Effect of hot plastic deformation on microstructure and mechanical property of Mg-Mn-Ce magnesium alloy

被引:16
作者
Jian Wei-Wei [1 ]
Kang Zhi-Xin [1 ]
Li Yuan-Yuan [1 ]
机构
[1] S China Univ Technol, Sch Mech Engn, Guangzhou 510640, Peoples R China
关键词
magnesium alloy; plastic deformation; grain refinement; microstructural evolution; mechanical property;
D O I
10.1016/S1003-6326(07)60242-8
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Hot plastic deformation was conducted using a new solid die on a Mg-Mn-Ce magnesium alloy. The results of microstructural examination through OM and TEM show that the grain size is greatly refined from 45 mu m to 1.1 mu m with uniform distribution due to the occurrence of dynamic recrystallization. The grain refinement and high angle grain boundary formation improve the mechanical properties through tensile testing with the strain rate of 1.0 X 10(-4) s(-1) at room temperature and Vickers microhardness testing. The maximum values of tensile strength, elongation and Vickers microhardness are increased to 256.37 MPa, 17.69% and HV57.60, which are 21.36%, 133.80% and 20.50% more than those of the as-received Mg-Mn-Ce magnesium alloy, respectively. The SEM morphologies of tensile fractured surface indicate that the density and size of ductile dimples rise with accumulative strain increasing. The mechanism of microstructural evolution and the relationship between microstructure and mechanical property of Mg-Mn-Ce magnesium alloy processed by this solid die were also analyzed.
引用
收藏
页码:1158 / 1163
页数:6
相关论文
共 15 条
[1]   Texture evolution of five wrought magnesium alloys during route A equal channel angular extrusion: Experiments and simulations [J].
Agnew, SR ;
Mehrotra, P ;
Lillo, TM ;
Stoica, GM ;
Liaw, PK .
ACTA MATERIALIA, 2005, 53 (11) :3135-3146
[2]   Magnesium science, technology and applications [J].
Eliezer, D ;
Aghion, E ;
Froes, FH .
ADVANCED PERFORMANCE MATERIALS, 1998, 5 (03) :201-212
[3]   The processing of difficult-to-work alloys by ECAP with an emphasis on magnesium alloys [J].
Figueiredo, Roberto B. ;
Cetlin, Paulo R. ;
Langdon, Terence G. .
ACTA MATERIALIA, 2007, 55 (14) :4769-4779
[4]   THE DEFORMATION AND AGEING OF MILD STEEL .3. DISCUSSION OF RESULTS [J].
HALL, EO .
PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON SECTION B, 1951, 64 (381) :747-753
[5]   Surface modification of magnesium alloys using triazine dithiols [J].
Kang, ZX ;
Mori, K ;
Oishi, Y .
SURFACE & COATINGS TECHNOLOGY, 2005, 195 (2-3) :162-167
[6]   Mechanical properties and microstructures of an AZ61 Mg Alloy produced by equal channel angular pressing [J].
Kim, WJ ;
An, CW ;
Kim, YS ;
Hong, SI .
SCRIPTA MATERIALIA, 2002, 47 (01) :39-44
[7]   Processing and mechanical properties of fine-grained magnesium alloys [J].
Kubota, K ;
Mabuchi, M ;
Higashi, K .
JOURNAL OF MATERIALS SCIENCE, 1999, 34 (10) :2255-2262
[8]   Microstructure evolution of AZ31 magnesium alloy during equal channel angular extrusion [J].
Li, YY ;
Zhang, DT ;
Chen, WP ;
Liu, Y ;
Guo, GW .
JOURNAL OF MATERIALS SCIENCE, 2004, 39 (11) :3759-3761
[9]   Developing superplasticity in a magnesium alloy through a combination of extrusion and ECAP [J].
Matsubara, K ;
Miyahara, Y ;
Horita, Z ;
Langdon, TG .
ACTA MATERIALIA, 2003, 51 (11) :3073-3084
[10]   Magnesium - Properties - applications - potential [J].
Mordike, BL ;
Ebert, T .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 302 (01) :37-45