Evaluation of the Taguchi method for wear behavior of Al/SiC/B4C composites

被引:32
作者
Soy, Ugur [1 ]
Ficici, Ferit [2 ]
Demir, Adem [1 ]
机构
[1] Sakarya Univ, Fac Technol, Dept Met & Mat Sci Engn, TR-54187 Sakarya, Turkey
[2] Sakarya Univ, Fac Technol, Dept Mech Engn, TR-54187 Sakarya, Turkey
关键词
Aluminum composite; wear behavior; Taguchi method; silicon carbide; boron carbide; pressure infiltration; METAL-MATRIX-COMPOSITES; DRY SLIDING WEAR; CUTTING PARAMETERS; OPTIMIZATION; FRICTION;
D O I
10.1177/0021998311410510
中图分类号
TB33 [复合材料];
学科分类号
摘要
In this study, the wear behaviors of aluminum matrix composites with an A360 matrix reinforced with silicon carbide (SiC) and boron carbide (B4C) ceramic particles using Taguchi method were investigated. Wear tests of unreinforced aluminum alloy and Al17%SiC and Al17%B4C particles reinforced aluminum composites (Al/17%SiC and Al/17%B4C, respectively) versus AISI316L stainless steel disc were carried out for a dry sliding condition in a so-called a pin-on-disc arrangement. The wear tests were realized at the sliding speeds of 0.5, 1.0, and 1.5 m s(-1) and under the loads of 10, 20, and 30 N. The obtained average specific wear rates for Al/17%B4C and Al/17%SiC composites are lower than unreinforced aluminum specific wear rate under the same test conditions. The experimental results are transformed into a signal-to-noise (S/N) ratio of using Taguchi method. Type of the material, applied load, and sliding speed exert a great effect on the specific wear rate, at 48.13%, 31.83%, and 8.77%, respectively. The estimated S/N ratio using the optimal testing parameters for specific wear rate were calculated and a good agreement was observed between the predicted and actual specific wear rate for a confidence level of 99.5%.
引用
收藏
页码:851 / 859
页数:9
相关论文
共 50 条
[31]   Effect of B4C and SiC nanoparticle reinforcement on the wear behavior and surface structure of aluminum (Al6063-T6) matrix composite [J].
Ramadoss, N. ;
Pazhanivel, K. ;
Kumar, S. Ganesh ;
Arivanandhan, M. ;
Anandan, P. .
SN APPLIED SCIENCES, 2020, 2 (05)
[32]   Synthesis of B4C and BN reinforced Al7075 hybrid composites using stir casting method [J].
Ramadoss, N. ;
Pazhanivel, K. ;
Anbuchezhiyan, G. .
JOURNAL OF MATERIALS RESEARCH AND TECHNOLOGY-JMR&T, 2020, 9 (03) :6297-6304
[33]   OPTIMIZATION OF MACHINING AA4015/B4C METAL MATRIX COMPOSITES BY TAGUCHI METHOD [J].
Thilagham, K. T. ;
Krishnamachary, P. C. ;
Saravanakumar, S. ;
Mahendran, A. ;
Kaliappan, S. ;
Soudagar, Manzoore elahi m. ;
Kannan, Sathish ;
AL Obaid, Sami ;
Alharbi, Sulaiman ali .
SURFACE REVIEW AND LETTERS, 2025, 32 (02)
[34]   Optimization of wear behaviour of hybrid Al(6061)-Al2O3-B4C composites through hybrid optimization method [J].
Gupta, P. K. ;
Gupta, M. K. .
MATERIALS PHYSICS AND MECHANICS, 2023, 51 (04) :23-37
[35]   Investigation on Dry Sliding Wear Behaviour of AlSi7Mg0.3/B4C/ZrO2 Hybrid Composites using Taguchi Method [J].
Prasa, S. Venkat ;
Venkateshwaran, N. ;
Sekar, S. ;
Rajkumar, A. ;
Duraivelu, K. .
JOURNAL OF POLYMER & COMPOSITES, 2024, 12 :S166-S177
[36]   Mechanical and microstructural analysis of Al-Al2O3/B4C hybrid composites [J].
Gupta, Pankaj K. ;
Gupta, M. K. .
PROCEEDINGS OF THE INSTITUTION OF MECHANICAL ENGINEERS PART L-JOURNAL OF MATERIALS-DESIGN AND APPLICATIONS, 2020, 234 (12) :1503-1514
[37]   Evaluation of Mechanical and Wear Properties of Al 5059/B4C/Al2O3 Hybrid Metal Matrix Composites [J].
Pranavi, Uppu ;
Reddy, Pathapalli Venkateshwar ;
Venukumar, Sarila ;
Cheepu, Muralimohan .
JOURNAL OF COMPOSITES SCIENCE, 2022, 6 (03)
[38]   Wear resistance of silicon infiltrated B4C/BN composites [J].
Jiang, Tao ;
Jin, Zhihao ;
Yang, Jianfeng ;
Qiao, Guanjun .
MATERIALS LETTERS, 2008, 62 (30) :4559-4562
[39]   Taguchi optimization of tribological properties of Al/Gr/B4C composite [J].
Sharma, Amit ;
Garg, Manish ;
Singh, Satnam .
INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2015, 67 (04) :380-388
[40]   Processing and mechanical properties of B4C reinforced Al matrix composites [J].
Topcu, I. ;
Gulsoy, H. O. ;
Kadioglu, N. ;
Gulluoglu, A. N. .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 482 (1-2) :516-521