Fretting wear behavior of zirconium alloy in B-Li water at 300 °C

被引:34
|
作者
Zhang, Lefu [1 ]
Lai, Ping [1 ]
Liu, Qingdong [1 ]
Zeng, Qifeng [2 ]
Lu, Junqiang [2 ]
Guo, Xianglong [1 ]
机构
[1] Shanghai Jiao Tong Univ, Sch Nucl Sci & Engn, 800 Dongchuan Rd, Shanghai 200240, Peoples R China
[2] Shanghai Nucl Engn Res & Design Inst, 29 Hongcao Rd, Shanghai 200233, Peoples R China
关键词
Fretting wear; Zirconium alloy; B-Li water; Wear mode; Oxide layer; HIGH-TEMPERATURE WATER; INCONEL; 690; ALLOY; SURFACE-ROUGHNESS; CONTACT; STEEL; HARDNESS; DEBRIS; FUEL; METHODOLOGY; MECHANISMS;
D O I
10.1016/j.jnucmat.2017.12.003
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The tangential fretting wear of three kinds of zirconium alloys tube mated with 304 stainless steel (SS) plate was investigated. The tests were conducted in an autoclave containing 300 degrees C pressurized B-Li water for tube-on-plate contact configuration. The worn surfaces were examined with scanning electron microscopy (SEM), energy dispersive spectroscopy (EDS) and 3D microscopy. The cross-section of wear scar was examined with transmission electron microscope (TEM). The results indicated that the dominant wear mechanism of zirconium alloys in this test condition was delamination and oxidation. The oxide layer on the fretted area consists of outer oxide layer composed of iron oxide and zirconium oxide and inner oxide layer composed of zirconium oxide. (C) 2017 Published by Elsevier B.V.
引用
收藏
页码:401 / 409
页数:9
相关论文
共 50 条
  • [1] Characterization and fretting wear behavior of zirconium alloy treated in high temperature water
    Li, Zheng-yang
    Zheng, Mei-yin
    Ren, Quan-yao
    Cai, Zhen-bing
    Jiao, Yong-jun
    WEAR, 2023, 532
  • [2] Effect of Normal Force on Fretting Wear Behavior of Zirconium Alloy Tube in Simulated Primary Water of PWR
    Zhang, Yusheng
    Lai, Jiang
    Ming, Hongliang
    Gao, Lixia
    Wang, Jianqiu
    Han, En-Hou
    ACTA METALLURGICA SINICA-ENGLISH LETTERS, 2023, 36 (05): : 865 - 880
  • [3] Effect of Normal Force on Fretting Wear Behavior of Zirconium Alloy Tube in Simulated Primary Water of PWR
    Yusheng Zhang
    Jiang Lai
    Hongliang Ming
    Lixia Gao
    Jianqiu Wang
    En-Hou Han
    Acta Metallurgica Sinica (English Letters), 2023, 36 : 865 - 880
  • [4] Effect of micro-arc oxidation on fretting wear behavior of zirconium alloy exposed to high temperature water
    Lai, Ping
    Zhang, Hao
    Zhang, Lefu
    Zeng, Qifeng
    Lu, Junqiang
    Guo, Xianglong
    WEAR, 2019, 424 : 53 - 61
  • [5] Corrosion and fretting wear behavior of Cr-based composite coatings on zirconium alloy
    Yu, Jian-guo
    Li, Zheng-yang
    Ren, Quan-yao
    Jiao, Yong-jun
    Cai, Zhen-bing
    VACUUM, 2025, 234
  • [6] Effects of displacement amplitude and normal force on fretting wear behavior of zirconium alloy tube in simulated primary water of PWR
    Zhang, Yusheng
    Wu, Bin
    Ming, Hongliang
    Wang, Jiazhen
    Wang, Jianqiu
    Han, En-Hou
    WEAR, 2024, 542
  • [7] Effect of temperature on fretting wear behavior and mechanism of alloy 690 in water
    Lai, Ping
    Gao, Xiaochuan
    Tang, Lichen
    Guo, Xianglong
    Zhang, Lefu
    NUCLEAR ENGINEERING AND DESIGN, 2018, 327 : 51 - 60
  • [8] The Fretting Wear Behavior of NiTi Shape Memory Alloy in Distilled Water
    Zhang Song
    Zhang Chunhua
    Zhang Zhuo
    Han Zhong
    Wang Qiang
    Zhang Yang
    RARE METAL MATERIALS AND ENGINEERING, 2008, 37 (10) : 1772 - 1775
  • [9] The fretting wear behavior of NiTi shape memory alloy in distilled water
    Shenyang University of Technology, Shenyang 110023, China
    不详
    不详
    不详
    Xiyou Jinshu Cailiao Yu Gongcheng, 2008, 10 (1772-1775): : 1772 - 1775
  • [10] Investigation on fretting wear of Al-Li alloy
    Xiao, Teng
    Wen, Daosheng
    Wang, Shouren
    Zhang, Mingyuan
    Kong, Beibei
    Yu, Qiqi
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2020, 72 (07) : 913 - 921