Kinetics of structural relaxation of bulk and ribbon Pd40Cu30Ni10P20 glasses determined from electrical resistance measurements

被引:10
作者
Khonik, S. V. [1 ]
Sviridov, V. V. [1 ]
Kobelev, N. P. [1 ]
Yazvitskii, M. Yu. [1 ]
Khonik, V. A. [1 ]
机构
[1] Voronezh State Pedagog Univ, Voronezh 394043, Russia
关键词
D O I
10.1134/S106378340708001X
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
The electrical resistances of ribbon and bulk Pd40Cu30Ni10P20 metallic glasses, whose quenching rates differ by four orders of magnitude, were precisely measured during cyclic heating. Three stages of electrical resistance relaxation are detected as the maximum heating temperature increases. The first and third stages decrease the electrical resistance, and the second stage increases it. The first stage is shown to be caused by the relaxation of deformation-induced internal stresses and not to be related to the excess free volume concentration, which differs by a factor of about 2 in the ribbon and bulk samples. The second stage reflects structural relaxation in the glass and is only partly related to its free volume. The third relaxation stage is assumed to be caused by fine precrystallization phenomena like phase separation. The effect of deformation by rolling or quenching from the temperature range of a supercooled melt on the resistance relaxation kinetics was also studied.
引用
收藏
页码:1411 / 1416
页数:6
相关论文
共 30 条
[1]   KINETIC-ANALYSIS OF STRUCTURAL RELAXATION IN FENICRPB AMORPHOUS-ALLOYS BY ELECTRICAL-RESISTIVITY MEASUREMENTS [J].
BARICCO, M ;
RIONTINO, G ;
ALLIA, P ;
VINAI, F .
MATERIALS SCIENCE AND ENGINEERING, 1988, 97 :537-539
[2]  
BERLEY AE, 2003, PHYS REV B, V68
[3]   Stress relaxation of bulk and ribbon glassy Pd40Cu30Ni10P20 [J].
Bobrov, OP ;
Csach, K ;
Khonik, VA ;
Kitagawa, K ;
Laptev, SN ;
Yazvitsky, MY .
SCRIPTA MATERIALIA, 2006, 54 (03) :369-373
[4]  
BOBROV OP, 2006, J APPL PHYS, V100, DOI SICI 033518
[5]  
BOBROV OP, 2006, IN PRESS SCR MAT
[6]  
Chakh K., 2006, DEFORM RAZRUSHENIE M, P22
[7]   Relationship between the shear viscosity and heating rate of metallic glasses below Tg [J].
Csach, K ;
Bobrov, OP ;
Khonik, VA ;
Lyakhov, SA ;
Kitagawa, K .
PHYSICAL REVIEW B, 2006, 73 (09)
[8]  
DEHEY P, 1996, J NONCRYST SOLIDS, V205, P696
[9]   Thermodynamics, enthalpy relaxation and fragility of the bulk metallic glass-forming liquid Pd43Ni10Cu27P20 [J].
Fan, GJ ;
Löffler, JF ;
Wunderlich, RK ;
Fecht, HJ .
ACTA MATERIALIA, 2004, 52 (03) :667-674
[10]  
FRITSCH G, 1988, LESS COMMON MET, V145, P339