Effects of heat treatment and hot forging on microstructure and mechanical properties of Co-Cr-Mo alloy for surgical implants

被引:29
作者
Okazaki, Yoshimitsu [1 ]
机构
[1] Natl Inst Adv Ind Sci & Technol, Inst Mech Syst Engn, Tsukuba, Ibaraki 3058564, Japan
关键词
microstructure; mechanical property; cobalt alloy; heat treatment; hot forging;
D O I
10.2320/matertrans.MRA2007274
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effects of heat treatment and hot forging on the microstructure and mechanical properties of Co-Cr-Mo alloy for implant applications were examined. In an alloy annealed at 1200 degrees C for 1 h, M23C6 carbides precipitated along the grain boundary in the gamma phase matrix containing a small amount of 6 phase. The 0.2% proof strength (sigma(0.2%PS)), ultimate tensile strength (CUTS), total elongation (T. E.), and reduction of area (R. A.) of annealed alloy were 553 +/- 2 MPa, 928 +/- 41 MPa, 21 +/- 2%, and 15 +/- 1%, respectively. The sigma(0.2%PS) and sigma(UTS) of the Co-Cr-Mo alloy hot-forged at a starting temperature of 1100 degrees C increased linearly with an increase in reduction in area, whereas T. E. gradually decreased with an increase in the reduction. The sigma(0.2%PS), sigma(UTS), T. E., and R. A. of 57% hot-forged alloy were 715 +/- 86MPa, 1109 +/- 61 MPa, 8 +/- 1%, and 10 +/- 1%, respectively. In the 57% hot-forged Co-Cr-Mo alloy, a large amount of M23C6 carbide and a small amount of M6C carbide were observed in the gamma phase matrix containing the E phase. In the light of these results, it appears that hot forging with a starting temperature of approximately 1100 degrees C provided excellent mechanical properties to the alloys.
引用
收藏
页码:817 / 823
页数:7
相关论文
共 9 条
[1]   The production and properties of wrought high carbon Co-Cr-Mo alloys [J].
Berry, G ;
Bolton, JD ;
Brown, JB ;
McQuaide, S .
COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 :11-31
[2]   Metal-on-metal hip replacements: Wear performance and cellular response to wear particles [J].
Campbell, P ;
McKellop, H ;
Alim, R ;
Mirra, J ;
Nutt, S ;
Dorr, L ;
Amstutz, HC .
COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 :193-209
[3]   Effect of carbon addition on microstructure and mechanical properties of a wrought Co-Cr-Mo implant alloy [J].
Lee, SH ;
Takahashi, E ;
Nomura, N ;
Chiba, A .
MATERIALS TRANSACTIONS, 2006, 47 (02) :287-290
[4]   Effect of heat treatment on microstructure and mechanical properties of Ni- and C-free Co-Cr-Mo alloys for medical applications [J].
Lee, SH ;
Takahashi, E ;
Nomura, N ;
Chiba, A .
MATERIALS TRANSACTIONS, 2005, 46 (08) :1790-1793
[5]   Process metallurgy of wrought CoCrMo alloy [J].
Lippard, HE ;
Kennedy, RL .
COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 :98-107
[6]   Comparison of two cobalt-based alloys for use in metal-on-metal hip prostheses: Evaluation of the wear properties in a simulator [J].
St John, KR ;
Poggie, RA ;
Zardiackas, LD ;
Afflitto, RM .
COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 :145-155
[7]   Corrosion of cemented titanium femoral stems [J].
Thomas, SR ;
Shukla, D ;
Latham, PD .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 2004, 86B (07) :974-978
[8]   Residual abrasive material from surface grinding of metal-metal hip implants: A source of third-body wear? [J].
Wang, A ;
Bobyn, JD ;
Yue, S ;
Medley, JB ;
Chan, FW .
COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 :125-134
[9]   Metal-on-metal wear testing of Co-Cr alloys [J].
Wang, KK ;
Wang, A ;
Gustavson, LJ .
COBALT-BASE ALLOYS FOR BIOMEDICAL APPLICATIONS, 1999, 1365 :135-144