Ageing of electrochemical double layer capacitors

被引:115
作者
Bittner, A. M. [1 ,2 ,3 ]
Zhu, M. [3 ,4 ]
Yang, Y. [3 ,5 ]
Waibel, H. F. [3 ]
Konuma, M. [3 ]
Starke, U. [3 ]
Weber, C. J. [6 ]
机构
[1] CIC nanoGUNE Consolider, E-20018 Donostia San Sebastian, Spain
[2] Ikerbasque, Basque Fdn Sci, E-48011 Bilbao, Spain
[3] Max Planck Inst Solid State Res, D-70569 Stuttgart, Germany
[4] Merck China, Chem Technol Off, Shanghai, Peoples R China
[5] Colorado Sch Mines, Dept Chem & Geochem, Golden, CO 80401 USA
[6] Freudenberg Vliesstoffe KG, Weinheim, Germany
关键词
Electrochemical double layer capacitor; Supercapacitor; XPS (X-ray photoelectron spectroscopy); Raman spectroscopy; Ageing; ESR (equivalent series resistance); CARBON-FIBER SURFACES; RAMAN-SPECTROSCOPIC CHARACTERIZATION; ACETONITRILE-BASED ELECTROLYTE; ACTIVATED CARBONS; CHEMICAL ALTERATION; POLYMER CHEMISTRY; EXPOSURE; ESCA; SUPERCAPACITORS; SPECTRA;
D O I
10.1016/j.jpowsour.2011.10.083
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The activated carbon in electrochemical double layer electrodes undergoes slow ageing. The effect becomes only apparent when capacitors are polarized to voltages at or above specified limits, or at high temperatures, for at least several months. A combination of "post mortem" analysis methods shows that the pores in the carbon are modified structurally, mainly by clogging up with organic species, but also electrochemically by decomposition of electrolyte, and by reduction and oxidation of the carbon in the electrodes. Key chemicals are trace water, the solvent acetonitrile, and the salt tetraethyl ammonium tetrafluoroborate. The changes differ hugely between negative and positive pole; the positively polarized electrode is much more affected. Also other compounds of the device, e.g. aluminum electrode support and paper separator, exhibit chemical ageing. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:262 / 273
页数:12
相关论文
共 69 条
[1]   Surface characterization of binary grafting of AAc/NIPAAm onto poly(tetrafluoroethylene) (PTFE) [J].
Adem, E ;
Avalos-Borja, M ;
Bucio, E ;
Burillo, G ;
Castillon, FF ;
Cota, L .
NUCLEAR INSTRUMENTS & METHODS IN PHYSICS RESEARCH SECTION B-BEAM INTERACTIONS WITH MATERIALS AND ATOMS, 2005, 234 (04) :471-476
[2]   Causes of supercapacitors ageing in organic electrolyte [J].
Azais, Philippe ;
Duclaux, Laurent ;
Florian, Pierre ;
Massiot, Dominique ;
Lillo-Rodenas, Maria-Angeles ;
Linares-Solano, Angel ;
Peres, Jean-Paul ;
Jehoulet, Christophe ;
Beguin, Frangois .
JOURNAL OF POWER SOURCES, 2007, 171 (02) :1046-1053
[3]  
BARANOV AV, 1987, OPT SPEKTROSK+, V62, P1036
[4]   On the characterization of disordered and heterogeneous carbonaceous materials by Raman spectroscopy [J].
Beyssac, O ;
Goffé, B ;
Petitet, JP ;
Froigneux, E ;
Moreau, M ;
Rouzaud, JN .
SPECTROCHIMICA ACTA PART A-MOLECULAR AND BIOMOLECULAR SPECTROSCOPY, 2003, 59 (10) :2267-2276
[5]   The characterization of activated carbons with oxygen and nitrogen surface groups [J].
Biniak, S ;
Szymanski, G ;
Siedlewski, J ;
Swiatkowski, A .
CARBON, 1997, 35 (12) :1799-1810
[6]   Ultracapacitor technologies and application in hybrid and electric vehicles [J].
Burke, Andrew .
INTERNATIONAL JOURNAL OF ENERGY RESEARCH, 2010, 34 (02) :133-151
[7]  
Byrne J.F., 1995, POROSITY CARBONS, P1
[8]   Electrolyte Systems for High Withstand Voltage and Durability I. Linear Sulfones for Electric Double-Layer Capacitors [J].
Chiba, Kazumi ;
Ueda, Tsukasa ;
Yamaguchi, Yoji ;
Oki, Yusuke ;
Shimodate, Fumitaka ;
Naoi, Katsuhiko .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2011, 158 (08) :A872-A882
[9]   ESCA APPLIED TO POLYMERS .23. RF GLOW-DISCHARGE MODIFICATION OF POLYMERS IN PURE OXYGEN AND HELIUM-OXYGEN MIXTURES [J].
CLARK, DT ;
DILKS, A .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1979, 17 (04) :957-976
[10]   APPLICATIONS OF ESCA TO POLYMER CHEMISTRY .10. CORE AND VALENCE ENERGY-LEVELS OF A SERIES OF POLYACRYLATES [J].
CLARK, DT ;
THOMAS, HR .
JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, 1976, 14 (07) :1671-1700