Effect of oxidation and residual stress on mechanical properties of SiC seal coated C/SiC composite

被引:42
作者
Patel, Manish [1 ]
Kiran, M. Phani S. [1 ]
Kumari, Sweety [1 ]
Singh, Vijender [1 ]
Singh, Sarabjit [1 ]
Prasad, V. V. Bhanu [1 ]
机构
[1] Def Met Res Lab, Hyderabad 500058, Andhra Prades, India
关键词
C/SiC composite; Thermal residual stress; Oxidation; Mechanical properties; CERAMIC-MATRIX COMPOSITES; TENSILE BEHAVIOR; 2D-C/SIC COMPOSITES; ROOM-TEMPERATURE; CARBON-FIBERS; KINETICS; DESIGN; C/C; MICROSTRUCTURE; 1500-DEGREES-C;
D O I
10.1016/j.ceramint.2017.10.085
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The effect of oxidation and thermal residual stress on mechanical properties of SiC seal coated C/SiC composite at ambient temperature and high temperature were studied. The oxidation of SiC seal coated C/SiC composite at 1300 and 1500 degrees C resulted in carbon fibres burn area near through thickness micro cracks in the SiC seal coating. With the increase in exposure time, the formation of SiO2 layer in SiC matrix near carbon fibres burns area was found. Residual mechanical properties of SiC seal coated C/SiC composite after exposure in air show significant degradation. First time, a continuous measurement of Young's modulus with temperature of C/SiC composite was carried out using an impulse excitation technique. The effect of relaxation of thermal residual stress on mechanical properties was observed with the help of continuous measurement of Young's modulus as a function of temperature in an inert atmosphere.
引用
收藏
页码:1633 / 1640
页数:8
相关论文
共 34 条
  • [1] Advanced ceramic materials for high temperature applications
    Belmonte, Manuel
    [J]. ADVANCED ENGINEERING MATERIALS, 2006, 8 (08) : 693 - 703
  • [2] Design, Manufacture, and Characterization of a Carbon Fiber-Reinforced Silicon Carbide Nozzle Extension
    Breede, Fabian
    Hofmann, Severin
    Jain, Neraj
    Jemmali, Raouf
    [J]. INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2016, 13 (01) : 3 - 16
  • [3] X-ray analysis of residual stresses in C/SiC composites
    Broda, M
    Pyzalla, A
    Reimers, W
    [J]. APPLIED COMPOSITE MATERIALS, 1999, 6 (01) : 51 - 66
  • [4] Experimental study of high-temperature tensile mechanical properties of 3D needled C/C-SiC composites
    Chen, Zhen
    Fang, Guodong
    Xie, Junbo
    Liang, Jun
    [J]. MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 654 : 271 - 277
  • [5] Oxidation behavior of C-SiC composites with a Si-W coating from room temperature to 1500°C
    Cheng, LF
    Xu, YD
    Zhang, LT
    Gao, R
    [J]. CARBON, 2000, 38 (15) : 2133 - 2138
  • [6] Cheng LF, 2002, J AM CERAM SOC, V85, P989, DOI 10.1111/j.1151-2916.2002.tb00205.x
  • [7] Design, fabrication, and application of thermostructural composites (TSC) like C/C, C/SiC, and SiC/SiC composites
    Christin, F
    [J]. ADVANCED ENGINEERING MATERIALS, 2002, 4 (12) : 903 - 912
  • [8] Modeling brittle and tough stress-strain behavior in unidirectional ceramic matrix composites
    Curtin, WA
    Ahn, BK
    Takeda, N
    [J]. ACTA MATERIALIA, 1998, 46 (10) : 3409 - 3420
  • [9] Evans A. G., 1995, HIGH TEMPERATURE MEC
  • [10] THE MECHANICAL-BEHAVIOR OF CERAMIC MATRIX COMPOSITES
    EVANS, AG
    MARSHALL, DB
    [J]. ACTA METALLURGICA, 1989, 37 (10): : 2567 - 2583