Degradation mechanism of the La-Mg-Ni-based metal hydride electrode La0.7Mg0.3Ni3.4Mn0.1

被引:57
作者
Liu, YF [1 ]
Pan, HG [1 ]
Gao, MX [1 ]
Lei, YQ [1 ]
Wang, QD [1 ]
机构
[1] Zhejiang Univ, Dept Mat Sci & Engn, Hangzhou 310027, Peoples R China
关键词
D O I
10.1149/1.1904943
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The degradation mechanism of the La-Mg-Ni-based hydrogen storage electrode alloy La0.7Mg0.3Ni3.4Mn0.1 during charge/ discharge cycling has been systematically studied using X-ray diffraction, X-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES), scanning electron microscopy (SEM), electrochemical impedance spectroscopy, and linear polarization measurements. The results indicate that the intense pulverization and the oxidation/corrosion of the active components during cycling are the two main factors responsible for the fast capacity degradation, and the degradation mechanism of La0.7Mg0.3Ni3.4Mn0.1 electrode can be classified into the three consequent stages, i.e., the pulverization and Mg oxidation stage, the Mg and La oxidation stage, and the oxidation-passivation stage. SEM observation indicates that the pulverization of the alloy particles is serious due to the high cell volume expansion ratio of the hydride to alloy phase of (La, Mg)Ni-3 and LaNi5. A large number of cracks in both the alloy particles and the electrode are thus produced. XPS and AES analyses reveal that composite passive layers of Mg(OH)(2) and La(OH)(2) are formed continuously on the surface of alloy particles and increase in thickness with cycling. This porous film not only decreases the surface electrocatalytic activity but also retards the transfer of hydrogen into/or from the alloy particles to electrolyte, and decreases the amount of hydrogen absorption elements La and Mg in the alloys as well. (c) 2005 The Electrochemical Society. All rights reserved.
引用
收藏
页码:A1089 / A1095
页数:7
相关论文
共 18 条
[1]   Hydrogen storage alloys with PuNi3-Type structure as metal hydride electrodes [J].
Chen, J ;
Kuriyama, N ;
Takeshita, HT ;
Tanaka, H ;
Sakai, T ;
Haruta, M .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2000, 3 (06) :249-252
[2]   Hydriding properties of LaNi3 and CaNi3 and their substitutes with PuNi3-type structure [J].
Chen, J ;
Takeshita, HT ;
Tanaka, H ;
Kuriyama, N ;
Sakai, T ;
Uehara, I ;
Haruta, M .
JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 302 (1-2) :304-313
[3]   AC impedance studies of the discharge process of a Mg2Ni-type hydrogen storage alloy electrode in 6M KOH solution [J].
Cui, N ;
Luo, JL .
JOURNAL OF ALLOYS AND COMPOUNDS, 1998, 265 (1-2) :305-310
[4]   STRUCTURAL RELATIONSHIPS IN RARE EARTH-TRANSITION METAL-HYDRIDES [J].
DUNLAP, BD ;
VICCARO, PJ ;
SHENOY, GK .
JOURNAL OF THE LESS-COMMON METALS, 1980, 74 (01) :75-79
[5]   Synthesis and structure determination of a new series of hydrogen storage alloys; RMg2Ni9 (R=La, Ce, Pr, Nd, Sm and Gd) built from MgNi2 laves-type layers alternating with AB(5) layers [J].
Kadir, K ;
Sakai, T ;
Uehara, I .
JOURNAL OF ALLOYS AND COMPOUNDS, 1997, 257 (1-2) :115-121
[6]   Structural investigation and hydrogen storage capacity of LaMg2Ni9 and (La0.65Ca0.35)(Mg1.32Ca0.68)Ni9 of the AB2C9 type structure [J].
Kadir, K ;
Sakai, T ;
Uehara, I .
JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 302 (1-2) :112-117
[7]   Hydrogen storage properties of new ternary system alloys:: La2MgNi9, La5Mg2Ni23, La3MgNi14 [J].
Kohno, T ;
Yoshida, H ;
Kawashima, F ;
Inaba, T ;
Sakai, I ;
Yamamoto, M ;
Kanda, M .
JOURNAL OF ALLOYS AND COMPOUNDS, 2000, 311 (02) :L5-L7
[8]   ELECTROCHEMICAL IMPEDANCE AND DETERIORATION BEHAVIOR OF METAL HYDRIDE ELECTRODES [J].
KURIYAMA, N ;
SAKAI, T ;
MIYAMURA, H ;
UEHARA, I ;
ISHIKAWA, H ;
IWASAKI, T .
JOURNAL OF ALLOYS AND COMPOUNDS, 1993, 202 :183-197
[9]   A study of the degradation of the electrochemical capacity of amorphous Mg50Ni50 alloy [J].
Liu, WH ;
Lei, YQ ;
Sun, DL ;
Wu, J ;
Wang, QD .
JOURNAL OF POWER SOURCES, 1996, 58 (02) :243-247
[10]  
Liu Y. H., 1987, TECHNIQUES ELECTROCH