Critical hydrogen concentration for crack propagation in a CrMo steel: Targeted experiments for accurate numerical modelling

被引:10
作者
Borja Peral, Luis [1 ]
Fernandez-Pariente, Ines [2 ]
Colombo, Chiara [3 ]
机构
[1] Univ Burgos, Higher Polytech Sch, Dept Civil Engn, Struct Integr Res Grp, Ave Cantabria S-N, Burgos 09006, Spain
[2] Univ Oviedo, Campus Gijon,East Bldg, Gijon 33203, Spain
[3] Politecn Milan, Dept Mech Engn, Via La Masa 1, I-20156 Milan, Italy
关键词
Hydrogen embrittlement; Hydrogen diffusion; CrMo steel; Crack tip; Cohesive Zone Modelling; TENSILE PROPERTIES; GASEOUS-HYDROGEN; EMBRITTLEMENT; TRANSPORT; FRACTURE; PLASTICITY; DIFFUSION; BEHAVIOR; GROWTH; GRADES;
D O I
10.1016/j.engfracmech.2022.108764
中图分类号
O3 [力学];
学科分类号
08 ; 0801 ;
摘要
This study focuses on CrMo steel experiencing decohesion mechanism in presence of hydrogen. A tailored experimental characterization is performed with tensile, permeation and toughness experimental tests to obtain all the inputs for the numerical simulations of a propagating crack in a C(T) specimen. The used finite element framework is based on the cohesive zone modelling. The aim of the numerical model and of the work is the identification of a critical hydrogen concen-tration inducing crack tip propagation. Given the tailored inputs, these models accurately esti -mate the hydrogen concentrations in the lattice and the reversible traps, and follow their redistribution along the ligament during the time. From the obtained results, we could quantify that a decrease of two orders of magnitude in the test speed reduces the critical hydrogen con-centration at the crack tip, necessary to activate the failure of the first cohesive element and therefore the propagation, from 0.994 to 0.784 wppm, that is-21%.
引用
收藏
页数:17
相关论文
共 64 条
[41]  
ORIANI RA, 1972, BERICH BUNSEN GESELL, V76, P848
[42]   Consequence of the diffusive hydrogen contents on tensile properties of martensitic steel during the desorption at room temperature [J].
Oudriss, A. ;
Fleurentin, A. ;
Courlit, G. ;
Conforto, E. ;
Berziou, C. ;
Rebere, C. ;
Cohendoz, S. ;
Sobrino, J. M. ;
Creus, J. ;
Feaugas, X. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 598 :420-428
[43]   Evaluation of hydrogen trapping and diffusion in two cold worked CrMo(V) steel grades by means of the electrochemical hydrogen permeation technique [J].
Peral, L. B. ;
Amghouz, Z. ;
Colombo, C. ;
Fernandez-Pariente, I .
THEORETICAL AND APPLIED FRACTURE MECHANICS, 2020, 110
[44]   Effect of internal hydrogen on the tensile properties of different CrMo(V) steel grades: Influence of vanadium addition on hydrogen trapping and diffusion [J].
Peral, L. B. ;
Zafra, A. ;
Fernandez-Pariente, I ;
Rodriguez, C. ;
Belzunce, J. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2020, 45 (41) :22054-22079
[45]   Effect of hydrogen on the fatigue crack growth rate of quenched and tempered CrMo and CrMoV steels [J].
Peral, L. B. ;
Zafra, A. ;
Blason, S. ;
Rodriguez, C. ;
Belzunce, J. .
INTERNATIONAL JOURNAL OF FATIGUE, 2019, 120 :201-214
[46]   Effects of hydrogen on the fracture toughness of CrMo and CrMoV steels quenched and tempered at different temperatures [J].
Peral, L. B. ;
Zafra, A. ;
Belzunce, J. ;
Rodriguez, C. .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (07) :3953-3965
[47]   The Positive Role of Nanometric Molybdenum-Vanadium Carbides in Mitigating Hydrogen Embrittlement in Structural Steels [J].
Peral, Luis Borja ;
Fernandez-Pariente, Ines ;
Colombo, Chiara ;
Rodriguez, Cristina ;
Belzunce, Javier .
MATERIALS, 2021, 14 (23)
[48]  
Pillot S, 2012, WOODHEAD PUBL MATER, P51
[49]  
Popov B.N., 2018, HDB ENV DEGRADATION, VThird, P133, DOI [10.1016/B978-0-323-52472-8.00007-1, DOI 10.1016/B978-0-323-52472-8.00007-1]
[50]   Crack propagation analysis of hydrogen embrittlement based on peridynamics [J].
Ran, Xiu ;
Qian, Songrong ;
Zhou, Ji ;
Xu, Zhengyun .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2022, 47 (14) :9045-9057