Formation and stability of 3CaO•CaCl2•12H2O

被引:33
|
作者
Shi, C [1 ]
机构
[1] CJS Technol Inc, Burlington, ON L7M 2Z2, Canada
关键词
formation; stability; X-ray diffraction; 3CaO-CaCl2 center dot 12H(2)O;
D O I
10.1016/S0008-8846(01)00576-2
中图分类号
TU [建筑科学];
学科分类号
0813 ;
摘要
Formation of 3CaO . CaCl2. 12H(2)O, which is a very unstable complex salt, in deteriorated concrete attacked by calcium chloride has been regarded as a main cause for the deterioration of cement concrete. In this study, a slurry from Ca(OH)(2)-CaCl2-H2O System was examined under different conditions. X-ray diffraction (XRD) analysis indicates that 3CaO-CaCl2. 12H(2)O cannot be detected in the original slurry, but is detected after acetone washing of the slurry. 3CaO . CaCl2. 12HO disappears when the acetone-washed sample is air-dried at 20 degreesC and 20% relative humidity. Thus, cautions should be taken during the preparation of samples during the examination of calcium chloride attacked concrete. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:1373 / 1375
页数:3
相关论文
共 50 条
  • [41] Thermodynamic modeling of solid solutions between monosulfate and monochromate 3CaO • Al2O3 • Ca[(CrO4)x(SO4)1-x] • nH2O
    Leisinger, Sabine M.
    Lothenbach, Barbara
    Le Saout, Gwenn
    Johnson, C. Annette
    CEMENT AND CONCRETE RESEARCH, 2012, 42 (01) : 158 - 165
  • [42] Modeling of H2O2 formation in PEMFCs
    Chen, Cheng
    Fuller, Thomas F.
    ELECTROCHIMICA ACTA, 2009, 54 (16) : 3984 - 3995
  • [43] CaCl2 as a Mineralizing Agent in Low-Temperature Recycling of Autoclaved Aerated Concrete: Cl-Immobilization by Formation of Chlorellestadite
    Ullrich, Angela
    Garbev, Krassimir
    Schweike, Uwe
    Koehler, Michael
    Bergfeldt, Britta
    Stemmermann, Peter
    MINERALS, 2022, 12 (09)
  • [44] A neutron diffraction study of the hydrous borate inderborite, CaMg[B3O3(OH)5]2(H2O)4•2H2O
    Gatta, G. Diego
    Cannao, Enrico
    Comboni, Davide
    Battiston, Tommaso
    Fabelo, Oscar
    AMERICAN MINERALOGIST, 2024, 109 (07) : 1258 - 1265
  • [45] Effects of pH and Nanoparticle Concentration on Al2O3–H2O Nanofluid Stability
    Khalad A. AlMuhaysh
    Antonis Sergis
    Yannis Hardalupas
    International Journal of Thermophysics, 2025, 46 (6)
  • [46] Ceramics in the K2O-CaO-SO3-P2O5 System
    Safronova, T., V
    Akhmedov, M. M.
    Shatalova, T. B.
    Tikhonova, S. A.
    Kazakova, G. K.
    RUSSIAN JOURNAL OF INORGANIC CHEMISTRY, 2021, 66 (08) : 1057 - 1066
  • [47] Effects of CaO and Fe2O3 on the Microstructure and Mechanical Properties of SiO2-CaO-MgO-Fe2O3 Ceramics from Steel Slag
    Zhao, Lihua
    Li, Yu
    Zhang, Lingling
    Cang, Daqiang
    ISIJ INTERNATIONAL, 2017, 57 (01) : 15 - 22
  • [48] Impact of CaCl 2-induced chemical pressure on the phase transition of H 2 O at high pressure
    Wei, Xinmiao
    Li, Xinyang
    Zhang, Zihan
    Liermann, Hanns-Peter
    Speziale, Sergio
    Pu, Mengqiong
    Zhang, Caizi
    Li, Ruiyu
    Yu, Hongyu
    Li, Liang
    Li, Fangfei
    Zhou, Qiang
    PHYSICAL REVIEW B, 2024, 109 (13)
  • [49] Influence of Li2O-Y2O3-SiO2 glass additive on conductivity and stability of cubic Li7La3Zr2O12
    Il'ina, E. A.
    Druzhinin, K., V
    Antonov, B. D.
    Pankratov, A. A.
    Vovkotrub, E. G.
    IONICS, 2019, 25 (11) : 5189 - 5199
  • [50] Effect of La2O3 on the viscosity and structure of CaO-SiO2(-Al2O3)-La2O3 melts
    Guo, Wentao
    Ding, Ziqi
    Wang, Jinming
    Wu, Jun
    Wang, Zhi
    MATERIALS CHEMISTRY AND PHYSICS, 2021, 266