Development of a process flowsheet for the beneficiation of low-grade iron ore fines from the Bellary-Hospet region of Karnataka, India

被引:1
作者
Umadevi, T. [1 ]
Abhishek, K. [1 ]
Singh, A. Pratap [1 ]
Sah, R. [1 ]
机构
[1] JSW Steel Ltd, Hyderabad, Andhra Pradesh, India
关键词
Low-grade iron ore fines; Mineralogy; Gravity separation; Size reduction; Magnetic separation; Iron/ iron ores;
D O I
10.1007/BF03402273
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
It was possible to beneficiate a low-grade iron ore fines sample from Bellary-Hospet, Karnataka, India assaying 56% Fe, 9.1% SiO2 and 5.2% Al2O3 and produce two concentrates, namely, a sinter-grade fines concentrate (43.7% by weight), assaying 63.6% Fe, 2.6% SiO2 and 1.7% Al2O3, and a pellet-grade concentrate (30.7% by weight) assaying 64.7% Fe, 2.9% SiO2 and 1.7%Al2O3. Rejects (25.6% by weight) assayed 32.5% Fe, 27.9% SiO2 and 15.4% Al2O3. The mineralogical characterization indicated that the sample consisted of 69.5% ironbearing minerals (56% hematite, 7.5% martite and 6% goethite-limonite), 12.5% quartz and 15.2% clay, and the rest were minor minerals. Liberation size was found to be in the size range of 25 to 100 mu m. The process flow sheet consists of jigs, spirals, grinding and low- and high-intensity magnetic separation of the deslimed feed.
引用
收藏
页码:162 / 168
页数:7
相关论文
共 9 条
  • [1] Burt R. O., 1994, GRAVITY CONCENTRATIO, P416
  • [3] Role of water velocity for efficient jigging of iron ore
    Mukherjee, A. K.
    Bhattacharjee, D.
    Mishra, B. K.
    [J]. MINERALS ENGINEERING, 2006, 19 (09) : 952 - 959
  • [4] Olubambi P.A., 2005, J MINERAL MAT CHARAC, V4, P21, DOI [10.4236/jmmce.2005.41003, DOI 10.4236/JMMCE.2005.41003]
  • [5] PRADIP D., 1994, MINERALS METALLURGIC, V6, P179
  • [6] Savoda J., 1987, MAGNETIC METHODS TRE, P516
  • [7] Shivamohan R., 1985, INT J MINER PROCESS, V15, P503
  • [8] Singh R., 2010, P 25 INT MIN PROC C, P1235
  • [9] Singh R., 2007, BENEFICIATION IRON O, V1, P17