High temperature corrosion resistant coatings for gas turbine components

被引:0
|
作者
Aguero, A. [1 ]
机构
[1] Inst Nacl Tecn Aeroespacial, Area Mat Met, Madrid 28850, Spain
关键词
oxidation; corrosion; coating; power generation; aeronautic; turbine;
D O I
暂无
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Hot section gas turbine components are made of superalloys, developed to withstand high temperatures in conditions in which mechanical stresses are high and that require high surface stability. However, during the 50s it became evident that compositions resulting in high mechanical strength for these materials were not compatible with those offering optimal protection from the working environments. The idea of employing protective coatings over materials with high mechanical strength resulted therefore from this situation. Presently, both aeronautic and power generation turbines operate at temperatures within the 900-1400 degrees C, thanks to these coatings, indispensable for their correct operation. In this work, the principal degradation mechanisms in these operating conditions and the different type of coatings presently employed by the industrial sector are described, beginning by the oldest Ni or Co aluminides, following with the addition of other metals such as Pt, Cr, etc. to the former coatings in order to increase their useful life, continuing with the overlay MCrAlY coatings and finishing with the thermal barrier coating systems. Moreover, the corresponding deposition techniques industrially employed to deposit these coatings are described, and finally, an insight of the latest research lines currently being developed is also included.
引用
收藏
页码:384 / 398
页数:15
相关论文
共 50 条
  • [21] Recent advances in corrosion resistant superhydrophobic coatings
    Radwan, Ahmed Bahgat
    Abdullah, Aboubakr M.
    Alnuaimi, Nasser A.
    CORROSION REVIEWS, 2018, 36 (02) : 127 - 153
  • [22] High performance corrosion resistant polyaniline/alkyd ecofriendly coatings
    Alam, Javed
    Riaz, Ufana
    Ahmad, Sharif
    CURRENT APPLIED PHYSICS, 2009, 9 (01) : 80 - 86
  • [23] Gas Turbine Aero Engine Compressor Blade Erosion and Heat Resistant Coatings
    Savkov, K.
    Doroshko, S.
    Urbaha, M.
    TRANSPORT MEANS 2011, 2011, : 274 - 278
  • [24] A survey of the literature on the use of high velocity oxy-fuel spray technology for high temperature corrosion and erosion-corrosion resistant coatings
    Kaur, Manpreet
    Singh, Harpreet
    Prakash, Satya
    ANTI-CORROSION METHODS AND MATERIALS, 2008, 55 (02) : 86 - 96
  • [25] Assessment of usability of the exploited gas turbine blade heat-resistant coatings
    Bogdan, Mariusz
    Blachnio, Jozef
    Spychala, Jaroslaw
    Zasada, Dariusz
    ENGINEERING FAILURE ANALYSIS, 2019, 105 : 337 - 346
  • [26] Study of high temperature corrosion properties about several arc sprayed coatings
    Liu, Q
    Ma, SN
    CONTRIBUTIONS OF SURFACE ENGINEERING TO MODERN MANUFACTURING AND REMANUFACTURING, 2002, : 116 - 118
  • [27] Multilayer coatings for corrosion protection of coal gasifier components
    Perez-Mariano, J.
    Lau, K. H.
    Alvarez, E.
    Malhotra, R.
    Hornbostel, M.
    Krishnan, G.
    Sanjurjo, A.
    MATERIALS CHEMISTRY AND PHYSICS, 2008, 112 (01) : 180 - 185
  • [28] Coatings for corrosion protection of porous substrates in gasifier components
    Perez-Mariano, J.
    Lau, K. H.
    Alvarez, E.
    Malhotra, R.
    Hornbostel, M.
    Krishnan, G.
    Sanjujo, A.
    SURFACE & COATINGS TECHNOLOGY, 2008, 202 (12) : 2794 - 2800
  • [29] Corrosion performance of high-temperature organic coatings subjected to heat treatments
    Wiering, Luke
    Qi, Xiaoning
    Battocchi, Dante
    PROGRESS IN ORGANIC COATINGS, 2021, 159
  • [30] EFFECT OF HIGH-TEMPERATURE CORROSION ON THE GAS-ABRASIVE RESISTANCE OF ELECTRIC-ARC COATINGS
    Student, M. M.
    Pokhmurs'ka, H. V.
    Hvozdets'kyi, V. V.
    Holovchuk, M. Ya.
    Romaniv, M. S.