Effect of electrodeposition parameters on the microstructure and properties of Cu-TiO2 nanocomposite coating

被引:11
作者
Khorashadizade, Faeze [1 ]
Saghafian, Hassan [1 ,2 ]
Rastegari, Saeed [1 ]
机构
[1] Iran Univ Sci & Technol, Sch Met & Mat Engn, Tehran, Iran
[2] Iran Univ Sci & Technol, CEHSAT, Tehran, Iran
关键词
Electrodeposition; Cu-TiO2 composite coating; Pulse plating; Wear resistance; Hardness; PULSE-REVERSE ELECTRODEPOSITION; PLATING PARAMETERS; WEAR BEHAVIOR; FRICTION;
D O I
10.1016/j.jallcom.2018.08.020
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the present research, Cu-TiO2 nanocomposite coatings were prepared via pulse plating using a copper sulfate bath with 5 g/L TiO2 nanoparticles; the process was undertaken on a steel substrate at room temperature for 60 min. Accordingly, the effects of process parameters such as duty cycle, pulse frequency, and average current density on the microstructure of the coating were investigated using scanning electron microscopy (SEM) and energy dispersive spectroscopy (EDS) analysis. Crystallite size and relative texture coefficient of the coatings were determined from X-ray diffraction (XRD) patterns. Also, microhardness and wear resistance of the coatings were measured using Vickers microhardness tester and pin-on-disk machine, respectively. Results showed that, the nanocomposite coating prepared at a duty cycle of 40%, frequency of 20 Hz and average current density of 2 A/dm(2) exhibited the highest microhardness with 1.98 wt% of TiO2 content. Co-deposition of TiO2 nanoparticles in copper coatings resulted in the modification of microstructure and variation in copper crystallite orientation, along with enhancements in microhardness and wear-resistances. The Cu-TiO 2 coating prepared under optimum conditions showed the copper crystallite size of 27 nm (40% smaller than the monolithic copper crystallite of pure copper coating) and microhardness of 180 HV (111% increase compared with pure copper coating). Also, the wear test results showed reductions in friction coefficient and wear rate as much as 33% and 50%, respectively, at the applied load of 3N compared with pure copper coating. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:98 / 107
页数:10
相关论文
共 24 条
  • [1] Allahkaram S. R., 2007, MATER DESIGN, V32, P4478
  • [2] Pulse and pulse reverse plating - Conceptual, advantages and applications
    Chandrasekar, M. S.
    Pushpavanam, Malathy
    [J]. ELECTROCHIMICA ACTA, 2008, 53 (08) : 3313 - 3322
  • [3] Eslami M., 2013, MATER DESIGN, V58, P557
  • [4] Effect of electrodeposition conditions on the properties of Cu-Si3N4 composite coatings
    Eslami, Maryam
    Saghafian, Hassan
    Golestani-fard, Farhad
    Robin, Alain
    [J]. APPLIED SURFACE SCIENCE, 2014, 300 : 129 - 140
  • [5] The influence of pulse plating parameters on structure and properties of Ni-W-TiO2 nanocomposite coatings
    Goldasteh, H.
    Rastegari, S.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2014, 259 : 393 - 400
  • [6] Effect of SiC nanoparticies on microstructure and wear behavior of Cu-Ni-W nanocrystalline coating
    Hashemi, M.
    Mirdamadi, Sh.
    Rezaie, H. R.
    [J]. ELECTROCHIMICA ACTA, 2014, 138 : 224 - 231
  • [7] Kanani N., 2004, ELECTROPLATING BASIC
  • [8] Development of electro-co-deposited Ni-TiC nano-particle reinforced nanocomposite coatings
    Karbasi, M.
    Yazdian, N.
    Vahidian, A.
    [J]. SURFACE & COATINGS TECHNOLOGY, 2012, 207 : 587 - 593
  • [9] Effects of pulse electrodeposition parameters on the properties of Ni-TiO2 nanocomposite coatings
    Lajevardi, S. A.
    Shahrabi, T.
    [J]. APPLIED SURFACE SCIENCE, 2010, 256 (22) : 6775 - 6781
  • [10] Composite electroplating of Cu-SiO2 nano particles on carbon fiber reinforced epoxy composites
    Li, Hao
    Wan, Yizao
    Liang, Hui
    Li, Xiaolei
    Huang, Yuan
    He, Fang
    [J]. APPLIED SURFACE SCIENCE, 2009, 256 (05) : 1614 - 1616