Impact of localized deformation on IASCC in austenitic stainless steels

被引:98
作者
Jiao, Z. [1 ]
Was, G. S. [1 ]
机构
[1] Univ Michigan, Dept Nucl Engn & Radiol Sci, Ann Arbor, MI 48109 USA
关键词
STRESS-CORROSION CRACKING; IRRADIATED MICROSTRUCTURE; INITIATION;
D O I
10.1016/j.jnucmat.2010.10.087
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Localized deformation has been identified as a potential primary contributor to IASCC. Seven austenitic alloys were irradiated to 1 and 5 dpa at 360 degrees C using 2-3.2 MeV protons and were tested both in simulated BWR environment and in argon. Cracking susceptibility was evaluated at both 1% and 3% strain intervals using crack length per unit area. Stacking fault energy (SFE), hardness, radiation-induced segregation (RIS) and localized deformation were characterized and their correlations with cracking were evaluated using a proposed term, correlation strength. Both SFE and hardness contributed to cracking but neither was the dominant factor. RIS did not play an important role in this study. The correlation strength of localized deformation with IASCC was found to be significantly higher than for others parameters, implying that localized deformation is the most important factor in IASCC. Although not well understood, localized deformation may promote cracking through intensive interaction of dislocations in slip channels with grain boundaries. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:246 / 256
页数:11
相关论文
共 50 条
[21]   Role of hydrogen in stress corrosion cracking of austenitic stainless steels [J].
Lu, B. T. ;
Qiao, L. J. ;
Luo, J. L. ;
Gao, K. W. .
PHILOSOPHICAL MAGAZINE, 2011, 91 (02) :215-235
[22]   IGSCC of non-sensitised austenitic stainless steels in BWR environment - Effect of deformation mode on grain boundary susceptibility [J].
Roychowdhury, S. ;
Kain, V. ;
Gupta, M. ;
Neogy, S. ;
Srivastava, D. ;
Dey, G. K. ;
Prasad, R. C. .
TEXTURES OF MATERIALS, PTS 1 AND 2, 2012, 702-703 :685-+
[23]   Stress corrosion cracking and life prediction evaluation of austenitic stainless steels in calcium chloride solution [J].
Leinonen, H .
CORROSION, 1996, 52 (05) :337-346
[24]   Determination of plasticity following deformation and welding of austenitic stainless steel [J].
Acar, Murat O. ;
Fitzpatrick, Michael E. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 701 :203-213
[25]   Hot Deformation Behaviors of as Cast 321 Austenitic Stainless Steel [J].
Zhao, Deli ;
Ren, Liguo ;
Wang, Yong ;
Wang, Wei ;
Zhu, Zhe ;
Fu, Wantang .
METALS, 2021, 11 (08)
[26]   Sensitization of Austenitic Stainless Steels: Current Developments, Trends, and Future Directions [J].
Srinivasan, N. .
METALLOGRAPHY MICROSTRUCTURE AND ANALYSIS, 2021, 10 (02) :133-147
[27]   Assessment of crack growth rates in austenitic stainless steels in operating BWRS [J].
Jansson, C ;
Morin, U .
PROCEEDINGS OF THE EIGHTH INTERNATIONAL SYMPOSIUM ON ENVIRONMENTAL DEGRADATION OF MATERIALS IN NUCLEAR POWER SYSTEMS - WATER REACTORS, VOLS 1 AND 2, 1997, :667-674
[28]   STRESS CORROSION CRACKING OF AUSTENITIC STAINLESS STEELS IN SIMULATED NUCLEAR REACTOR CONDITIONS [J].
Siegl, J. ;
Hausild, P. ;
Nedbal, I. ;
Novotny, R. .
NEW METHODS OF DAMAGE AND FAILURE ANALYSIS OF STRUCTURAL PARTS, 2010, 2010, :281-290
[29]   Characterization of the hot deformation microstructure of AISI 321 austenitic stainless steel [J].
Ghazani, M. Shaban ;
Eghbali, B. .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2018, 730 :380-390
[30]   Stress corrosion cracking in austenitic stainless steels: Experiments, mechanisms and numerical simulations [J].
Magnin, T ;
ChambreuilParet, A ;
Chateau, JP .
METALS MATERIALS AND PROCESSES, 1996, 8 (03) :203-210