Defect production in strained p-type Si1-xGex by Er implantation

被引:4
|
作者
Mamor, M. [1 ,2 ,3 ]
Pipeleers, B. [1 ,2 ]
Auret, F. D. [4 ]
Vantomme, A. [1 ,2 ]
机构
[1] Katholieke Univ Leuven, Inst Kern En Stralingsfys, B-3001 Louvain, Belgium
[2] Katholieke Univ Leuven, INPAC, B-3001 Louvain, Belgium
[3] Sultan Qaboos Univ, Dept Phys, Muscat 123, Oman
[4] Univ Pretoria, Dept Phys, ZA-0002 Pretoria, South Africa
关键词
1.54; MU-M; LIGHT-EMITTING-DIODES; ION-BEAM SYNTHESIS; SILICON-GERMANIUM; LAYER HETEROSTRUCTURES; M ELECTROLUMINESCENCE; ELECTRONIC-PROPERTIES; CRYSTALLINE SI; ERBIUM; PHOTOLUMINESCENCE;
D O I
10.1063/1.3531539
中图分类号
O59 [应用物理学];
学科分类号
摘要
Strained p-Si1-xGex (x=5.3%, 10.2%, and 15.4%) was irradiated at room temperature with 160 keV Er-166(2+) ions to a fluence of 1 x 10(10) or 3 x 10(13) Er/cm(2). The defects induced by ion implantation were investigated experimentally using high-resolution x-ray diffraction, Rutherford backscattering and channeling spectroscopy, and deep level transient spectroscopy. X-ray diffraction indicates that the damage induced by Er implantation produces a slight perpendicular expansion of the SiGe lattice. For all compositions, channeling measurements reveal that Er implantation in p-Si1-xGex to a fluence of 3 x 10(13) Er/cm(2) induces an amorphous region below the Si1-xGex surface. Annealing at 850 degrees C for 30 s, results in a reduction in damage density, a relaxation of the implantation-induced perpendicular expansion of the SiGe lattice in the implanted region, while a more pronounced relaxation of the compressive strain SiGe is observed for higher Ge content (x=0.10 and 0.15). On the other hand, for the annealed SiGe samples that were implanted with Er at the fluence of 10(10) Er/cm(2), the compressive strain in the SiGe layer is nearly completely retained. Deep level transient spectroscopy studies indicate that two prominent defects with discrete energy levels above the valence band are introduced during Er implantation. Their activation energy was found to decrease with increasing Ge content. However, the relatively large local strain induced by high fluence Er implantation reduces the activation energy by 40 meV with respect to the low fluence Er implanted p-Si1-xGex. This shift (40 meV) in the activation energy remains constant regardless of the Ge content, suggesting that the Si1-xGex layers remained fully strained after Er implantation. The observed defects are further compared to those introduced by alpha particle irradiation and electron beam metal deposition. The results indicate that defects introduced by Er implantation have similar electronic properties as those of defects detected after electron beam deposition and alpha particle irradiation. Therefore, it is concluded that these defects are due to the Er implantation-induced damage and not to the Er species specifically. (C) 2011 American Institute of Physics. [doi: 10.1063/1.3531539]
引用
收藏
页数:10
相关论文
共 50 条
  • [21] First-principles calculation of p-type alloy scattering in Si1-xGex
    Joyce, S.
    Murphy-Armando, F.
    Fahy, S.
    PHYSICAL REVIEW B, 2007, 75 (15):
  • [22] Dislocation scatterings in p-type Si1-xGex under weak electric field
    Hur, Ji-Hyun
    Jeon, Sanghun
    NANOTECHNOLOGY, 2015, 26 (49)
  • [23] Point-defect associated thermionic hole emissions from p-type Si/Si1-xGex/Si quantum well structures
    Kim, K
    Kim, HS
    Lee, HJ
    JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 1999, 3 (7-8) : 417 - 423
  • [24] Strained-Si NMOSFET on relaxed Si1-xGex formed by ion implantation of Ge
    John, S
    Ray, SK
    Oswal, SK
    Banerjee, SK
    MICROELECTRONIC DEVICE TECHNOLOGY, 1997, 3212 : 129 - 133
  • [25] Femtosecond intersubband dynamics of holes in p-type Si1-xGex/Si multiple quantum wells
    Kaindl, RA
    Wurm, M
    Reimann, K
    Woerner, M
    Efsaesser, T
    Miesner, C
    Brunner, K
    Abstreiter, G
    ULTRAFAST PHENOMENA XII, 2001, 66 : 369 - 371
  • [26] Phonon-Drag Contribution to Seebeck Coefficient in P-Type Si, Ge and Si1-xGex
    Manimuthu, Veerappan
    Omprakash, Muthusamy
    Arivanandhan, Mukannan
    Salleh, Faiz
    Hayakawa, Yasuhiro
    Ikeda, Hiroya
    IEICE TRANSACTIONS ON ELECTRONICS, 2017, E100C (05): : 482 - 485
  • [27] Hole mobility of strained Si/(001)Si1-xGex
    WANG XiaoYan1
    2 Department of Electron and Electricity Engineering
    Science China(Physics,Mechanics & Astronomy), 2012, (01) : 48 - 54
  • [28] Electron mobility of strained Si/(001) Si1-xGex
    Wang Xiao-Yan
    Zhang He-Ming
    Song Jian-Jun
    Ma Jian-Li
    Wang Guan-Yu
    An Jiu-Hua
    ACTA PHYSICA SINICA, 2011, 60 (07)
  • [29] RELAXATION OF SI/SI1-XGEX STRAINED LAYER STRUCTURES
    GIBBINGS, CJ
    TUPPEN, CG
    HALLIWELL, MAG
    HOCKLY, M
    DAVEY, ST
    LYONS, MH
    HETEROSTRUCTURES ON SILICON : ONE STEP FURTHER WITH SILICON, 1989, 160 : 121 - 128
  • [30] High electron mobility in strained Si channel of Si1-xGex/Si/Si1-xGex heterostructure with abrupt interface
    Sugii, N
    Nakagawa, K
    Kimura, Y
    Yamaguchi, S
    Miyao, M
    SEMICONDUCTOR SCIENCE AND TECHNOLOGY, 1998, 13 (8A) : A140 - A142