Influence of metallic matrix on erosion-corrosion behaviour of high chromium cast irons under slurry impingement conditions

被引:11
作者
Giourntas, L. [1 ]
Brownlie, F. [1 ,2 ]
Hodgkiess, T. [1 ,3 ]
Galloway, A. M. [2 ]
机构
[1] Weir Adv Res Ctr, Glasgow, Lanark, Scotland
[2] Univ Strathclyde, Dept Mech & Aerosp Engn, Glasgow, Lanark, Scotland
[3] Univ Glasgow, Sch Engn, Glasgow, Lanark, Scotland
关键词
Erosion-corrosion; Chromium cast irons; Slurry impingement; CARBIDE VOLUME FRACTION; WEAR-RESISTANCE; ABRASION RESISTANCE; STAINLESS-STEELS; MICROSTRUCTURE; PARTICLES; TITANIUM; IMPACT; ANGLE;
D O I
10.1016/j.wear.2021.203834
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Chromium cast irons (CCI) comprise versatile materials that encompass a range of compositions and microstructures often chosen to promote good wear resistance. There are, however, issues that arise when the cast iron is required to operate in conditions where corrosion, as well as, wear is a factor. This scenario usually results in adapting the composition of the CCI in order to achieve higher chromium content in the metallic matrix and, thereby, to attain the corrosion resistance exhibited by high-Cr stainless steels. This paper comprises a comparison of the corrosive wear behaviour of an austenitic-based hypoeutectic cast iron and a martensitic-based, near-eutectic cast iron with the associated stainless steels, in a saline water under solid-liquid submerged jet conditions. A comprehensive experimental methodology has been adopted including evaluation of the behaviour of the materials in free erosion-corrosion conditions and with the application of cathodic protection. This approach has extended the understanding of the fundamental deterioration mechanisms in different hydrodynamic conditions and has highlighted the complexities of the mechanical/electrochemical interactions occurring during erosion-corrosion. An important feature is the influence of micro-galvanic interactions at phase boundaries. The impact of the findings has been discussed in terms of CCI alloy selection and corrosion control strategies.
引用
收藏
页数:12
相关论文
共 42 条
  • [1] Damage by indentation and single impact of hard particles on a high chromium white cast iron
    Adler, TA
    Dogan, ON
    [J]. WEAR, 1997, 203 : 257 - 266
  • [2] Effect of impingement angle on slurry erosion behaviour and mechanisms of 1017 steel and high-chromium white cast iron
    Al-Bukhaiti, M. A.
    Ahmed, S. M.
    Badran, F. M. F.
    Emara, K. M.
    [J]. WEAR, 2007, 262 (9-10) : 1187 - 1198
  • [3] [Anonymous], 2017, TRIBOLOGY FRICTION W
  • [4] Erosion-corrosion behaviour of lean duplex stainless steels in 3.5% NaCl solution
    Aribo, Sunday
    Barker, Richard
    Hu, Xinming
    Neville, Anne
    [J]. WEAR, 2013, 302 (1-2) : 1602 - 1608
  • [5] The effect of titanium on the abrasion resistance of 15Cr-3Mo white cast iron
    Arikan, MM
    Çimenoglu, H
    Kayali, ES
    [J]. WEAR, 2001, 247 (02) : 231 - 235
  • [6] Modelling the particles impingement angle to produce maximum erosion
    Ben-Ami, Y.
    Uzi, A.
    Levy, A.
    [J]. POWDER TECHNOLOGY, 2016, 301 : 1032 - 1043
  • [7] Comparison of Hot Wire TIG Stellite 6 weld cladding and lost wax cast Stellite 6 under corrosive wear conditions
    Brownlie, F.
    Anene, C.
    Hodgkiess, T.
    Pearson, A.
    Galloway, A. M.
    [J]. WEAR, 2018, 404 : 71 - 81
  • [8] Chattopadhyay R., 2001, SURFACE WEAR ANAL TR
  • [9] CHEN HX, 1993, WEAR, V166, P197
  • [10] Role of fracture toughness in impact-abrasion wear
    Chintha, A. R.
    Valtonen, K.
    Kuokkala, V-t
    Kundu, S.
    Peet, M. J.
    Bhadeshia, H. K. D. H.
    [J]. WEAR, 2019, 428 : 430 - 437