Post examination of tungsten monoblocks subjected to high heat flux tests of ITER full-tungsten divertor qualification program

被引:38
|
作者
Sun, Zhaoxuan [1 ,2 ]
Li, Qiang [1 ]
Wang, Wanjing [1 ]
Wang, Ji-Chao [1 ,2 ]
Wang, Xingli [1 ,2 ]
Wei, Ran [1 ,2 ]
Xie, Chunyi [1 ]
Luo, Guang-nan [1 ,2 ,3 ,4 ]
Hirai, T. [5 ]
Escourbiac, F. [5 ]
Panayotis, S. [5 ]
机构
[1] Chinese Acad Sci, Inst Plasma Phys, Hefei 230031, Anhui, Peoples R China
[2] Univ Sci & Technol China, Grad Sch, Sci Isl Branch, Hefei 230031, Anhui, Peoples R China
[3] Hefei Ctr Phys Sci & Technol, Hefei 230022, Anhui, Peoples R China
[4] Chinese Acad Sci, Hefei Sci Ctr, Hefei 230027, Anhui, Peoples R China
[5] ITER Org, Route Vinon Sur Verdon,CS 90 046, F-13067 St Paul Les Durance, France
基金
中国国家自然科学基金;
关键词
ITER; Tungsten; Divertor; High heat flux; Monoblock; MOCK-UPS;
D O I
10.1016/j.fusengdes.2017.06.009
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
In 2015, as part of ITER Full-Tungsten Divertor Qualification Program, Institute of Plasma Physics Chinese Academy of Sciences (ASIPP) manufactured six small-scale Tungsten (W) monoblock mock-ups that were tested at the electron beam facility, ITER Divertor Test Facility (IDTF, St Petersburg, RF). The high heat flux (HHF) tests consisted of 5000 cycles at 10 MW/m(2), followed by 300 cycles at 20 MW/m(2) and additional 700 cycles at 20 MW/m(2). All mock-ups fulfilled the requirements of high heat flux performance successfully. One (WTC-5) of the six mock-ups was then selected to carry out critical heat flux (CHF) test with local heat flux up to 37-39 MW/m(2). After HHF test, ultrasonic test (UT) and destructive tests were performed to characterize the damages of monoblocks. The debonding of the Cu/CuCrZr interface was detected by both nondestructive and destructive tests. Intergranular rupture of W was observed by Scanning Electron Microscope (SEM). The recrystallization was found in the W monoblocks and the recrystallized depth were analyzed by metallography and Vickers hardness measurement. (C) 2017 Elsevier B.V. All rights reserved.
引用
收藏
页码:60 / 69
页数:10
相关论文
共 33 条
  • [31] Improved structural strength and lifetime of monoblock divertor targets by using doped tungsten alloys under cyclic high heat flux loading
    Nogami, S.
    Guan, W. H.
    Hattori, T.
    James, K.
    Hasegawa, A.
    PHYSICA SCRIPTA, 2017, T170
  • [32] High heat flux tests of tungsten - RAFM steel mock-up brazed by Ti-Zr-4Be alloy
    Bachurina, D. M.
    Suchkov, A. N.
    Sevryukov, O. N.
    Kirillova, V. O.
    Leontyeva-Smirnova, M. V.
    Vershinina, T. N.
    Piskarev, P. Yu.
    Ruzanov, V. V.
    Kuznetcov, V. E.
    Kolesnik, M. S.
    Mazul, I. V.
    FUSION ENGINEERING AND DESIGN, 2025, 211
  • [33] Fracture mechanical analysis of a tungsten monoblock-type plasma-facing component without macroscopic interlayer for high-heat-flux divertor target
    Li, Muyuan
    Gallay, Franklin
    Richou, Marianne
    You, Jeong-Ha
    FUSION ENGINEERING AND DESIGN, 2017, 122 : 124 - 130