The meaning of high stress abrasion and its application in white cast irons

被引:27
作者
Gates, J. D.
Gore, G. J.
Hermand, M. J-P.
Guerineau, M. J-P.
Martin, P. B.
Saad, J.
机构
[1] Univ Queensland, UQ Mat Performance, St Lucia, Qld 4072, Australia
[2] Univ Queensland, Div Mat, St Lucia, Qld 4072, Australia
[3] Univ Queensland, CAST CRC, St Lucia, Qld 4072, Australia
[4] Bradken Resources Pty Ltd, Runcorn, Qld 4113, Australia
基金
澳大利亚研究理事会;
关键词
white cast iron; high stress abrasion; impact-abrasion; wear mode diagnostics; ball mill; BMAT;
D O I
10.1016/j.wear.2006.12.033
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
White cast irons perform much less favourably in industrial service environments such as ball mills than would be predicted by standard laboratory abrasion tests. Pin abrasive tests are widely thought to simulate high stress abrasion, but in reality they grossly over-estimate service lives of white iron mill liners compared to pearlitic steel liners. The 'impact-abrasion' hypothesis has suggested that the key difference between laboratory and service conditions is impact. However, we have found no evidence of such a phenomenon in ball mills, and instead the observed behaviour is attributed to high stress abrasion in the service environment. The defining characteristics of high stress abrasion are re-stated in a way that emphasises the load able to be transmitted to the wearing surface through the abrasive particle. Data are presented which indicate that abrasive wear mode can be identified from quantitative performance comparisons between key classes of wear-resistant alloys. Three useful diagnostics are proposed. Using these diagnostics it is shown that pin abrasive tests do not represent high stress abrasion in any industrially-relevant sense. Appropriately modest performance of white irons can be reproduced in various laboratory apparatus having zero or negligible impact energy: RWAT-analogues using solid metal wheels (xWAT), the Abex block-on-track apparatus, and a simple laboratory ball mill abrasion test (BMAT). Of these, the BMAT most closely reproduces the contact and particle mechanics of service conditions, and can give quantitative alloy performance comparisons closely matching those in service. This paper discusses some features of the BMAT and presents preliminary data for white cast irons. (c) 2007 Elsevier B.V. All rights reserved.
引用
收藏
页码:6 / 35
页数:30
相关论文
共 50 条
  • [1] Impact-abrasion behavior of low alloy white cast irons
    Qian, M
    Chaochang, W
    WEAR, 1997, 209 (1-2) : 308 - 315
  • [2] Effects of chromium carbide volume fraction on high-stress abrasion performance of NbC-bearing high chromium white cast irons
    Pourasiabi, Hamid
    Gates, J. D.
    WEAR, 2022, 498
  • [3] Solidification and abrasion wear of white cast irons alloyed with 20% carbide forming elements
    Matsubara, Y
    Sasaguri, N
    Shimizu, K
    Yu, S
    Yu, K
    WEAR, 2001, 250 (250-251) : 502 - 510
  • [4] Comparing the abrasion performance of NiHard-4 and high-Cr-Mo white cast irons: The effects of chemical composition and microstructure
    Jokari-Sheshdeh, Maziar
    Ali, Yahia
    Gallo, Santiago Corujeira
    Lin, Weikang
    Gates, J. D.
    WEAR, 2022, 492-493
  • [5] Effects of Silicon in High-Cr White Cast Irons
    Gundlach, Richard B.
    Tartaglia, John M.
    INTERNATIONAL JOURNAL OF METALCASTING, 2024, 18 (03) : 1843 - 1853
  • [6] Effects of Abrasive Rock Type on CVF-Dependent Performance Trends of White Cast Irons in the Inner Circumference Abrasion Test
    Demirer, E.
    Pourasiabi, Hamid
    McInnes, L. J.
    Knibbe, R.
    Gates, J. D.
    TRIBOLOGY TRANSACTIONS, 2022, 65 (03) : 389 - 404
  • [7] Mild and severe wear of steels and cast irons in sliding abrasion
    Pintaude, G.
    Bernardes, F. G.
    Santos, M. M.
    Sinatora, A.
    Albertin, E.
    WEAR, 2009, 267 (1-4) : 19 - 25
  • [8] Effects of Particle Impingement and Coarse Particle Abrasion on Wear Performance of White Cast Irons in Sliding Bed Applications
    Demirer, E.
    Pourasiabi, Hamid
    Gates, J. D.
    TRIBOLOGY TRANSACTIONS, 2022, 65 (04) : 662 - 676
  • [9] Structure refinement effect on two and three-body abrasion resistance of high chromium cast irons
    Penagos, J. J.
    Ono, F.
    Albertin, E.
    Sinatora, A.
    WEAR, 2015, 340 : 19 - 24
  • [10] Wear and oxidation behaviour of multicomponent white cast irons
    Ziadi, A
    Belzunce, FJ
    Rodriguez, C
    Riba, J
    MATERIALS SCIENCE AND TECHNOLOGY, 2005, 21 (10) : 1181 - 1186