Design and optimization of an intumescent flame retardant coating using thermal degradation kinetics and Taguchi's experimental design

被引:12
作者
Derakhshesh, Zahra [3 ]
Khorasani, Manouchehr [1 ]
Akhlaghi, Shahin [2 ]
Keyvani, Bahram [3 ]
Alvani, Ali Asghar Sabbagh [1 ]
机构
[1] Amirkabir Univ Technol, Color & Polymer Res Ctr, Tehran, Iran
[2] Islamic Azad Univ, S Tehran Branch, Dept Polymer Engn, Tehran, Iran
[3] Islamic Azad Univ, Saveh Branch, Fac Engn, Dept Chem, Save, Iran
关键词
intumescent coating; thermal degradation kinetics; Taguchi method; ANOVA; PHOSPHORUS; MECHANISM;
D O I
10.1002/pi.4160
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Two supplementary approaches in terms of thermal degradation kinetics and Taguchi's experimental design were employed toward developing a design effort for intumescent coatings. A model intumescent system including ammonium polyphosphate (APP), pentaerythritol (PER), melamine (MEL), thermoplastic acrylic resin and liquid hydrocarbon resin was chosen and then subjected to thermogravimetric analysis and heat insulation tests to provide experimental data. Kinetic analysis of the thermogravimetric data based on the Friedman and Kissinger methods revealed that activation energy (Ea) and reaction order (n) could be used as parameters to accurately judge whether the selected intumescent components represented coordinated thermal characteristics. Examination of the calculated Ea and n values showed that the decomposition of thermoplastic acrylic resin and liquid hydrocarbon resin occurred first and that the APP, PER and MEL components were degraded immediately after. Such a degradation sequence was quite consistent with the functional mechanism of intumescent systems. In addition, simultaneous implementation of analysis of variance and mean effect assessment on the Taguchi data demonstrated that the designed formulation, based on the optimized coupling of 10 g MEL into APP/PER 25 g/11 g, exhibited the highest fireproofing time among the prepared coating samples. The APP content had the most important contribution to the flame retardant behaviour, and APP versus PER interactions showed the highest severity index. Scanning electron microscopy showed that the higher flame retardancy of the optimized sample was related to the presence of a large number of micropores in the expanded charring layer structure. Copyright (C) 2012 Society of Chemical Industry
引用
收藏
页码:926 / 933
页数:8
相关论文
共 20 条
[1]  
[Anonymous], 2002, ANAL ANAL CHEM, DOI DOI 10.1021/AC60131A045
[2]  
Antia EK, 1982, EUR POLYM J, V18, P167
[3]   INTUMESCENT FIRE-RETARDANT SYSTEMS [J].
CAMINO, G ;
COSTA, L ;
MARTINASSO, G .
POLYMER DEGRADATION AND STABILITY, 1989, 23 (04) :359-376
[4]   STUDY OF THE MECHANISM OF INTUMESCENCE IN FIRE RETARDANT POLYMERS .5. MECHANISM OF FORMATION OF GASEOUS PRODUCTS IN THE THERMAL-DEGRADATION OF AMMONIUM POLYPHOSPHATE [J].
CAMINO, G ;
COSTA, L ;
TROSSARELLI, L .
POLYMER DEGRADATION AND STABILITY, 1985, 12 (03) :203-211
[5]   A new intumescent flame retardant containing phosphorus and nitrogen: Preparation, thermal properties and application to UV curable coating [J].
Chen, Lijuan ;
Song, Lei ;
Lv, Pin ;
Jie, Ganxin ;
Tai, Qilong ;
Xing, Weiyi ;
Hu, Yuan .
PROGRESS IN ORGANIC COATINGS, 2011, 70 (01) :59-66
[6]   Interactions between chlorinated paraffins and melamine in intumescent paint - investing a way to suppress chlorinated paraffins from the formulations [J].
Ducrocq, P. ;
Duquesne, S. ;
Magnet, S. ;
Bourbigot, S. ;
Delobel, R. .
PROGRESS IN ORGANIC COATINGS, 2006, 57 (04) :430-438
[7]   Study on preparation and fire-retardant mechanism analysis of intumescent flame-retardant coatings [J].
Gu, Jun-wei ;
Zhang, Guang-cheng ;
Dong, Shan-lai ;
Zhang, Qiu-yu ;
Kong, Jie .
SURFACE & COATINGS TECHNOLOGY, 2007, 201 (18) :7835-7841
[8]   Testing fire protective properties of intumescent coatings by in-line temperature measurements on a cone calorimeter [J].
Han, Zhidong ;
Fina, Alberto ;
Malucelli, Giulio ;
Camino, Giovanni .
PROGRESS IN ORGANIC COATINGS, 2010, 69 (04) :475-480
[9]   A review of recent progress in phosphorus-based flame retardants [J].
Levchik, Sergei V. ;
Weil, Edward D. .
JOURNAL OF FIRE SCIENCES, 2006, 24 (05) :345-364
[10]   An Investigation of the thermal degradation of the intumescent coating containing MoO3 and Fe2O3 [J].
Li, Guoxin ;
Yang, Junfen ;
He, Tingshu ;
Wu, Yonghua ;
Liang, Guozheng .
SURFACE & COATINGS TECHNOLOGY, 2008, 202 (13) :3121-3128