Thermal decomposition properties and compatibility of CL-20 with binders HTPB, PBAN, GAP and polyNIMMO

被引:71
作者
Golofit, T. [1 ]
Zysk, K. [1 ]
机构
[1] Warsaw Univ Technol, Fac Chem, PL-00664 Warsaw, Poland
关键词
CL-20; Binder; Compatibility; DSC; Thermal decomposition kinetics; STANAG; 4147; BONDED EXPLOSIVES; KINETICS; SYSTEMS;
D O I
10.1007/s10973-015-4418-2
中图分类号
O414.1 [热力学];
学科分类号
摘要
The compatibility of filler 2,4,6,8,10,12-hexanitro-2,4,6,8,10,12-hexaazaisowurtzitane (CL-20) with rocket propellant binders: hydroxyl-terminated polybutadiene (HTPB), butadiene-acrylonitrile-acrylic acid terpolymer (PBAN), glycidyl azide polymer (GAP) and poly(3-nitratomethyl-3-methyloxetane) (polyNIMMO), has been examined. The compatibility of the compounds has been tested in accordance with the STANAG 4147 standard and its modification consisting in the change of the heating rate. As it arises from STANAG 4147 standard criterion, CL-20 is not compatible with polyNIMMO, PBAN and GAP and possibly incompatible with HTPB. Changes of relative position of peaks between measurements performed in hermetical pans and pans with a pinhole and with different heating rate were observed. In case of polyNIMMO and HTPB, changes of measurement parameters lead to estimated compatibility change. The analysis of the thermal decomposition of CL-20 revealed that it is a two-phase process. The first phase is associated with decomposition in solid phase; the second phase is associated with decomposition of volatile intermediate products of CL-20 decomposition. Due to the complex process of decomposition of tested samples, the apparent activation energy was used for the assessment of the compatibility. The apparent activation energy of the initial phase of decomposition CL-20 and its mixtures with binders are compatible with one another within the limits of measurement error. Results of measurement of apparent activation energy do not indicate a destabilizing effect of binders on the initial phase of decomposition of CL-20.
引用
收藏
页码:1931 / 1939
页数:9
相关论文
共 21 条
[1]  
Abramov VG, 1978, FIZ GOREN VZRYVA, V14, P135, DOI [10.1007/BF00789730, DOI 10.1007/BF00789730]
[2]  
Cieslak K, 2013, NEW TRENDS RES ENERG, V1, P110
[3]  
FRIEDMAN HL, 1964, J POLYM SCI POL SYM, P183
[4]  
Janney IL, 1982, P 11 N AM THERM AN S, VII, P643
[5]   Compatibility study of 1,3,3-trinitroazetidine with some energetic components and inert materials [J].
Jizhen, L. ;
Xuezhong, F. ;
Xiping, F. ;
Fengqi, Z. ;
Rongzu, H. .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2006, 85 (03) :779-784
[6]   Kinetics of thermal decomposition of hexanitrohexaazaisowurtzitane [J].
Korsounskii, BL ;
Nedel'ko, VV ;
Chukanov, NV ;
Larikova, TS ;
Volk, F .
RUSSIAN CHEMICAL BULLETIN, 2000, 49 (05) :812-818
[7]   Thermal analysis of binary systems - Explosive - lead compound [J].
Ksiazczak, A ;
Maranda, A ;
Rosenkiewicz, D .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2000, 60 (01) :97-102
[8]   Influence of DSC measurement conditions on kinetic parameters of thermal decomposition of 2,4,6-trinitrotoluene [J].
Ksiazczak, A ;
Ksiazczak, T .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2000, 60 (01) :25-33
[9]  
Ksiazczak A, 2005, ISSUES ARMAMENT TECH, V95, P133
[10]   Thermal decomposition properties and compatibility of CL-20, NTO with silicone rubber [J].
Lee, J. -S. ;
Jaw, K. -S. .
JOURNAL OF THERMAL ANALYSIS AND CALORIMETRY, 2006, 85 (02) :463-467