Mimicking Barkhausen noise measurement by in-situ transmission electron microscopy-effect of microstructural steel features on Barkhausen noise

被引:22
作者
Honkanen, Mari [1 ]
Santa-aho, Suvi [2 ]
Laurson, Lasse [3 ]
Eslahi, Nasser [4 ]
Foi, Alessandro [4 ]
Vippola, Minnamari [1 ,2 ]
机构
[1] Tampere Univ, Tampere Microscopy Ctr, POB 692, FI-33014 Tampere, Finland
[2] Tampere Univ, Fac Engn & Nat Sci, Mat Sci & Environm Engn, POB 589, FI-33104 Tampere, Finland
[3] Tampere Univ, Fac Engn & Nat Sci, Computat Phys Lab, POB 692, FI-33014 Tampere, Finland
[4] Tampere Univ, Fac Informat Technol & Commun Sci, Comp Sci, POB 553, FI-33104 Tampere, Finland
关键词
Barkhausen noise (BN); Ferromagnetic; Electron backscatter diffraction (EBSD); In situ transmission electron microscopy  (TEM); Magnetic domains; Steels; EMISSION; MAGNETIZATION; HARDNESS; STRESS; DISLOCATIONS; DYNAMICS; STRENGTH; TEM;
D O I
10.1016/j.actamat.2021.117378
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
A relationship between microstructural steel features and an outcome of the Barkhausen noise (BN) measurement was studied. Two different microstructures, martensite and pearlite-ferrite were used. Commonly, BN is linked directly to the sample hardness. A BN outcome from both martensite and pearliteferrite was, however, similar even though martensite has three times higher hardness. To reveal the connection between microstructural features and BN, a typical industrial BN measurement was mimicked by in-situ transmission electron microscopy (TEM). Martensite needed higher field strength to move domain walls (DWs) than pearlite-ferrite. In martensite, DWs gathered to areas with high dislocation density. Fe 3 C lamellae in pearlite were strong pinning sites. DWs perpendicular and parallel to martensite laths started to move with the same field strength value. In pearlite, DWs perpendicular to lamellae started to move before the parallel ones. The RMS envelope of ferrite-pearlite starts earlier than that of martensite due to soft ferrite. Magnetically harder pearlite probably caused "a tail" and the envelope ends almost at the same time with martensite. . Nevertheless, similar peak width values were found for both samples. Martensite and pearlite have a lot of strong pinning sites, dislocations and Fe 3 C, respectively. Fe 3 C density is not as high as dislocation density. Ferrite has strong pinning sites only at low incidence, but as known, huge BN information volume compared to martensite and pearlite. This resulted in the similar pulse count from martensite and ferrite-pearlite. (c) 2021 The Author(s). Published by Elsevier Ltd on behalf of Acta Materialia Inc. This is an open access article under the CC BY license ( http://creativecommons.org/licenses/by/4.0/ )
引用
收藏
页数:11
相关论文
共 47 条
[11]   Dynamics of a ferromagnetic domain wall and the Barkhausen effect [J].
Cizeau, P ;
Zapperi, S ;
Durin, G ;
Stanley, HE .
PHYSICAL REVIEW LETTERS, 1997, 79 (23) :4669-4672
[12]   THE INFLUENCE OF PEARLITE ON BARKHAUSEN NOISE GENERATION IN PLAIN CARBON-STEELS [J].
CLAPHAM, L ;
JAGADISH, C ;
ATHERTON, DL .
ACTA METALLURGICA ET MATERIALIA, 1991, 39 (07) :1555-1562
[13]  
Cullity G.C, 2008, INTRO MAGNETIC MAT, DOI [10.1002/9780470386323. fmatter, DOI 10.1002/9780470386323.FMATTER]
[14]   Monitoring the microstructural changes during tempering of quenched SAE 5140 steel by magnetic barkhausen noise [J].
Davut, Kemal ;
Guer, C. Hakan .
JOURNAL OF NONDESTRUCTIVE EVALUATION, 2007, 26 (2-4) :107-113
[15]   In situ transmission electron microscopy for magnetic nanostructures [J].
Duc-The Ngo ;
Kuhn, Luise Theil .
ADVANCES IN NATURAL SCIENCES-NANOSCIENCE AND NANOTECHNOLOGY, 2016, 7 (04)
[16]   Scaling exponents for Barkhausen avalanches in polycrystalline and amorphous ferromagnets [J].
Durin, G ;
Zapperi, S .
PHYSICAL REVIEW LETTERS, 2000, 84 (20) :4705-4708
[17]  
Eslahi N, 2019, 2019 IEEE 8TH INTERNATIONAL WORKSHOP ON COMPUTATIONAL ADVANCES IN MULTI-SENSOR ADAPTIVE PROCESSING (CAMSAP 2019), P111, DOI [10.1109/camsap45676.2019.9022478, 10.1109/CAMSAP45676.2019.9022478]
[18]  
Fiorillo F., 2004, CHARACTERIZATION MEA, DOI [10.1016/B978-012257251-7/50014-9, DOI 10.1016/B978-012257251-7/50014-9]
[19]   Relation Between Magnetic Barkhausen Noise and Hardness for Jominy Quench Tests in SAE 4140 and 6150 Steels [J].
Franco, Freddy A. ;
Gonzalez, M. F. R. ;
de Campos, M. F. ;
Padovese, L. R. .
JOURNAL OF NONDESTRUCTIVE EVALUATION, 2013, 32 (01) :93-103
[20]   Advances in magnetic microscopy [J].
Freeman, MR ;
Choi, BC .
SCIENCE, 2001, 294 (5546) :1484-1488