Crystallization, glass transition, and molecular dynamics in PDMS of low molecular weights: A calorimetric and dielectric study

被引:62
作者
Klonos, Panagiotis A. [1 ]
机构
[1] Natl Tech Univ Athens, Dept Phys, Zografou Campus, Athens 15780, Greece
关键词
Polydimethylsiloxane; Polymer crystallization; Glass transition; Differential scanning calorimetry; Thermally stimulated depolarization currents; Polymer chains ordering; RIGID AMORPHOUS FRACTION; CORE-SHELL NANOCOMPOSITES; INTERFACIAL INTERACTIONS; POLYMER CRYSTALLIZATION; SEGMENTAL DYNAMICS; CARBON NANOTUBES; COLD CRYSTALLIZATION; SURFACE MODIFICATION; FUMED SILICA; POLYDIMETHYLSILOXANE;
D O I
10.1016/j.polymer.2018.11.028
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this work linear polydimethylsiloxane (PDMS) of five low molecular weights, W-m similar to 2-8 kg/mol, i.e. mainly below the entanglement threshold, is studied employing differential scanning calorimetry (DSC), thermally stimulated depolarization currents (TSDC), a special dielectric technique in the temperature domain, and broadband dielectric spectroscopy (BDS). It is shown mainly via raw data that the crystallization and glass transition for the larger W(m)s follow expected trends, however, for W-m similar to 2 k (corresponding to similar to 22 monomers/chain) crystallization is severely suppressed and slower. Moreover, it is demonstrated that upon isothermal annealing the crystalline fraction (CF) is maximized for all W(m)s with the exception of the lower one. For the latter, results indicate that during the annealing only the first stages of crystallization (nucleation, ordering of the polymer around the nuclei) take place, while the main crystallization event (formation of crystals) is recorded only upon heating, via the cold crystallization process. The suppressed crystallizability originates from the retarded nucleation. In particular for the lower W-m, the presence of large numbers of chain ends should be at the origins of hindered short range ordering of the polymer chains, as well as in relation to the difficult formation of physical crosslinks. At the same time, in TSDC and BDS uniquely for W-m similar to 2 k upon annealing and CF similar to 0, next to the relaxation peaks related with the glass transition of the bulk-like polymer (alpha and alpha(c)), an additional quite strong peak (alpha(n)(ew)) is recorded at higher temperatures. The overall characteristics of alpha(n)(ew) relaxation resemble those of PDMS chains constrained and ordered in the interfacial layer in amorphous silica/PDMS nanocomposites (alpha(int) relaxation). Thus, combing the overall results with results from the literature, it is proposed that alpha(n)(ew) is a direct recoding of retarded dynamics of the polymer chains being ordered around the crystallization nuclei or around extremely small crystals.
引用
收藏
页码:169 / 180
页数:12
相关论文
共 50 条
  • [11] Glass transition of an overcooled aluminum melt: A study in molecular dynamics
    Kolotova, L. N.
    Norman, G. E.
    Pisarev, V. V.
    RUSSIAN JOURNAL OF PHYSICAL CHEMISTRY A, 2015, 89 (05) : 802 - 806
  • [12] In situ prepared poly(DL-lactic acid)/silica nanocomposites: Study of molecular composition, thermal stability, glass transition and molecular dynamics
    Nerantzaki, Maria
    Prokopiou, Lydia
    Bikiaris, Dimitrios N.
    Patsiaoura, Dimitra
    Chrissafis, Kostantinos
    Klonos, Panagiotis
    Kyritsis, Apostolos
    Pissis, Polycarpos
    THERMOCHIMICA ACTA, 2018, 669 : 16 - 29
  • [13] Dynamics, fragility, and glass transition of low-molecular-weight linear homopolymers
    Andreozzi, L.
    Autiero, C.
    Faetti, M.
    Giordano, M.
    Zulli, F.
    PHILOSOPHICAL MAGAZINE, 2008, 88 (33-35) : 4151 - 4159
  • [14] Study on the glass transition dynamics and crystallization kinetics of molecular liquid, dimethyl phthalate, confined in Anodized Aluminum Oxide (AAO) nanopores with Atomic Layer Deposition (ALD) coatings
    Chat, Katarzyna
    Tu, Wenkang
    Unni, Aparna Beena
    Geppert-Rybczynska, Monika
    Adrjanowicz, Karolina
    JOURNAL OF MOLECULAR LIQUIDS, 2020, 311
  • [15] Morphology and molecular dynamics investigation of PDMS adsorbed on titania nanoparticles: Effects of polymer molecular weight
    Klonos, Panagiotis
    Dapei, Giorgia
    Sulym, Iryna Ya
    Zidropoulos, Spilios
    Sternik, Dariusz
    Derylo-Marczewska, Anna
    Borysenko, Mykola V.
    Gun'ko, Vladimir M.
    Kyritsis, Apostolos
    Pissis, Polycarpos
    EUROPEAN POLYMER JOURNAL, 2016, 74 : 64 - 80
  • [16] Molecular dynamics simulations on heterogeneity and percolation of epoxy nanofilm during glass transition process
    Wang, Zhikun
    Lv, Qiang
    Chen, Shenghui
    Faller, Roland
    Li, Chunling
    Sun, Shuangqing
    Hu, Songqing
    MATERIALS CHEMISTRY AND PHYSICS, 2018, 213 : 239 - 248
  • [17] Molecular dynamics, crystallization and hydration study of Poly(Propylene succinate) based Poly(Ester amide)s
    Klonos, Panagiotis A.
    Kluge, Marcel
    Robert, Tobias
    Kyritsis, Apostolos
    Bikiaris, Dimitrios N.
    POLYMER, 2020, 186 (186)
  • [18] Isothermal crystallization kinetics of poly(ethylene terephthalate)s of different molecular weights
    Zendehzaban, Mehdi
    Shamsipur, Mojtaba
    JOURNAL OF THE IRANIAN CHEMICAL SOCIETY, 2013, 10 (01) : 77 - 84
  • [19] Crystallization of polymer chains induced by graphene: Molecular dynamics study
    杨俊升
    黄多辉
    曹启龙
    李强
    王立志
    王藩侯
    Chinese Physics B, 2013, 22 (09) : 599 - 603
  • [20] Molecular dynamics simulations of the glass transition in polymer melts
    Paul, W
    POLYMER, 2004, 45 (11) : 3901 - 3905