Pitting on the crevice wall prior to crevice corrosion: Iron in sulfate/chromate solution

被引:17
作者
Shu, Hung-Kai [2 ]
Al-Faqeer, Faisal M. [3 ]
Pickering, Howard W. [1 ]
机构
[1] Penn State Univ, Dept Mat Sci & Engn, University Pk, PA 16802 USA
[2] Natl Taiwan Univ, Dept Mat Sci & Engn, Taipei, Taiwan
[3] Ctr Res & Dev, Dhahran 31311, Saudi Arabia
关键词
Localized corrosion; IR voltage; Polarization curve; Hydrogen evolution; Corrosion product; LOCALIZED CORROSION; STAINLESS-STEEL; MECHANISM; INITIATION; PH;
D O I
10.1016/j.electacta.2010.10.013
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Experimental results are presented for the induction period that precedes the onset of crevice corrosion. In situ visual examination and ex situ microscopy revealed that the first corrosive attack on the (passive) crevice wall occurs as a pit near the bottom of the crevice. Additional pits and corrosion product form higher and higher on the crevice wall during the induction period. The measured current is initially low in the passive range (10 mu A), increasing gradually, but the measured current does not record the large increases in anodic current that produce the pits. The latter result and the observation that gas bubbles form within the pits indicate that the pitting initially is a local cell process of metal dissolution and cathodic reactions on the sample, including H-2 formation which occurs inside the pits in this iron/sulfate-chromate solution (pH 8.8, room temperature). Then, a transition from merging pits to corrosive attack across the width of the crevice wall occurs accompanied by a much steeper increasing current. This latter morphology (horizontal boundary that moves up the wall towards the crevice opening, heaviest attack just below this boundary and passive crevice wall above this boundary) is representative of stable crevice corrosion of the IR type reported in the literature. (C) 2010 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1719 / 1728
页数:10
相关论文
共 46 条
[11]   An Extended Finite Element Method Based Approach for Modeling Crevice and Pitting Corrosion [J].
Duddu, Ravindra ;
Kota, Nithyanand ;
Qidwai, Siddiq M. .
JOURNAL OF APPLIED MECHANICS-TRANSACTIONS OF THE ASME, 2016, 83 (08)
[12]   Crevice corrosion of Q235 carbon steels in a solution of NaHCO3 and NaCl [J].
Hu, Q. ;
Qiu, Y. B. ;
Guo, X. P. ;
Huang, J. Y. .
CORROSION SCIENCE, 2010, 52 (04) :1205-1212
[13]   Susceptibility of 254 SMO Alloys to Crevice Corrosion in NaCl Solution [J].
Arab, Sanaa T. ;
Abdulsalam, Mohammed I. ;
Alghamdi, Huda M. .
ARABIAN JOURNAL FOR SCIENCE AND ENGINEERING, 2014, 39 (07) :5405-5412
[14]   Single-boss crevice former for studying crevice corrosion of UNS S32003 in chloride-containing solution at high temperature [J].
Karayan, Ahmad Ivan ;
Guerrero, Javier Esquivel ;
Castaneda, Homero .
JOURNAL OF ALLOYS AND COMPOUNDS, 2015, 619 :544-552
[15]   Numerical Simulation for Crevice Corrosion of 304 Stainless Steel in Sodium Chloride Solution [J].
Wang Wei ;
Sun Hu-yuan ;
Sun Li-juan ;
Song Zu-wei ;
Zang Bei-ni .
CHEMICAL RESEARCH IN CHINESE UNIVERSITIES, 2010, 26 (05) :822-828
[16]   Inverse Crevice Corrosion of Carbon Steel: Effect of Solution Volume to Surface Area [J].
Wu, Linda ;
Guo, Dan ;
Li, Mi ;
Joseph, Jiju M. ;
Noel, James J. ;
Keech, Peter G. ;
Wren, J. Clara .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2017, 164 (09) :C539-C553
[17]   Effect of Tungsten on the Pitting and Crevice Corrosion Resistance of Type 25Cr Super Duplex Stainless Steels [J].
Haugan, Eirik B. ;
Naess, Monika ;
Rodriguez, Cristian Torres ;
Johnsen, Roy ;
Iannuzzi, Mariano .
CORROSION, 2017, 73 (01) :53-67
[18]   Crevice corrosion resistance of high alloyed materials in 3.5 % NaCl solution [J].
Alar, Vesna ;
Stojanovic, Ivan ;
Simunovic, Vinko ;
Novak, Tomislav .
INTERNATIONAL JOURNAL OF MATERIALS RESEARCH, 2014, 105 (06) :603-606
[19]   Experimental design to study the influence of temperature, pH, and chloride concentration on the pitting and crevice corrosion of UNS S30403 stainless steel [J].
Dastgerdi, Arash Azimi ;
Brenna, Andrea ;
Ormellese, Marco ;
Pedeferri, MariaPia ;
Bolzoni, Fabio .
CORROSION SCIENCE, 2019, 159
[20]   Effect of Nitrided and Nitrocarburised Austenite on Pitting and Crevice Corrosion Resistance of 316 LVM Steel Implants [J].
Kajzer, Anita ;
Ceglarska, Magdalena ;
Sura, Nika ;
Kajzer, Wojciech ;
Borowski, Tomasz ;
Tarnowski, Michal ;
Pilecki, Zbigniew .
MATERIALS, 2020, 13 (23) :1-15