This paper comprises a comparison of the corrosive wear behaviour of an austenitic-based hypoeutectic cast iron and a martensitic-based, near-eutectic cast iron with the associated stainless steels, in a saline water under solid-liquid submerged jet conditions. A comprehensive experimental methodology has been adopted including evaluation of the behaviour of the materials in free erosion-corrosion conditions and with the application of cathodic protection. This approach has extended the understanding of the fundamental deterioration mechanisms in different hydrodynamic conditions and has highlighted the complexities of the mechanical/electrochemical interactions occurring during erosion-corrosion. An important feature is the influence of micro-galvanic interactions at phase boundaries. The impact of the findings has been discussed in terms of CCI alloy selection and corrosion control strategies.
引用
收藏
页数:12
相关论文
共 42 条
[11]   Microstructure refinement of hypereutectic high Cr cast irons using hard carbide-forming elements for improved wear resistance [J].
Chung, R. J. ;
Tang, X. ;
Li, D. Y. ;
Hinckley, B. ;
Dolman, K. .
WEAR, 2013, 301 (1-2) :695-706
[12]   Abnormal erosion-slurry velocity relationship of high chromium cast iron with high carbon concentrations [J].
Chung, R. J. ;
Tang, X. ;
Li, D. Y. ;
Hinckley, B. ;
Dolman, K. .
WEAR, 2011, 271 (9-10) :1454-1461
[13]   Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe-25wt.%Cr-4wt.%C [J].
Chung, R. J. ;
Tang, X. ;
Li, D. Y. ;
Hinckley, B. ;
Dolman, K. .
WEAR, 2009, 267 (1-4) :356-361
[14]  
Finnie I., 1958, P 3 US NAT C APPL ME, P527
[15]   THE EFFECT OF CARBIDE VOLUME FRACTION ON THE LOW STRESS ABRASION RESISTANCE OF HIGH CR-MO WHITE CAST IRONS [J].
FULCHER, JK ;
KOSEL, TH ;
FIORE, NF .
WEAR, 1983, 84 (03) :313-325
[16]   Enhanced approach of assessing the corrosive wear of engineering materials under impingement [J].
Giourntas, L. ;
Hodgkiess, T. ;
Galloway, A. M. .
WEAR, 2015, 338 :155-163
[17]   Erosion-corrosion assessment of materials for use in the resources industry [J].
Jones, M. ;
Llewellyn, R. J. .
WEAR, 2009, 267 (11) :2003-2009
[18]  
Karafyllias G., 2016, RELATIVE PERFORMANCE RELATIVE PERFORMANCE
[19]  
Karafyllias G., 2017, THESIS U STRATHCLYDE THESIS U STRATHCLYDE
[20]   The effect of low pH in erosion-corrosion resistance of high chromium cast irons and stainless steels [J].
Karafyllias, George ;
Galloway, Alexander ;
Humphries, Edward .
WEAR, 2019, 420 :79-86