Effect of temperature on microstructure and texture evolution during uniaxial tension of commercially pure titanium

被引:32
作者
Bishoyi, B. D. [1 ]
Sabat, R. K. [2 ]
Sahu, J. [3 ]
Sahoo, S. K. [1 ]
机构
[1] NIT Rourkela, Dept Met & Mat Engn, Rourkela 769008, India
[2] IISc Bangalore, Dept Mat Engn, Bangalore 560012, Karnataka, India
[3] Indian Inst Technol, Dept Met Engn & Mat Sci, Bombay 400076, Maharashtra, India
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2017年 / 703卷
关键词
CP-titanium; Tension test; Deformation twinning; Microstructure; EBSD; MECHANICAL-PROPERTIES; DEFORMATION MECHANISMS; ALPHA-TITANIUM; CP-TI; BEHAVIOR; DEPENDENCE; ANISOTROPY; STRESS; METALS; ALLOYS;
D O I
10.1016/j.msea.2017.07.081
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Commercially pure (CP) titanium samples were subjected to uniaxial tension of 5, 15, 25, 35 and 45 elongation (%) at room temperature (298 K), 673 K and 873 K respectively. The texture and microstructure evolution as a function of temperature and elongation (%) were evaluated in the present study. The following observations were made: (i) twins of both {10 (1) over bar 2} type tensile twins and {11 (2) over bar 2} type compressive twins were significant during deformation at 298 K while at high temperatures, these twins were observed till 15 elongation (%) only; (ii) both the twins were mostly activated in the grains/orientations of high Schmid factor values, although these twins were also activated in some grains with low Schmid factor values; (iii) both grain refinement and mis-orientation developments as a function of elongation (%) was higher for the samples deformed at 298 K compared to those at 673 K and 873 K; (iv) The initial texture concentrated along (11 (2) over bar 5) < 1 <(1)over bar> 00 > was observed to be strengthened with progressive deformation irrespective of the temperature of deformation. However, the texture intensity was higher during deformation at high temperaturesd
引用
收藏
页码:399 / 412
页数:14
相关论文
共 44 条
[21]   EBSD characterization of twinning in cold-rolled CP-Ti [J].
Li, X. ;
Duan, Y. L. ;
Xu, G. F. ;
Peng, X. Y. ;
Dai, C. ;
Zhang, L. G. ;
Li, Z. .
MATERIALS CHARACTERIZATION, 2013, 84 :41-47
[22]  
Mecking H., 1977, Work hardening in tension and fatigue, P67
[23]  
Nabarro F.R.N., 1986, P INT C STRENGTH MET, P1667
[24]   Evolution of microstructure and texture in commercial pure aluminum subjected to high pressure torsion processing [J].
Naghdy, Soroosh ;
Kestens, Leo ;
Hertele, Stijn ;
Verleysen, Patricia .
MATERIALS CHARACTERIZATION, 2016, 120 :285-294
[25]   GRAIN-SIZE STRENGTHENING IN TERMS OF DISLOCATION DENSITY MEASURED BY RESISTIVITY [J].
NARUTANI, T ;
TAKAMURA, J .
ACTA METALLURGICA ET MATERIALIA, 1991, 39 (08) :2037-2049
[26]   Mechanical properties and deformation mechanisms of a commercially pure titanium [J].
Nemat-Nasser, S ;
Guo, WG ;
Cheng, JY .
ACTA MATERIALIA, 1999, 47 (13) :3705-3720
[27]   Anisotropic response of high-purity α-titanium: Experimental characterization and constitutive modeling [J].
Nixon, Michael E. ;
Cazacu, Oana ;
Lebensohn, Ricardo A. .
INTERNATIONAL JOURNAL OF PLASTICITY, 2010, 26 (04) :516-532
[28]  
Partridge P.G., 1967, METALS METALLURGY TR, V118, P169, DOI [10.1179/mtlr.1967.12.1.169, /10.1179/mtlr.1967.12.1.169, DOI 10.1179/MTLR.1967.12.1.169]
[29]   Mechanisms of anisotropy of mechanical properties of α-titanium in tension conditions [J].
Roth, A. ;
Lebyodkin, M. A. ;
Lebedkina, T. A. ;
Lecomte, J. -S. ;
Richeton, T. ;
Amouzou, K. E. K. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 596 :236-243
[30]   Texture and microstructure evolution of commercially pure titanium during hot rolling: Role of strain-paths [J].
Sahoo, S. K. ;
Sabat, R. K. ;
Sahni, S. ;
Suwas, S. .
MATERIALS & DESIGN, 2016, 91 :58-71