Friction and wear of DLC films on 304 austenitic stainless steel in corrosive solutions

被引:29
|
作者
Yamauchi, N
Okamoto, A
Tukahara, H
Demizu, K
Ueda, N
Sone, T
Hirose, Y
机构
[1] Technol Res Inst Osaka Prefecture, Izumi, Osaka 5941157, Japan
[2] Kanazawa Univ, Dept Mat Sci & Engn, Kanazawa, Ishikawa 9201192, Japan
关键词
friction; wear; DLC; corrosion; stainless steel; plasma CVD;
D O I
10.1016/S0257-8972(03)00406-7
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Diamond-like carbon (DLC) films are well known for their high hardness, low friction and excellent wear resistance. In the present work, the friction coefficient and wear resistance of DLC films deposited on 304 austenitic stainless steel were investigated in corrosive solutions. DLC films were deposited on the substrate by the CVD method using radio frequency (13.56 MHz) plasma. A mixture of methane (CH4) and hydrogen (H-2) was used as processing gas. The CH4 concentration was varied from 20 to 100%. DLC films were subjected to friction and wear tests using a ball-on-flat surface friction apparatus in solutions of 3 mass% NaCl, 0.05 N HCl, 0.05 N H2SO4 and 0.05 N HNO3. The flat surface was oscillated against the alumina ball. In the tests performed within the corrosive solution, the friction coefficients of the DLC films and substrate were approximately 0.1 and 0.5, respectively. The DLC films deposited on the 304 substrate showed a remarkably lower volume of wear than the substrate alone. Accordingly, the DLC coating process was confirmed to be effective in decreasing the friction coefficient and improving the corrosion wear resistance of 304 in 3 mass% NaCl and acidic solutions. (C) 2003 Elsevier Science B.V All rights reserved.
引用
收藏
页码:465 / 469
页数:5
相关论文
共 50 条
  • [31] The effect of ceramic friction pairs on the tribocorrosion behavior of AISI 304 stainless steel in seawater
    Fan, Na
    Chai, Liqiang
    Wang, Peng
    Liang, Jun
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2019, 71 (06) : 779 - 786
  • [32] Friction stir processing of austenitic stainless steel cold spray coating deposited on 304L stainless steel substrate: feasibility study
    Thomas Perard
    Alexey Sova
    Hugo Robe
    Vincent Robin
    Yasser Zedan
    Philippe Bocher
    Eric Feulvarch
    The International Journal of Advanced Manufacturing Technology, 2021, 115 : 2379 - 2393
  • [33] Friction stir processing of austenitic stainless steel cold spray coating deposited on 304L stainless steel substrate: feasibility study
    Perard, Thomas
    Sova, Alexey
    Robe, Hugo
    Robin, Vincent
    Zedan, Yasser
    Bocher, Philippe
    Feulvarch, Eric
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 115 (7-8) : 2379 - 2393
  • [34] Mechanical properties of DLC coating sputter deposited on surface nanocrystallized 304 stainless steel
    Fu, T.
    Zhou, Z. F.
    Zhou, Y. M.
    Zhu, X. D.
    Zeng, Q. F.
    Wang, C. P.
    Li, K. Y.
    Lu, J.
    SURFACE & COATINGS TECHNOLOGY, 2012, 207 : 555 - 564
  • [35] Characterization of thick and soft DLC coatings deposited on plasma nitrided austenitic stainless steel
    Dalibon, Eugenia L.
    Heim, Daniel
    Forsich, Christian
    Rosenkranz, Andreas
    Guitar, M. Agustina
    Bruehl, Sonia P.
    DIAMOND AND RELATED MATERIALS, 2015, 59 : 73 - 79
  • [36] Corrosion behaviour of borided AISI 304 austenitic stainless steel
    Gunen, Ali
    Karakas, Mustafa Serdar
    Kurt, Bulent
    Calik, Adnan
    ANTI-CORROSION METHODS AND MATERIALS, 2014, 61 (02) : 112 - 118
  • [37] Wear Behavior of Harmonic Structured 304L Stainless Steel
    Prabhat K. Rai
    S. Shekhar
    M. Nakatani
    M. Ota
    S. K. Vajpai
    K. Ameyama
    K. Mondal
    Journal of Materials Engineering and Performance, 2017, 26 : 2608 - 2618
  • [38] FRICTION AND WEAR BEHAVIOUR OF BORIDED AISI 304 STAINLESS STEEL WITH NANO PARTICLE AND MICRO PARTICLE SIZE OF BORIDING AGENTS
    Gunen, A.
    Ulutan, M.
    Gok, M. S.
    Kurt, B.
    Orhan, N.
    JOURNAL OF THE BALKAN TRIBOLOGICAL ASSOCIATION, 2014, 20 (03): : 362 - 379
  • [39] Wear Behavior of Harmonic Structured 304L Stainless Steel
    Rai, Prabhat K.
    Shekhar, S.
    Nakatani, M.
    Ota, M.
    Vajpai, S. K.
    Ameyama, K.
    Mondal, K.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (06) : 2608 - 2618
  • [40] Quantitative inspection of iron contamination on 304 Austenitic stainless steel
    Cheng, Congqian
    Cao, Tieshan
    Zhao, Jie
    Song, Guanyu
    STRUCTURAL INTEGRITY IN NUCLEAR ENGINEERING, 2011, : 175 - 179