Microstructure evolution in HAZ and suppression of Type IV fracture in advanced ferritic power plant steels

被引:78
作者
Abe, F. [1 ]
Tabuchi, M. [1 ]
Tsukamoto, S. [1 ]
Shirane, T. [2 ]
机构
[1] Natl Inst Mat Sci, Consortium JRCM, Japan Res & Dev Ctr Metals, Tsukuba, Ibaraki 305, Japan
[2] Mitsubishi Heavy Ind Co Ltd, Nagasaki 8510392, Japan
关键词
9Cr steel; Boron; Nitrogen; Type IV fracture; Creep strength; HAZ microstructure; WELDED-JOINTS; CREEP STRENGTH; BORON; BEHAVIOR;
D O I
10.1016/j.ijpvp.2010.08.005
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The effect of boron and nitrogen on the microstructure evolution in heat affected zone (HAZ) of 9Cr steel during simulated heating and on the Type IV fracture in welded joints has been investigated at 650 C. Gr.92 exhibits a significant decrease in time to rupture after thermal cycle to a peak temperature near AD, while the creep life of Gr.92N, subjected to only normalizing but no tempering, and 9Cr-boron steel is substantially the same as that of the base metals. In Gr.92 after A(C3) thermal cycle, very few precipitates are formed along PAGBs in the fine-grained microstructure. In the P92N and 9Cr-boron steel after AD heat cycle, on the other hand, not only PAGBs but also lath and block boundaries are covered by M(23)C(6) carbides in the coarse-grained microstructure. It is concluded that the degradation in creep life in Gr.92 after the A(C3) thermal cycle is not caused by grain refinement but that the reduction of boundary and sub-boundary hardening is the most important. Soluble boron is essential for the change in alpha/gamma transformation behavior during heating and also for the suppression of Type IV fracture in welded joints. Newly alloy-designed 9Cr steel with 160 ppm boron and 85 ppm nitrogen exhibits much higher creep rupture strength of base metal than P92 and also no Type IV fracture in welded joints at 650 degrees C. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:598 / 604
页数:7
相关论文
共 20 条
[1]   Suppression of Type IV fracture in welded joints of advanced ferritic power plant steels - effect of boron and nitrogen [J].
Abe, F. ;
Tabuchi, M. ;
Kondo, M. ;
Okada, H. .
MATERIALS AT HIGH TEMPERATURES, 2006, 23 (3-4) :145-154
[2]   Microstructure and creep strength of welds in advanced ferritic power plant steels [J].
Abe, F ;
Tabuchi, M .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2004, 9 (01) :22-30
[3]  
ABE F, 2005, WELD WORLD, V49, P58
[4]  
Abe F, 2008, INT J MATER RES, V99, P387, DOI 10.3139/146.101650
[5]   Suppression of Type IV fracture and improvement of creep strength of 9Cr steel welded joints by boron addition [J].
Abe, Fujio ;
Tabuchi, Masaaki ;
Kondo, Masayuki ;
Tsukamoto, Susumu .
INTERNATIONAL JOURNAL OF PRESSURE VESSELS AND PIPING, 2007, 84 (1-2) :44-52
[6]   Precipitate design for creep strengthening of 9% Cr tempered martensitic steel for ultra-supercritical power plants [J].
Abe, Fujio .
SCIENCE AND TECHNOLOGY OF ADVANCED MATERIALS, 2008, 9 (01)
[7]   Type IV cracking in ferritic power plant steels [J].
Francis, J. A. ;
Mazur, W. ;
Bhadeshia, H. K. D. H. .
MATERIALS SCIENCE AND TECHNOLOGY, 2006, 22 (12) :1387-1395
[8]   NON-EQUILIBRIUM GRAIN-BOUNDARY SEGREGATION OF BORON IN AUSTENITIC STAINLESS-STEEL .2. FINE SCALE SEGREGATION BEHAVIOR [J].
KARLSSON, L ;
NORDEN, H .
ACTA METALLURGICA, 1988, 36 (01) :13-24
[9]  
KIMMINS ST, 1983, MET SCI, V17, P19
[10]   Suppressing type IV failure via modification of heat affected zone microstructures using high boron content in 9Cr heat resistant steel welded joints [J].
Kondo, M ;
Tabuchi, M ;
Tsukamoto, S ;
Yin, F ;
Abe, F .
SCIENCE AND TECHNOLOGY OF WELDING AND JOINING, 2006, 11 (02) :216-223