Impact of Oxidation Conditions and Surface Defects on the Reliability of Large-area Gate Oxide on the C-face of 4H-SiC

被引:14
|
作者
Hatakeyama, T. [1 ,2 ]
Suzuki, T. [1 ,2 ]
Ichinoseki, K. [1 ,3 ]
Matsuhata, H. [3 ]
Fukuda, K. [3 ]
Shinohe, T. [1 ,2 ]
Arai, K. [3 ]
机构
[1] Toshiba Co Ltd, Corp R&D Ctr, R&D Assoc Future Electron Devices, Adv Inverter Lab,Saiwai Ku, 1 Komukai Toshiba Cho, Kawasaki, Kanagawa 2128582, Japan
[2] Toshiba Co Ltd, Corp R&D Ctr, Elect Dev Lab, Kawasaki, Kanagawa 2128582, Japan
[3] Natl Inst Adv Ind Sci & Technol, Energy Semicond Elect Res Lab, Tsukuba, Ibaraki 305, Japan
来源
SILICON CARBIDE AND RELATED MATERIALS 2009, PTS 1 AND 2 | 2010年 / 645-648卷
关键词
MOSFET; Gate Oxide; Reliability; Dislocation; TDDB; Surface Defect; CHEMICAL-VAPOR-DEPOSITION;
D O I
10.4028/www.scientific.net/MSF.645-648.799
中图分类号
TB33 [复合材料];
学科分类号
摘要
This paper discusses the issues regarding reliability of large-area (up to 25mm(2)) gate oxide on the C-face of 4H-SiC. We have shown that the TDDB characteristics of large-area gate oxide improved by separating gate oxidation processes into oxide growth by dry-oxidation and successive interface control by anneal in N2O ambient or that by wet-oxidation followed by anneal in El, ambient. In particular, dry-oxidation followed by anneal in N2O ambient for interface treatment (dry+N2O process) is effective for the suppression of the random failure in TDDB characteristics. The estimated lifetime of gate oxide of less than 9mm(2) by the dry+N2O process is six-digits larger than 30 years. In the case of the TDDB characteristics of 25mm(2) gate oxide grown by the dry+N2O process, the initial and random failure in TDDB characteristics is dominant. However, even in this case, we have confirmed that the evaluated lifetime of 25mm(2) gate oxide is more than 30 years. In order to clarify the mechanism of the degradation of the TDDB characteristics of large-area gate oxide, we examined the effect of the surface defect on the TDDB characteristics by observing the surface of each broken MOS capacitor after the TDDB test. We have found following results. (1) The initial failures in TDDB characteristics are mainly due to surface defects such as "down fall", "comet", and "triangular defect". (2) The footprints of random failure do not correspond to the positions of smaller surface defects such as "bump". Finally, we have found that the quality of the epitaxial layer affects random failure rate in the TDDB characteristics of large area gate oxide; the random failure in the TDDB characteristics of 25mm(2) gate oxide on epitaxial layer grown by a certain epitaxial vendor is almost suppressed. However, the cause of the difference in TDDB characteristics is not identified.
引用
收藏
页码:799 / +
页数:2
相关论文
共 50 条
  • [21] Angle-resolved Photoelectron Spectroscopy studies of initial stage of oxidation on C-face 4H-SiC
    Sasago, T.
    Yamahori, S.
    Nohira, H.
    GALLIUM NITRIDE AND SILICON CARBIDE POWER TECHNOLOGIES 4, 2014, 64 (07): : 245 - 252
  • [22] Growth and characterization of nitrogen-doped C-face 4H-SiC epilayers
    Chen, Wenzhou
    Lee, Kung-Yen
    Capano, Michael A.
    JOURNAL OF CRYSTAL GROWTH, 2006, 297 (02) : 265 - 271
  • [23] Ultrahigh-temperature oxidation of 4H-SiC (0001) and gate oxide reliability dependence on oxidation temperature
    Wan, Caiping
    Xu, Hengyu
    Xia, Jinghua
    Ao, Jin-Ping
    JOURNAL OF CRYSTAL GROWTH, 2020, 530 (530)
  • [24] Shape Control of Trenched 4H-SiC C-Face by Thermal Chlorine Etching
    Koketsu, Hidenori
    Hatayama, Tomoaki
    Yano, Hiroshi
    Fuyuki, Takashi
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2012, 51 (05)
  • [25] Reduction in Background Carrier Concentration for 4H-SiC C-face Epitaxial Growth
    Johji Nishio
    Hirokuni Asamizu
    Mitsuhiro Kushibe
    Hidenori Kitai
    Kazutoshi Kojima
    MRS Advances, 2016, 1 (54) : 3631 - 3636
  • [26] Shape control of trenched 4H-SiC C-face by thermal chlorine etching
    Graduate School of Materials Science, Nara Institute of Science and Technology, Ikoma, Nara 630-0192, Japan
    Jpn. J. Appl. Phys., 1600, 5 PART 1
  • [27] Influence of the Oxidation Temperature and Atmosphere on the Reliability of Thick Gate Oxides on the 4H-SiC C(000-1) face
    Grieb, M.
    Peters, D.
    Bauer, A. J.
    Friedrichs, P.
    Ryssel, H.
    SILICON CARBIDE AND RELATED MATERIALS 2007, PTS 1 AND 2, 2009, 600-603 : 597 - +
  • [28] Reduction in Background Carrier Concentration for 4H-SiC C-face Epitaxial Growth
    Nishio, Johji
    Asamizu, Hirokuni
    Kushibe, Mitsuhiro
    Kitai, Hidenori
    Kojima, Kazutoshi
    MRS ADVANCES, 2016, 1 (54): : 3631 - 3636
  • [29] Gate oxide reliability on trapezoid-shaped defects and obtuse triangular defects in 4H-SiC epitaxial wafers
    Ishiyama, Osamu
    Yamada, Keiichi
    Sako, Hideki
    Tamura, Kentaro
    Kitabatake, Makoto
    Senzaki, Junji
    Matsuhata, Hirofumi
    JAPANESE JOURNAL OF APPLIED PHYSICS, 2014, 53 (04)
  • [30] Density of Etch Pits on C-face 4H-SiC Surface Produced by ClF3 Gas
    Habuka, Hitoshi
    Furukawa, Kazuchika
    Kanai, Toshimitsu
    Kato, Tomohisa
    DEFECTS-RECOGNITION, IMAGING AND PHYSICS IN SEMICONDUCTORS XIV, 2012, 725 : 49 - +