Power Module Using Ceramic Heat Sink and Multilayers Silver Sintering

被引:7
|
作者
Botter, Nicolas [1 ]
Khazaka, Rabih [2 ]
Avenas, Yvan [1 ]
Bouvard, Didier [1 ]
Missiaen, Jean-Michel [1 ]
机构
[1] Univ Grenoble Alpes, CNRS, Grenoble INP, G2Elab SIMAP, F-38000 Grenoble, France
[2] Safran Tech, Elect & Elect Syst Res Grp, F-78114 Magny Les Hameaux, France
来源
IEEE TRANSACTIONS ON COMPONENTS PACKAGING AND MANUFACTURING TECHNOLOGY | 2022年 / 12卷 / 07期
关键词
Silver; Ceramics; Adhesives; Sintering; Aluminum nitride; III-V semiconductor materials; Multichip modules; Adhesion layer; assembly; ceramic heat sink; power modules; silver sintering; HIGH-TEMPERATURE; RELIABILITY; ELECTRONICS; PASTE;
D O I
10.1109/TCPMT.2022.3179432
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A new packaging technology allowing the development of high-performance power modules for harsh environments and the optimization of the manufacturing process is presented. The assembly is achieved using an aluminum nitride ceramic heat sink and multilayer silver sintering to make both current track and die attach layers. In order to control the properties of silver sintered layers, a focus on the pressureless sintering process parameters at conventional and unusually high temperatures was performed. Depending on the sintering temperature and the dwell time, the relative density of the sintered layers was evaluated in the range of 56%-88%. The electrical resistivity was measured in a large temperature range for various densities, and the latter can only be 30% higher than the one of bulk silver once the paste is sintered at 500 degrees C for 1 h. Finally, the mechanical and microstructure properties of assemblies using several metal adhesion layers on the ceramic heat sink and silver sintered multilayers were investigated. Assemblies using Ti/Ni/Ag sputtered layers and silver ink sintered layer as adhesion layers on the AlN ceramic show acceptable shear stress values of about 20 MPa, while the values less than 10 MPa are obtained for W/Ni/Au and W/Ni/Ag adhesion layers. For W/Ni/Au adhesion layers, Ag-Au solid solution was formed at the interface between the sintered silver and the Au finish, leading to a depletion zone at the sintered silver interface and, hence, low shear stress. For W/Ni/Ag adhesion layers, the low shear stress value is mainly due to the oxidation of the Ni layer.
引用
收藏
页码:1082 / 1090
页数:9
相关论文
共 50 条
  • [41] Power Module on Copper Lead Frame with Novel Sintering Paste and SnSb solder
    Wai, Leong Ching
    Yamamoto, Kazunori
    Boon, Simon Lim Siak
    Yue, Tang Gong
    2020 IEEE 22ND ELECTRONICS PACKAGING TECHNOLOGY CONFERENCE (EPTC), 2020, : 302 - 306
  • [42] Pressureless Silver Sintering Die-Attach for SiC Power Devices
    Hascoet, Stanislas
    Buttay, Cyril
    Planson, Dominique
    Chiriac, Rodica
    Masson, Amandine
    SILICON CARBIDE AND RELATED MATERIALS 2012, 2013, 740-742 : 851 - +
  • [43] Power Electronic Assemblies on Printed Wiring Boards Mounted by Silver Sintering
    Schiffmacher, Alexander
    Litzenberger, Lorenz
    Wilde, Juergen
    Polezhaev, Vladimir
    Huesgen, Till
    2018 7TH ELECTRONIC SYSTEM-INTEGRATION TECHNOLOGY CONFERENCE (ESTC), 2018,
  • [44] Sintering process of inkjet-printed silver patterns using a heated inert gas
    Shin, Kwon-Yong
    Park, Nam Son
    Hwang, Jun Young
    Kang, Kyungtae
    Lee, Sang-Ho
    MICROELECTRONIC ENGINEERING, 2018, 193 : 91 - 97
  • [45] A NEW TYPE OF CERAMIC SINTERING APPARATUS USING MICROWAVE HEATING
    田永赉
    李包顺
    施剑林
    宋癸祯
    郭景坤
    陶金陵
    ChineseScienceBulletin, 1991, (11) : 900 - 902
  • [46] Drying and sintering of ceramic based parts using microwave heating
    Esin, A
    Mahmutyazicioglu, N
    Altintas, S
    EURO CERAMICS VIII, PTS 1-3, 2004, 264-268 : 731 - 734
  • [47] Analysis and Design Optimization of Tilted Rounded-Rectangular Pin-Fins Heat Sink for xEV Double-Sided Cooling Power Module
    Cho, Seongmoo
    Pyun, Sunghyun
    Yoon, Sang Won
    IEEE JOURNAL OF EMERGING AND SELECTED TOPICS IN POWER ELECTRONICS, 2024, 12 (02) : 1803 - 1812
  • [48] Characterisation of ceramic coatings sintering using residual stress measurements
    Wang, X
    Xiao, P
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2004, 24 (02) : 283 - 288
  • [49] Sintering of Inkjet-Printed Silver Nanoparticles at Room Temperature Using Intense Pulsed Light
    J. S. Kang
    J. Ryu
    H. S. Kim
    H. T. Hahn
    Journal of Electronic Materials, 2011, 40 : 2268 - 2277
  • [50] A Multichip Phase-Leg IGBT Module Using Nanosilver Paste by Pressureless Sintering in Formic Acid Atmosphere
    Yan, Haidong
    Mei, Yun-Hui
    Li, Xin
    Ma, Changsheng
    Lu, Guo-Quan
    IEEE TRANSACTIONS ON ELECTRON DEVICES, 2018, 65 (10) : 4499 - 4505