共 35 条
Microstructure and oxidation resistance of carbon/carbon composites coated with Si3N4-Si/MoSi2-SiC multi-layers by slurry coating and post heat-treatment process
被引:0
|作者:
Jeon, JH
Lai, ZH
Zhu, JC
Yin, ZD
机构:
[1] Korea Inst Machinery & Mat, Dept Mat Technol, Chang Won 641010, South Korea
[2] Harbin Inst Technol, Sch Mat Sci & Engn, Harbin 150001, Peoples R China
来源:
FUNCTIONALLY GRADED MATERIALS VII
|
2003年
/
423-4卷
关键词:
carbon/carbon composites;
multi-layer coatings;
oxidation resistance;
D O I:
10.4028/www.scientific.net/MSF.423-425.223
中图分类号:
T [工业技术];
学科分类号:
08 ;
摘要:
Si3N4-Si/MoSi2-SiC multi-coating layer was fabricated on the surface of two dimensional carbon-carbon (C/C) composites in order to improve their oxidation resistance at high temperatures. Si-6wt%Al inner layer and Si-Mo outer layer was pre-coated to C/C composites by a slurry dipping process, and then they were heat-treated at 1500degreesC for 1 hour in a vacuum and then heat-treated 1 hour in nitrogen atmosphere. Dispersed MoSi2 phase in the Si matrix and SiC interface layer between C/C composite substrate and Si/MoSi2 layer was formed by the reaction between Mo and Si and between Si and C, respectively, during heat-treatment in a vacuum. On the other hand, Si3N4 layer was formed by the reaction between liquid Si and nitrogen gas during heat-treatment in nitrogen atmosphere. The oxidation resistance of C/C composites coated with a Si3N4-Si/MoSi2-SiC multi-layer was excellent during a cyclic oxidation test at 1400degreesC up to 5 hours.
引用
收藏
页码:223 / 226
页数:4
相关论文