Impact of mechanical activation on sintering kinetics and mechanical properties of ultrafine-grained 95W-Ni-Fe tungsten heavy alloys

被引:37
作者
Chuvil'deev, V. N. [1 ]
Nokhrin, A., V [1 ]
Boldin, M. S. [1 ]
Baranov, G., V [2 ]
Sakharov, N., V [1 ]
Belov, V. Yu [2 ]
Lantsev, E. A. [1 ]
Popov, A. A. [1 ]
Melekhin, N., V [1 ]
Lopatin, Yu G. [1 ]
Blagoveshchenskiy, Yu, V [3 ]
Isaeva, N., V [3 ]
机构
[1] Lobachevsky State Univ Nizhny Novgorod, Nizhnii Novgorod, Russia
[2] Russian Fed Nucl Ctr, All Russian Res Inst Expt Phys, Sarov, Nizhny Novgorod, Russia
[3] Russian Acad Sci, AA Baykov Inst Met & Mat Sci, Moscow, Russia
关键词
Tungsten alloys; Mechanical activation; Spark plasma sintering; Diffusion; Grain boundaries; Strength; DENSIFICATION BEHAVIOR; TENSILE PROPERTIES; MICROSTRUCTURE; PHASE; BOUNDARIES; COMPOSITE; POWDERS; CONSOLIDATION; SEGREGATION; NANOPOWDERS;
D O I
10.1016/j.jallcom.2018.09.176
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
This paper is a study of sintering mechanisms, structure, and mechanical properties of ultrafine-grained 95W-Ni-Fe tungsten heavy alloys. Powder particle sizes were controlled by mechanical activation (MA) of original coarse-grained components and by addition of ultrafine particles. W-Ni-Fe alloys were obtained by sintering in hydrogen and Spark Plasma Sintering (SPS) in a vacuum. The dependence of ultrafine-grained (UFG) alloy density on sintering temperatures has been found to be non-monotonic with a maximum corresponding to the optimal sintering temperature. It has been demonstrated that the sintering activation energy of UFG alloys is significantly lower than that of coarse-grained alloys. It has been shown that the optimal SPS temperature for mechanically activated nanopowders goes down by 350-400 degrees C in comparison with the optimal sintering temperature in hydrogen for coarse-grained 95W-Ni-Fe powder composition. The reason for a lower optimal sintering temperature lies in a decreased activation energy of grain-boundary diffusion and formation of a non-equilibrium solid solution of nickel and iron in the surface layer of tungsten ci-W particles during high-energy MA. High-energy MA and SPS were used to obtain samples of UFG tungsten alloys with high mechanical properties: macro-elastic limit - up to 2250 MPa, yield stress - up to 2500 MPa. (C) 2018 Elsevier B.V. All rights reserved.
引用
收藏
页码:666 / 688
页数:23
相关论文
共 79 条
[1]  
Agte K., 1964, TUNGSTEN MOLYBDENIUM, P229
[2]   An investigation on the solid state sintering of mechanically alloyed nano-structured 90W-Ni-Fe tungsten heavy alloy [J].
Akhtar, Farid .
INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2008, 26 (03) :145-151
[3]  
[Anonymous], 1982, DEFORMATION MECH MAP
[4]  
[Anonymous], 1990, SINTERING KEY PAPERS
[5]  
Baranov G. V., 2010, THESIS, P198
[6]   Application of work-of-sintering concepts in powder metals [J].
Blaine, Deborah C. ;
Park, Seong Jin ;
Suri, Pavan ;
German, Randall M. .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2006, 37A (09) :2827-2835
[7]   SINTERING ATMOSPHERE EFFECTS ON TENSILE PROPERTIES OF HEAVY ALLOYS [J].
BOSE, A ;
GERMAN, RM .
METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (10) :2467-2476
[8]  
[Брагов Анатолий Михайлович Bragov A.M.], 2018, [Физическая мезомеханика, Fizicheskaya mezomekhanika], V21, P96, DOI 10.24411/1683-805X-2018-12010
[9]   Effect of Recovery and Recrystallization on the Hall–Petch Relation Parameters in Submicrocrystalline Metals: I. Experimental Studies [J].
Chuvil’deev V.N. ;
Nokhrin A.V. ;
Myshlyaev M.M. ;
Kopylov V.I. ;
Lopatin Y.G. ;
Melekhin N.V. ;
Piskunov A.V. ;
Bobrov A.A. ;
Pirozhnikova O.E. .
Chuvil’deev, V.N. (nokhrin@nifti.unn.ru), 2018, Pleiades journals (2018) :71-89
[10]   Study of mechanical properties and corrosive resistance of ultrafine-grained α-titanium alloy Ti-5Al-2V [J].
Chuvil'deev, V. N. ;
Kopylov, V. I. ;
Nokhrin, A. V. ;
Tryaev, P. V. ;
Kozlova, N. A. ;
Tabachkova, N. Yu. ;
Lopatin, Yu G. ;
Ershova, A. V. ;
Mikhaylov, A. S. ;
Gryaznov, M. Yu. ;
Chegurov, M. K. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 723 :354-367